摘要:
A process for producing a rubber composition comprising the first step of heat-treating at 120°C or more a mixture comprising of 100 parts by weight of an ethylene-α-olefin copolymer rubber, 0.5-5 parts by weight of at least one dinitrodiamine and at least one radical generating agent to obtain a heat-treated mixture, the second step of adding a filler to the heat-treated mixture and kneading them to obtain a rubber mixture and the third step of compounding a crosslinking agent with the rubber mixture obtained in the second step at 100°C or less to obtain a rubber composition. According to said process, an ethylene-α-olefin copolymer rubber composition which is excellent in heat resistance and durability is obtained.
摘要:
In a process of crosslinking a rubber compound with the usage of an organic peroxide as the crosslinking agent, is incorporated to the rubber compound in an amount of 0.5 - 20 parts by weight per 100 parts of a rubber substrate a compound selected from imidazole type compounds, thiourea type compounds, thiazole type compounds, thiuram type compounds, dithiocarbamate type compounds, phenol type compounds, triazole type compounds and amine type compounds. The process results no surface tackiness of the rubber product crosslinked in the presence of oxygen.
摘要:
The present invention provides a vulcanized rubber useful for heat resistant vibration-isolator which can be obtained by vulcanizing a composition comprising: (A) 110-175 parts by weight of an oil-extended copolymer comprising 100 parts by weight of an ethylene- alpha -olefin-non-conjugated diene copolymer rubber with an intrinsic viscosity [ eta ] of 3 dl/g or more and 10-75 parts by weight of an extender oil; (B) 5-20 parts by weight of a liquid diene polymer with melt viscosity of 100-3000 poises at 25 DEG C, per 100 parts by weight of an ethylene- alpha -olefin-non-conjugated diene copolymer rubber; and (C) 10-80 parts by weight of a reinforcing filler, per 100 parts by weight of an ethylene- alpha -olefin-non-conjugated diene copolymer rubber; with an organic peroxide. The vulcanized rubbers of the present invention have an excellent thermal stability and durability, a low dynamic spring constant, and an excellent processability; they are useful for heat resistant vibration-isolator rubber, and are most suitable for, for example, uses of vibration-isolator for automobiles for engine mount, strato mount, suspension bush, exhaust mount and the like, and uses of vibration-isolator for vehicles for railway, vehicles for construction, industrial instruments, and instruments for office-automation and the like.
摘要:
The present invention provides a vulcanized rubber useful for heat resistant vibration-isolator which can be obtained by vulcanizing a composition comprising:
(A) 110-175 parts by weight of an oil-extended copolymer comprising 100 parts by weight of an ethylene-α-olefin-non-conjugated diene copolymer rubber with an intrinsic viscosity [η] of 3 dl/g or more and 10-75 parts by weight of an extender oil; (B) 5-20 parts by weight of a liquid diene polymer with melt viscosity of 100-3000 poises at 25 °C, per 100 parts by weight of an ethylene-α-olefin-non-conjugated diene copolymer rubber; and (C) 10-80 parts by weight of a reinforcing filler, per 100 parts by weight of an ethylene-α-olefin-non-conjugated diene copolymer rubber; with an organic peroxide.
The vulcanized rubbers of the present invention have an excellent thermal stability and durability, a low dynamic spring constant, and an excellent processability; they are useful for heat resistant vibration-isolator rubber, and are most suitable for, for example, uses of vibration-isolator for automobiles for engine mount, strato mount, suspension bush, exhaust mount and the like, and uses of vibration-isolator for vehicles for railway, vehicles for construction, industrial instruments, and instruments for office-automation and the like.
摘要:
A process for producing a rubber composition comprising the first step of heat-treating at 120°C or more a mixture comprising of 100 parts by weight of an ethylene-α-olefin copolymer rubber, 0.5-5 parts by weight of at least one dinitrodiamine and at least one radical generating agent to obtain a heat-treated mixture, the second step of adding a filler to the heat-treated mixture and kneading them to obtain a rubber mixture and the third step of compounding a crosslinking agent with the rubber mixture obtained in the second step at 100°C or less to obtain a rubber composition. According to said process, an ethylene-α-olefin copolymer rubber composition which is excellent in heat resistance and durability is obtained.
摘要:
In a process of crosslinking a rubber compound with the usage of an organic peroxide as the crosslinking agent, is incorporated to the rubber compound in an amount of 0.5 - 20 parts by weight per 100 parts of a rubber substrate a compound selected from imidazole type compounds, thiourea type compounds, thiazole type compounds, thiuram type compounds, dithiocarbamate type compounds, phenol type compounds, triazole type compounds and amine type compounds. The process results no surface tackiness of the rubber product crosslinked in the presence of oxygen.