摘要:
A method of conditioning stucco comprises the steps of supplying a quantity of stucco particles to a reaction vessel, the stucco particles comprising calcium sulphate hemihydrate and/or calcium sulphate anhydrite, as well as calcium sulphate dihydrate; and conditioning the stucco particles at a temperature of at least 100°C and a humidity of at least 70%. During the step of conditioning the stucco particles, the bulk density of the stucco particles within the reaction vessel is at least 1 g/cm 3 .