Cathode for lithium secondary battery and production method for the same
    2.
    发明公开
    Cathode for lithium secondary battery and production method for the same 失效
    KathodefürLithiumSekundärbatterieund Verfahren zu ihrer Herstellung

    公开(公告)号:EP0714144A1

    公开(公告)日:1996-05-29

    申请号:EP95118294.8

    申请日:1995-11-21

    IPC分类号: H01M4/52 H01M4/54

    摘要: The invention provides a cathode for a lithium secondary battery including lithiated nickel dioxide with a large discharge capacity as an active material and having a high density so that a larger amount of the active material can be charged in a battery container with a limited volume, a production method for the same and a lithium secondary battery utilizing the cathode. The cathode for a lithium secondary battery includes lithiated nickel dioxide as an active material, and the lithiated nickel dioxide is produced by firing a mixture of a lithium compound and a nickel compound at a temperature ranging between 350°C and 800°C. The supernatant obtained by dispersing 5 g of the lithiated nickel dioxide in 100 cm³ of water in a glass vessel for 5 minutes and allowing the resultant solution to stand for 30 seconds has pH of 12.00 or less. The production method includes the steps of obtaining the lithiated nickel dioxide as above and treating or milling the lithiated nickel dioxide in an atmosphere including carbon dioxide.

    摘要翻译: 本发明提供了一种锂二次电池的阴极,其包括具有大放电容量的锂化二氧化镍作为活性材料并且具有高密度,使得可以将更多量的活性材料充电到具有有限体积的电池容器中, 其制造方法和利用阴极的锂二次电池。 锂二次电池用阴极包括锂化二氧化镍作为活性物质,锂化二氧化镍通过在350〜800℃的温度范围内煅烧锂化合物和镍化合物的混合物来制造。上清液 通过将5g锂化二氧化镍在100cm 3的水中分散在玻璃容器中5分钟,并使所得溶液静置30秒,pH为12.00以下。 制备方法包括如下步骤:获得如上所述的锂化二氧化镍,并在包括二氧化碳的气氛中处理或研磨锂化二氧化镍。

    Lithium secondary battery having thermal switch
    3.
    发明公开
    Lithium secondary battery having thermal switch 失效
    Lithiumsekundärbatteriemit Thermischerschalter

    公开(公告)号:EP0862231A1

    公开(公告)日:1998-09-02

    申请号:EP98103460.6

    申请日:1998-02-27

    IPC分类号: H01M2/34

    摘要: Provided is a lithium secondary battery comprising an electrode assembly which consists of a cathode, an anode and a separator laminated therebetween, and a battery case in which the electrode assembly is placed, said lithium secondary battery characterized by having a thermal switch which has a mechanism for electrically connecting the cathode and the anode at a portion other than an active material-containing layer in accordance with an increase in the battery temperature.
    The lithium secondary battery can prevent itself from being left in a charged condition after having an unusual trouble, and can operate the safety device even when its internal pressure decreases.

    摘要翻译: 提供一种锂二次电池,其包括由阴极,阳极和层压在其间的隔板组成的电极组件和其中放置电极组件的电池壳体,所述锂二次电池的特征在于具有热开关,其具有机构 用于根据电池温度的升高将非活性材料含有层以外的部分电连接阴极和阳极。 锂二次电池在发生异常故障之后可以防止其处于充电状态,并且即使在其内部压力降低的情况下也可以操作安全装置。

    Method for manufacturing ROM type optical disk
    4.
    发明公开
    Method for manufacturing ROM type optical disk 失效
    制造ROM型光盘的方法

    公开(公告)号:EP0532004A3

    公开(公告)日:1994-02-23

    申请号:EP92115513.1

    申请日:1992-09-10

    摘要: According to the present invention, there is provided a method for manufacturing a ROM type optical disk in which application program data are written, wherein application program data ([2], [3]) having no information on positions for writing data stored in a storage device (1) are written in an optical disk (3) for supplying data by a data writing optical disk drive (2), and then, the application program data ([2], [3]) and information ([1]) on positions for writing data are read out of an optical disk (3) for supplying data by a data reading optical disk drive (4) and stored in a storage device (5) for manufacturing a ROM type optical disk.

    摘要翻译: 根据本发明,提供了一种用于制造其中写入应用程序数据的ROM型光盘的方法,其中应用程序数据([2],[3])没有关于写入存储在 存储装置(1)被写入用于由数据写入光盘驱动器(2)提供数据的光盘(3),然后,应用程序数据([2],[3])和信息([1] )写入数据的位置从用于由数据读取光盘驱动器(4)提供数据的光盘(3)读出并存储在用于制造ROM型光盘的存储装置(5)中。

    Cathode for lithium secondary battery
    6.
    发明公开
    Cathode for lithium secondary battery 失效
    KathodefürLithiumsekundärbatterie

    公开(公告)号:EP0858117A1

    公开(公告)日:1998-08-12

    申请号:EP98101904.5

    申请日:1998-02-04

    IPC分类号: H01M4/62 H01M10/40 H01M10/38

    摘要: A cathode for a lithium secondary battery wherein the surface of the cathode (3) of which a composition containing a cathode active material, a conductive substance and a binder is supported on a current collector, is coated with at least one ion-permeable resin (4) selected from resins having a temperature of deflection under load (measured at 18.6 kg/cm 2 load according to JIS K 7207) not lower than 100 °C, provide a lithium secondary battery with high energy density having improved safety. Examples of such ion-permeable resin are: polyimides, polyamide-imides and aramides.

    摘要翻译: 一种用于锂二次电池的阴极,其中阴极(3)的表面包含阴极活性材料,导电物质和粘合剂的组合物负载在集电器上,涂覆有至少一种离子可渗透树脂( 4)选自具有不低于100℃的负载下的挠曲温度(根据JIS K 7207测量的18.6kg / cm 2负载)的树脂,提供具有改善的安全性的具有高能量密度的锂二次电池。 这种离子可渗透树脂的实例是:聚酰亚胺,聚酰胺 - 酰亚胺和芳族酰胺。

    Non-aqueous electrolyte lithium secondary battery
    7.
    发明公开
    Non-aqueous electrolyte lithium secondary battery 失效
    LithiumsekundärbatteriemitnichtwässrigemElektrolyt

    公开(公告)号:EP0756344A1

    公开(公告)日:1997-01-29

    申请号:EP96111843.7

    申请日:1996-07-23

    IPC分类号: H01M4/62

    CPC分类号: H01M4/621 H01M4/587

    摘要: A non-aqueous electrolyte lithium secondary battery, comprising a cathode containing, as active material, a material that can be doped/undoped with lithium ions, an anode containing, as active material, a carbonaceous material that can be doped/undoped with lithium ions, a separator interposed between the cathode and anode and an electrolyte prepared by dissolving lithium salt in an organic solvent, wherein the anode contains a polymer having carbonate groups represented by the structural formula [I]:
    said polymer having a number average molecular weight of not less than 300 and not more than 200,000.
    The cycle life and high-rate capacity of the lithium secondary battery are improved without reducing low-temperature capacity.

    摘要翻译: 一种非水电解质锂二次电池,其包含含有可掺杂/未掺杂锂离子的材料作为活性材料的阴极,含有可掺杂/未掺杂锂离子的碳质材料作为活性材料的阳极 插入在阴极和阳极之间的隔膜和通过将锂盐溶解在有机溶剂中而制备的电解质,其中阳极含有具有由结构式表示的碳酸酯基团的聚合物:CHEM>所述聚合物的数均分子量为 不低于300,不超过20万。 在不降低低温容量的情况下,锂二次电池的循环寿命和高速容量得到改善。