Abstract:
Zinc oxide coated with silicon oxide of the present invention is zinc oxide which is coated with silicon oxide wherein surfaces of zinc oxide particles are coated with silicon oxide coatings, and the coated zinc oxide particles comprises at least one element selected from a group consisting of Mg, Ca, and Ba.
Abstract:
Provided is silicon oxide-coated zinc oxide, which can inhibit a decrease in viscosity resulting from a carbomer in a case where the silicon oxide-coated zinc oxide is used in water-based materials, a composition containing silicon oxide-coated zinc oxide, and a cosmetic product. The silicon oxide-coated zinc oxide of the present invention contains zinc oxide particles and a silicon oxide coating on a surface of the zinc oxide particles, in which an electric conductivity of a water suspension of the silicon oxide-coated zinc oxide is 120 µS/cm or less.
Abstract:
Provided are a silicon oxide-coated zinc oxide, a method for producing the same, a composition and a cosmetic including a silicon oxide-coated zinc oxide. The silicon oxide-coated zinc oxide is a silicon oxide-coated zinc oxide formed by coating surfaces of zinc oxide particles with a silicon oxide coat, in which an average particle diameter of the zinc oxide particles is in a range of more than 50 nm and 500 nm or less, and, when an abundance ratio of silicon in the silicon oxide coat in a Q 3 environment is indicated by Q 3 , and an abundance ratio in a Q 4 environment is indicated by Q 4 , Q 3 +Q 4 ≥0.6 and Q 4 /(Q 3 +Q 4 )≥0.5 are satisfied.
Abstract:
Provided are a silicon-oxide-coated zinc oxide capable of suppressing the elution of zinc ions from zinc oxide particles, a method for manufacturing the same, a silicon-oxide-coated-zinc-oxide-containing composition, and a cosmetic. The silicon-oxide-coated zinc oxide is a silicon-oxide-coated zinc oxide formed by coating the surfaces of zinc oxide particles with a silicon oxide coating, in which the average particle diameter of the zinc oxide particles is in a range of 1 nm or more and 50 nm or less, when the abundance ratio of silicon in the silicon oxide coating in a Q 3 environment is indicated by Q 3 , and the abundance ratio in a Q 4 environment is indicated by Q 4 , Q 3 +Q 4 ≥0.6 and Q 4 /(Q 3 +Q 4 )≥0. 5, and furthermore, the decomposition ratio of Brilliant Blue generated by the photocatalytic activity of the zinc oxide particles is 3% or less.
Abstract:
Zinc oxide powder of the present invention contains zinc oxide particles, in which primary particles of the zinc oxide particles have a minor axis of 35 nm or more and 350 nm or less and have a Heywood diameter of 35 nm or more and 400 nm or less, and a coefficient of variation of a number distribution of the Heywood diameters of the primary particles of the zinc oxide powder is 50% or less.