摘要: A mixture of 100 parts by weight of zeolite powder, 0.1 to 20 parts by weight of β-1,3-glucan, a 1:1 layered clayey mineral, a 2:1 layered clayey mineral and a proper amount of water is kneaded to prepare a plasticizable molding composition of zeolite. The composition is molded by, for example, extrusion into a honeycomb structure and fired to give a fired honeycomb zeolite which is excellent in dimensional accuracy and mechanical strengths and useful as desiccant, catalyst, carrier therefor and so forth.