OPTICAL FIBER CORE AND OPTICAL FIBER TAPE CORE
    3.
    发明公开
    OPTICAL FIBER CORE AND OPTICAL FIBER TAPE CORE 审中-公开
    OPTISCHER FASERKERN UND OPTISCHER FASERBANDKERN

    公开(公告)号:EP2060941A1

    公开(公告)日:2009-05-20

    申请号:EP06810153.4

    申请日:2006-09-08

    IPC分类号: G02B6/44

    摘要: The present invention relates to an optical fiber accommodated in an optical fiber cable, and more particularly, to an optical fiber which optimizes optical fiber coating resin and color resin and restrains an increase in transmission loss of the optical fiber due to an operating environment and aged deterioration and provides an optical fiber and optical fiber ribbon without any increase of transmission loss irrespective of the operating environment and aged deterioration, and especially when exposed to water or high humidity.
    The optical fiber is an optical fiber coated with at least two layers of coating resin, wherein the outermost coated coating resin is a colored layer made of color resin and when the optical fiber is immersed in water which is heated to 60°C for 168 hours, an extraction rate of the coating resin of the optical fiber is set to 1.5 mass percent or below.

    摘要翻译: 本发明涉及容纳在光纤电缆中的光纤,更具体地说,涉及一种优化光纤涂层树脂和着色树脂的光纤,并且抑制由于操作环境和老化而导致的光纤的传输损耗的增加 劣化,并且不管操作环境和老化劣化,特别是当暴露于水或高湿度时,提供光纤和光纤带,而不会增加传输损耗。 光纤是涂覆有至少两层涂布树脂的光纤,其中最外涂层涂层树脂是由彩色树脂制成的着色层,当光纤浸入加热至60℃168小时的水中时 ,将光纤的涂布树脂的提取率设定为1.5质量%以下。

    OPTICAL FIBER CORE
    4.
    发明公开
    OPTICAL FIBER CORE 审中-公开
    FASEROPTISCHER KERN

    公开(公告)号:EP2253978A1

    公开(公告)日:2010-11-24

    申请号:EP09719756.0

    申请日:2009-02-16

    IPC分类号: G02B6/44

    摘要: A coated optical fiber of the present invention comprises a glass fiber coated by at least two coating layers (a soft layer and a hard layer), wherein the glass surface of the glass fiber, where the at least two coating layers of the optical fiber are removed, has a peak intensity ratio of 0.6 or more in C 3 H 7 O+(m/z 59) or C 4 H 9 O+(m/z 73) with respect to Si+(m/z 28) peak in cation analysis of TOF-SIMS. The fiber avoids any increase in its transmission loss even when it is exposed to a high-humidity environment or immersed in water.

    摘要翻译: 本发明的涂覆光纤包括由至少两个涂层(软层和硬层)涂覆的玻璃纤维,其中玻璃纤维的玻璃表面,其中光纤的至少两个涂层是 在阳离子分析中,相对于Si +(m / z 28)峰,C 3 H 7 O +(m / z 59)或C 4 H 9 O +(m / z 73)的峰强度比为0.6以上 TOF-SIMS。 即使在暴露于高湿度环境或浸入水中时,纤维也能避免传输损失的任何增加。

    OPTICAL FIBER CORE
    5.
    发明公开
    OPTICAL FIBER CORE 审中-公开
    纤芯

    公开(公告)号:EP2120075A1

    公开(公告)日:2009-11-18

    申请号:EP08721568.7

    申请日:2008-03-07

    IPC分类号: G02B6/44

    摘要: An optical fiber which reduces transmission loss increase even in a high humidity environment or under water is provided. To solve the above issue, an optical fiber according to the present invention comprises a glass optical fiber coated with at least two coating layers, soft and hard layers. The optical fiber is further coated by a colored resin to make a colored optical fiber. The hard layer and the color layer of the colored optical fiber have a free volume radius of at least 0.290nm according to positron annihilation lifetime spectroscopy.

    OPTICAL FIBER
    6.
    发明公开
    OPTICAL FIBER 审中-公开
    光纤

    公开(公告)号:EP2051119A1

    公开(公告)日:2009-04-22

    申请号:EP06796474.2

    申请日:2006-08-10

    IPC分类号: G02B6/44

    摘要: The present invention provides an optical fiber in which composites constructing its coating are not complicated, so, there is also little constraint in view of production, and, moreover, delamination between a glass optical fiber and a primary layer, and a bubble in the primary layer hardly arise. The optical fiber of the present invention is an optical fiber which has a glass optical fiber which has a core 1, which passes an optical signal, in a center portion, and a cladding 2 surrounding this, a primary protective layer 3 made to coat the glass optical fiber, a secondary protective layer 4 applied on this primary protective layer 3, and a third protective layer 5 applied to an outer periphery of this secondary protective layer 4, wherein glass transition temperature of the primary protective layer 3 is made to be higher than -20°C and 10°C or lower, glass transition temperature of the secondary protective layer 4 is made to be -10°C or less, and the glass transition temperature of the primary protective layer 3 is set higher than that of the secondary protective layer 4.

    摘要翻译: 本发明提供了一种光纤,其中构成其涂层的复合材料不复杂,因此从生产角度来看也几乎没有限制,此外,玻璃光纤与主层之间的分层以及主层中的气泡 层几乎不会出现。 本发明的光纤是具有玻璃光纤的光纤,该玻璃光纤具有在中央部分通过光信号的芯体1和包围其的包层2,主保护层3覆盖 玻璃光纤,在该一次保护层3上涂敷的二次保护层4,以及涂敷在该二次保护层4的外周上的第三保护层5,其中使一次保护层3的玻璃化转变温度更高 在-20℃以上,10℃以下的情况下,二次保护层4的玻璃化转变温度为-10℃以下,一次保护层3的玻璃化转变温度设定为比 次级保护层4。

    OPTICAL FIBER
    7.
    发明公开
    OPTICAL FIBER 审中-公开
    光纤

    公开(公告)号:EP2048529A1

    公开(公告)日:2009-04-15

    申请号:EP06782297.3

    申请日:2006-07-28

    IPC分类号: G02B6/44

    摘要: An optical fiber is provided, which is unlikely to cause interlayer delamination between a glass optical fiber and a primary coating layer even when it is immersed in water. The optical fiber of the present invention includes a glass optical fiber 1 consisting of a core and a cladding, a primary coating layer 2 overlaid on the glass optical fiber, and a secondary coating layer 3 overlaid on the primary coating layer, wherein the relaxation modulus of the secondary coating layer is set at 400 MPa or less.

    摘要翻译: 提供一种即使浸渍在水中也不会在玻璃光纤与一次被覆层之间产生层间剥离的光纤。 本发明的光纤包括由芯和包层组成的玻璃光纤1,覆盖在玻璃光纤上的第一覆盖层2和覆盖在第一覆盖层上的第二覆盖层3,其中松弛模量 设定为400MPa以下。