Method of manufacturing a fiber reinforced plastic armored cable
    1.
    发明公开
    Method of manufacturing a fiber reinforced plastic armored cable 失效
    纤维增强塑料铠装电缆及其制造工艺

    公开(公告)号:EP0461871A3

    公开(公告)日:1992-10-07

    申请号:EP91305285.8

    申请日:1991-06-12

    IPC分类号: G02B6/44

    摘要: In the manufacture of a fiber reinforced plastic armored cable, long reinforcing fibers (12) are impregnated with an uncured thermosetting resin (13) and formed into a predetermined shape to obtain a plurality of rod-like members with the thermosetting resin held uncured and then the uncured rod-like members are passed through a die of a melt (15) extruder, by which the rod-like members are each coated with a thermoplastic resin layer. The coated layers of the rod-like members are immediately cooled (16) to simultaneously form a plurality of fiber reinforced plastic armoring strands with the thermosetting resin held uncured. The armoring strands thus obtained are wound around a cable (A) which is fed while being rotated. The cable having wound thereon the strands is passed through a die portion of a melt extruder (21), by which the cable is sheathed with a thermoplastic resin layer which is immediately cooled (23) and solidified. The sheathed cable is guided into a curing tank (24) using a liquid as the heating medium to cure the thermosetting resin in the armoring strands. Thereafter, the sheathed cable is wound onto a drum (26) via a rotary take-up device.

    Method of manufacturing a fiber reinforced plastic armored cable
    5.
    发明公开
    Method of manufacturing a fiber reinforced plastic armored cable 失效
    用其制备的纤维增强塑料铠装电缆和过程。

    公开(公告)号:EP0461871A2

    公开(公告)日:1991-12-18

    申请号:EP91305285.8

    申请日:1991-06-12

    IPC分类号: G02B6/44

    摘要: In the manufacture of a fiber reinforced plastic armored cable, long reinforcing fibers (12) are impregnated with an uncured thermosetting resin (13) and formed into a predetermined shape to obtain a plurality of rod-like members with the thermosetting resin held uncured and then the uncured rod-like members are passed through a die of a melt (15) extruder, by which the rod-like members are each coated with a thermoplastic resin layer. The coated layers of the rod-like members are immediately cooled (16) to simultaneously form a plurality of fiber reinforced plastic armoring strands with the thermosetting resin held uncured. The armoring strands thus obtained are wound around a cable (A) which is fed while being rotated. The cable having wound thereon the strands is passed through a die portion of a melt extruder (21), by which the cable is sheathed with a thermoplastic resin layer which is immediately cooled (23) and solidified. The sheathed cable is guided into a curing tank (24) using a liquid as the heating medium to cure the thermosetting resin in the armoring strands. Thereafter, the sheathed cable is wound onto a drum (26) via a rotary take-up device.

    摘要翻译: 在纤维增强塑料铠装电缆的制造中,长的增强纤维与在未固化的热固性树脂浸渍,并形成为预定的形状,得到与热固性树脂保持未固化的棒状部件,然后将未固化的棒状部件的多元性 通过的熔融挤出机模头,通过该棒状构件的每个涂覆有热塑性树脂层传递。 棒状部件的涂覆层被立即冷却,以同时形成纤维的多根增强与保持未固化的热固性树脂的塑料铠装线股。 由此获得的铠装线料围绕电缆缠绕所有这一切在旋转的同时被馈送。 具有缠绕在其上的电缆线股是通过熔融挤出机,通过该电缆护套的热塑性树脂层中的所有被立即冷却并固化的部分通过。 的护套线被引导到使用液体作为所述热介质以固化在铠装丝的热固性树脂的固化箱。 那里之后,护套电缆通过旋转卷绕装置卷绕到鼓上。