摘要:
The invention provides a process for preparing a metal hydroxide comprising the steps of: (a) providing particles of a metal silicate; (b) mixing the particles with a mineral acid solution to obtain a slurry which comprises precipitated silica; (c) separating the precipitated silica from the slurry to obtain a remaining solution; (d) increasing the pH of the remaining solution to such an extent that a metal hydroxide is formed; (e) separating the metal hydroxide so obtained from the remaining solution; and (f) adding to the remaining solution obtained in step (e) an acid solution, thereby forming a salt containing solution, or (g) removing at least part of the base added in step (d) from the remaining solution obtained in step (e), thereby forming a salt containing solution.
摘要:
Disclosed herein are methods of forming a soil amendment from metal slag, the method may comprise: increasing sodium in a bentonite clay by reacting bentonite clay and sodium salt to provide ion-exchanged sodium bentonite clay, wherein the bentonite clay comprises both sodium and calcium; feeding carbon dioxide through a reactor containing a mixture of the metal slag and the ion-exchanged sodium bentonite clay; wherein sodium ions of the ion exchanged bentonite clay transfers the carbon dioxide to a calcium silicate phase of the metal slag; reacting the ion-exchanged sodium bentonite clay with calcium silicate to consume the sodium carbonate of the ion-exchanged sodium bentonite clay and provide sodium silicate and calcium carbonate; reacting the sodium silicate to provide sodium carbonate and silicon dioxide; and combining the calcium carbonate and silicon dioxide to form the soil amendment, wherein the metal slag is a calcium slag silicate.
摘要:
[Object] To provide a method for producing hollow nanoparticles each having a shell mainly including calcium silicate and having a particle size on the order of nanometers, where the method can freely control the particle size, shape, and shell thickness of the hollow nanoparticles. [Solution] The hollow nanoparticles are produced by performing a first step of forming a core-shell particle having a core particle containing calcium and, on a surface thereof, a coating layer including amorphous silica; a second step of hydrothermally converting the coating layer of the core-shell particle into a shell mainly including calcium silicate; and a third step of removing the core particle from the core-shell particle while allowing the shell of the core-shell particle to remain.
摘要:
The invention provides a process for preparing a metal hydroxide comprising the steps of: (a) providing particles of a metal silicate; (b) mixing the particles with a mineral acid solution to obtain a slurry which comprises precipitated silica; (c) separating the precipitated silica from the slurry to obtain a remaining solution; (d) increasing the pH of the remaining solution to such an extent that a metal hydroxide is formed; and (e) separating the metal hydroxide so obtained from the remaining solution.