CONDUCTIVE PRIMER MIX
    3.
    发明公开
    CONDUCTIVE PRIMER MIX 失效
    LEITFÄHIGEZÜNDMITTELMISCHUNG

    公开(公告)号:EP1040088A4

    公开(公告)日:2000-11-08

    申请号:EP97912641

    申请日:1997-07-07

    IPC分类号: C06B41/02 C06C7/00

    CPC分类号: C06C7/00 C06B41/02

    摘要: Electrically ignitable conductive primer mixture comprising aluminum and carbon black and having reduced tetrazene, the mixture also containing lead styphnate, antimony sulfide and barium nitrate.

    摘要翻译: 包含铝和炭黑并具有还原四苯的电可燃导电底漆混合物,该混合物还含有斯蒂芬酸铅,硫化锑和硝酸钡。

    Conducting primer compositions
    4.
    发明公开
    Conducting primer compositions 失效
    引导原料组合物

    公开(公告)号:EP0372893A3

    公开(公告)日:1990-08-29

    申请号:EP89312639.1

    申请日:1989-12-04

    发明人: Bentley, John R.

    IPC分类号: C06C7/00 C06B41/02 C06B23/00

    CPC分类号: C06C7/00 C06B23/00 C06B41/02

    摘要: A conducting composition for detonators having insen­sitivity to one amp of current or one watt of power con­sisting of 40 to 80 percent by weight of lead styphnate, 2 to 10 percent by weight of carbon black and/or graphite and the balance lead oxide or other exposive or non-explosive material. Firing times of less than eight milliseconds can be achieved where at least one percent of graphite is included in the composition.

    Conducting primer compositions
    5.
    发明公开
    Conducting primer compositions 失效
    Stromleitende ZusammensetzungfürInitialladung。

    公开(公告)号:EP0372893A2

    公开(公告)日:1990-06-13

    申请号:EP89312639.1

    申请日:1989-12-04

    发明人: Bentley, John R.

    IPC分类号: C06C7/00 C06B41/02 C06B23/00

    CPC分类号: C06C7/00 C06B23/00 C06B41/02

    摘要: A conducting composition for detonators having insen­sitivity to one amp of current or one watt of power con­sisting of 40 to 80 percent by weight of lead styphnate, 2 to 10 percent by weight of carbon black and/or graphite and the balance lead oxide or other exposive or non-explosive material. Firing times of less than eight milliseconds can be achieved where at least one percent of graphite is included in the composition.

    摘要翻译: 一种用于雷管的导电组合物,其对一次电流或一瓦特功率不敏感,其由40-80重量%的硫酸铅,2-10重量%的炭黑和/或石墨组成,余量为氧化铅或其它曝光 或非爆炸材料。 在组合物中至少含有1%石墨的情况下,可以达到少于8毫秒的发射时间。