맥반석 건조 모르타르의 제조방법
    41.
    发明公开
    맥반석 건조 모르타르의 제조방법 有权
    矿石碎屑的制备方法

    公开(公告)号:KR1020000055929A

    公开(公告)日:2000-09-15

    申请号:KR1019990004838

    申请日:1999-02-11

    发明人: 강재훈

    IPC分类号: C04B28/16 C04B33/00 C04B28/14

    摘要: PURPOSE: A method is to provide a dry mortar comprising mineral stone containing no cement as a principal component. The dry mortar can be used together with a proper amount of water for floor or wall materials of the buildings. CONSTITUTION: A preparation method includes pulverizing mineral stones alone without addition of cement; washing the mineral stone powder in the range of 8 to 60 mesh with water; and drying the washed mineral stone powder to have a moisture content of less than 8%. The particule mineral stone is mixed with a mixed gypsum of gypsum plaster, natural gypsum, gypsum retarder and anhydrous gypsum at a mixing ratio of 6-7 : 10. The mixture is then mixed with water to have a weak alkaline pH value and a compaction strength of more than 80 kilograms per square centimeter.

    摘要翻译: 目的:提供一种包含不含水泥的矿石作为主要成分的干砂浆。 干砂浆可以与适量的水一起用于建筑物的地板或墙壁材料。 构成:一种制备方法,包括单独粉碎矿石,不加水泥; 用水冲洗8至60目的矿物石粉; 并将经洗涤的矿石粉末干燥,使含水量低于8%。 颗粒矿石与混合石膏石膏,天然石膏,石膏缓凝剂和无水石膏以6-7:10的混合比混合。然后将混合物与水混合以具有弱碱性pH值和压实 实力超过80公斤每平方厘米。

    기능성 재료용 조성물
    42.
    发明公开
    기능성 재료용 조성물 失效
    功能材料组成

    公开(公告)号:KR1020000013579A

    公开(公告)日:2000-03-06

    申请号:KR1019980032524

    申请日:1998-08-11

    申请人: 윤여경

    发明人: 양대모

    IPC分类号: C04B33/00

    摘要: PURPOSE: A composition for functional materials is effective as a functional material and available in the form of powder for immediate use. CONSTITUTION: A composition for functional material comprises:A first hypogene granite powder consisting 79.76 wt.% of SiO2, 9.87 wt.% of Al2O3, 0.21 wt.% of Fe2O3, 3.79 wt.% of K2O, 2.81 wt.% of Na2O, 1.59 wt.% of CaO, 0.86 wt.% of MgO, and 1.11 wt.% of other microingredients containing 0.5-2.0 ppm of germanium; A second hypogene granite powder consisting 73.41 wt.% of SiO2, 14.56 wt.% of Al2O3, 1.13 wt.% of Fe2O3, 4.13 wt.% of K2O, 2.48 wt.% of Na2O, 2.28 wt.% of CaO, 0.72 wt.% of MgO, and 1.29 wt.% of other microingredients containing 0.5-2.0 ppm of germanium; A third hypogene granite powder consisting 73.53 wt.% of SiO2, 12.52 wt.% of Al2O3, 4.76 wt.% of Fe2O3, 3.78 wt.% of K2O, 2.07 wt.% of Na2O, wt.% of CaO, 0.51 wt.% of MgO, and 1.27 wt.% of other microingredients containing 0.5-2.0 ppm of germanium; A forth hypogene granite powder consisting 51.42 wt.% of SiO2, 9.16 wt.% of Al2O3, 1.87 wt.% of Fe2O3, 4.18 wt.% of K2O, 3.74 wt.% of Na2O, 4.17 wt.% of CaO, 14.19 wt.% of MgO, and 8.27 wt.%; and a fifth hypogene granite powder consisting 79.89 wt.% of SiO2, 14.92 wt.% of Al2O3, 0.31 wt.% of Fe2O3, 1.24 wt.% of K2O, 0.64 wt.% of Na2O, 1.89 wt.% of CaO, 0.17 wt.% of MgO, and 0.94 wt.% of other microingredients.

    摘要翻译: 目的:功能材料的组合物作为功能材料是有效的,可以立即使用粉末形式。 构成:用于功能材料的组合物包括:第一次生成花岗岩粉末,其包含79.76重量%的SiO 2,9.87重量%的Al 2 O 3,0.21重量%的Fe 2 O 3,3.79重量%的K 2 O,2.81重量%的Na 2 O, CaO的1.59重量%,MgO的0.86重量%和含有0.5-2.0ppm锗的其它微量粒子的1.11重量% 第二种致畸花岗岩粉末由73.41重量%的SiO 2,14.56重量%的Al 2 O 3,1.13重量%的Fe 2 O 3,4.13重量%的K 2 O,2.48重量%的Na 2 O,2.28重量%的CaO,0.72重量% %的MgO和1.29重量%的其它含有0.5-2.0ppm锗的微量元素; 第三种原位花岗岩粉末由73.53重量%的SiO 2,12.52重量%的Al 2 O 3,4.76重量%的Fe 2 O 3,3.78重量%的K 2 O,2.07重量%的Na 2 O,CaO的重量%,0.51重量% %的MgO和1.27重量%的其它含有0.5-2.0ppm的锗的微量粒料; 第四次生成花岗岩粉末由51.42重量%的SiO 2,9.16重量%的Al 2 O 3,1.87重量%的Fe 2 O 3,4.18重量%的K 2 O,3.74重量%的Na 2 O,4.17重量%的CaO,14.19重量% %的MgO和8.27重量%; 和第五种原生花岗岩粉末,其组成为:79.89重量%的SiO 2,14.92重量%的Al 2 O 3,0.31重量%的Fe 2 O 3,1.24重量%的K 2 O,0.64重量%的Na 2 O,1.89重量%的CaO,0.17 MgO的重量百分数和0.94重量%的其它微量染料。

    기능성 흙벽돌
    43.
    发明公开
    기능성 흙벽돌 无效
    功能性土砖

    公开(公告)号:KR1020000003905A

    公开(公告)日:2000-01-25

    申请号:KR1019980025208

    申请日:1998-06-30

    申请人: 한봉수 이상태

    发明人: 한봉수 이상태

    IPC分类号: E04C1/00 C04B33/00

    摘要: PURPOSE: A functional soil brick is provided to affect good effects to human body by the ingredients emitted from the functional ingredients. CONSTITUTION: A functional soil brick is composed of more than 2 kinds of ingredients 5-25wt% among loess 75-95wt%, elvan, bio-ceramics, rice-straw, lime and wormwood powder and so on; a making method has the steps of: mixing the each ingredients powder, and adding water and then inputting into a brick forming mold to form, and drying.

    摘要翻译: 目的:功能性土壤砖由功能成分发出的成分影响人体的良好效果。 构成:功能性土砖由黄土75-95wt%,埃尔文,生物陶瓷,稻草,石灰和蒿木粉等2种以上5-25wt%的成分组成; 制造方法具有以下步骤:将各成分粉末混合,加入水,然后输入砖形模具中以形成和干燥。

    생약재 함유 흙벽돌
    44.
    发明公开
    생약재 함유 흙벽돌 无效
    含有自然天然药物的土壤

    公开(公告)号:KR1020000003904A

    公开(公告)日:2000-01-25

    申请号:KR1019980025207

    申请日:1998-06-30

    申请人: 한봉수 이상태

    发明人: 한봉수 이상태

    IPC分类号: E04C1/00 C04B33/00

    摘要: PURPOSE: A soil brick is provided to affect good effects to human body by the ingredients emitted from loess, elvan, natural medicines. CONSTITUTION: A soil brick is composed of: natural medicines including loess 56-88wt%, Korean angelica root, wormwood, peony, peppermint, licorice root, aromatic trees, cinnamon; elvan 0.5-2.5wt%; lime 0.5-2.5wt%; white clay 0.5-2.5wt%; hardwood charcoal powder 0.5-2.5wt%.

    摘要翻译: 目的:提供土壤砖,以通过黄土,埃尔文,天然药物排放的成分对人体产生良好的影响。 构成:土砖由天然药物,包括黄土56-88wt%,韩国当归,蒿木,牡丹,薄荷,甘草根,芳香树,肉桂; 埃尔万0.5-2.5重量%; 石灰0.5-2.5重量%; 白土0.5-2.5重量%; 硬木炭粉0.5-2.5重量%。

    황토(黃土)를 주재로 한 물 정화용 볼의 제조방법
    46.
    发明公开
    황토(黃土)를 주재로 한 물 정화용 볼의 제조방법 失效
    黄土地主要材料制造方法水净化炮弹球

    公开(公告)号:KR1019990045947A

    公开(公告)日:1999-06-25

    申请号:KR1019990006389

    申请日:1999-02-25

    申请人: 손병덕

    发明人: 손병덕

    CPC分类号: Y02W30/92

    摘要: 본발명은종래에생활용수나식수로사용하는수도물은댐이나저수지에서물을저장하였다가상수원수로공급받아정수장에서정화처리하여가정의물탱크나아파트단지에서는지하저장소에유입시킨후 사용하는과정을거치게되었던바상수원수의수질은고도의산업화과정에서생성되는각종중금속, 농약, 세균등으로많이오염된저급수상태이므로수용가에서는수도물을기피하는현실에서생수를고가로구입하여식수및 용수로사용하므로서경제적으로부담이되는등의폐단을해소하기위해황토분말, 맥반석분말에참나무톱밥을배합비로혼합반죽하여금형틀에서동일형상의황토볼을형성건조한후 900℃의가열로에서고체화된 완제품을제조하여물탱크내에침전시켜물속에함유된중금속및 유해한성분을황토분, 맥반석분, 참숯이해독, 분해, 수질을정화하여깨끗한물을제공해주므로서건강증진에큰 기여를할 수있도록한 것임.

    황토흙 풀반죽
    47.
    发明公开
    황토흙 풀반죽 无效
    赭色面团池面团

    公开(公告)号:KR1019990042712A

    公开(公告)日:1999-06-15

    申请号:KR1019970063609

    申请日:1997-11-27

    申请人: 변정훈

    发明人: 변정훈

    IPC分类号: C04B33/00

    摘要: 황토흙을 건축자재로 쓰기 위하여 물을 넣어 곱게 반죽하여 벽돌을 찍어 내어 실험을 해보면 모서리 부분같은 곳이 잘 깨지고 부스러기가 생겨 건축하는데 적당치 않아 황토흙으로 벽돌을 찍어도 일반 세멘벽돌 처럼 잘 부서지지 않도록 연구실험을 해오던중 황토흙 반죽을 밀가루로 풀을쑤어(풀의 농도는 벽지가 잘붙을 정도로) 물대신 상용해 보았더니 벽돌이 단단하고 모서리 부분쪽이 부서지지 않고 부스러기가 생기지 않고 벽돌면이 대패로 나무를 다듬어 놓은것처럼 매끈하고, 옷이나 손에 묻지 않았습니다.
    방바닥에도 두껍게 깔고 흙손으로 곱게 손질을 해보았더니 매끈하고 충격을 가하여도 흙부스러기가 생기지 않았으며, 한지를 바르고 콩기름을 먹였더니 별도로 장판을 깔 필요가 없었습니다.
    또 천정에도 그물망을 치고 붙여 보았더니 잘 붙고 떨어지지 않았습니다. 벽돌들을 만들어 칸막이를 끼웠다 빼내었다 할 수 있도록하여 모래와 세멘트를 물로 반죽한 세멘벽돌 재료를 넣고 한쪽에는 황토흙을 풀로 반죽한 재료를 넣어 1차 압력을 가한후 칸막이를 빼내고 2차 압력을 가한후 벽돌을 빼내어 건조시켜 보았더니 시멘트와 황토흙이 한덩어리가 되어 단단하게 부착이 되어 건축자재로 적합하며, 황토흙을 풀로 반죽하여 사용해보니 각종 건축자재로도 사용하는데 적합한 유용한 발명인 것이다.

    황토매트의 제조방법
    48.
    发明公开
    황토매트의 제조방법 失效
    黄土垫的制造方法

    公开(公告)号:KR1019990041705A

    公开(公告)日:1999-06-15

    申请号:KR1019970062350

    申请日:1997-11-24

    申请人: 이용호

    发明人: 이용호

    IPC分类号: C04B33/00

    摘要: 본 발명은 황토 매트의 제조방법에 관한 것으로서, 방취, 방균과 습도조절 및 원적외선방사 기능이 있는 황토와 맥반석 및 원적외선 방사세라믹을 혼합하여 만든 것이다.
    본 발명은 종래의 황토 매트가 각종 배합제의 사용에도 불구하고 쉽게 부서지는 단점이 있는데 반하여, 견고한 상태가 오래 유지될 뿐만 아니라, 방취, 방균, 습도조절 및 원적외선의 방사로 쾌적한 수면상태의 유지와 인체의 혈액순환을 원활하게 하여 주는 효과를 얻을 수가 있다.

    직화구이용 금강약돌 숯
    49.
    发明公开
    직화구이용 금강약돌 숯 无效
    烤火炭烧烤

    公开(公告)号:KR1019990012112A

    公开(公告)日:1999-02-25

    申请号:KR1019970035390

    申请日:1997-07-26

    申请人: 함이규

    发明人: 함이규

    IPC分类号: C04B33/00

    摘要: 본 발명은 육고기를 불에 구울때 가스화로의 불꽃을 원적외선 복사열로 변환시켜 육고기의 겉과 속을 균일하고 신속하게 익힐 수 있도록 금강약돌가루와 내열소지가루를 물과 적정량으로 혼합하여 일정한 형체로 성형한 후 고온에서 고형체로 소결하여 금강약돌 숯으로 형성하여 이를 가스화로의 상부에 균일하게 깔아 놓고 그 상부에서 육고기를 구우면 가스불꽃이 금강약돌 숯에서 원적외선 복사열로 변환되어 고기의 겉과 속이 균일하고 신속하게 익을 뿐 아니라 육고기의 내부기름기가 밖으로 유출시켜 육고기의 맛을 담백하게 하는 직화구이용 금강약돌 숯

    적벽돌 제조방법
    50.
    发明授权
    적벽돌 제조방법 失效
    制备红砖的工艺

    公开(公告)号:KR100169206B1

    公开(公告)日:1999-01-15

    申请号:KR1019960001351

    申请日:1996-01-23

    发明人: 김승남

    IPC分类号: C04B33/00 C04B33/04 C04B35/00

    摘要: 본원 발명의 목적은 시각적으로 외표면이 자연미를 가지며 시멘트를 사용하여 적층시 결속력을 증대시킬 수 있는 적벽돌의 제조방법을 제공하는데 있다.
    상기한 목적을 달성하기 위한 본 발명은 점토 75~90% 중량비와 파쇄된 장석 10~25% 중량비를 혼합하여 벽돌모양으로 성형한 후 적어도 일측표면의 점토를 긁어내어 장석들이 외부로 드러나게 돌출시키며 건조로에서 80~150℃의 열풍을 공급하여 20~40시간 건조시킨 후 소성로에서 1150~1250℃에서 30~50시간 소성시키므로써 벽돌표면으로 돌출된 장석의 외표면이 녹으면서 둥글둥글하게 돌출된 상태가 되도록하는 적벽돌의 제조방법을 요지로 한다.