摘要: A concrete anticorrosive is provided to prevent corrosion of concrete and extend a life of concrete while removing sulfur ions present in an organic material and neutralizing sulfate ions as a strong base. A concrete anticorrosive is prepared by dissolving 5-20wt% of copper ions and 5-20wt% of nickel ions in water. The concrete anticorrosive further comprises liquid sodium hydroxide or/and potassium hydroxide. The sodium hydroxide or potassium hydroxide is contained in an amount of 10-50wt%. The copper ion is at least one selected from copper nitrate, copper bromide, copper chloride, and copper sulfate. The nickel ion is at least one selected from nickel acetate, nickel bromide, nickel chloride, nickel iodide, nickel nitrate, and nickel sulfate.
摘要翻译: 提供混凝土防腐蚀以防止混凝土的腐蚀,并延长混凝土的使用寿命,同时去除存在于有机材料中的硫离子并中和作为强碱的硫酸根离子。 通过将5-20wt%的铜离子和5-20wt%的镍离子溶解在水中来制备混凝土防腐蚀剂。 混凝土防腐剂还包含液体氢氧化钠或/和氢氧化钾。 氢氧化钠或氢氧化钾的含量为10-50重量%。 铜离子是选自硝酸铜,溴化铜,氯化铜和硫酸铜中的至少一种。 镍离子是选自乙酸镍,溴化镍,氯化镍,碘化镍,硝酸镍和硫酸镍中的至少一种。
-
公开(公告)号:KR101006829B1
公开(公告)日:2011-01-12
申请号:KR1020080099388
申请日:2008-10-10
申请人: (주)대우건설 , 충청대학교 산학협력단 , 한국기술개발 주식회사 , 주식회사 동아기술공사 , 주식회사 도우엔지니어즈
摘要: 본 발명은 콘크리트 공시체를 넣은 용기의 일측에 형성된 통공을 통하여 공기 압축기와 진공 펌프를 이용하여 물을 분사하고, 용기의 또 다른 일측에 형성 된 통공을 통하여 이산화탄소(CO
2 )를 주입하여 콘크리트 공시체의 중성화 촉진을 테스트하는 방법을 제공하는 것이다. 이때, 물을 0~50℃ 범위의 것을 사용할 수 있고, 물 분사는 노즐 출구의 지름을 10~200㎛ 범위로 조절하여 사용할 수 있으며, 이산화탄소의 주입은 용기내의 CO
2 내부압이 0.1~900토르(torr) 범위로 조정하여 사용할 수도 있다. 여기에서, 물 주입은 분당 1ℓ~2ℓ로 하여 분사할 수 있고, 분사시간은 공시체의 크기 등에 따라 게이지를 통해 조절하면 되고, 이산화탄소의 주입 역시 주입구 측의 압력 게이지를 통해 설정 압력으로 주입하면 된다. 물론 주입된 물은 테스트 종료 후 하부의 통구를 통해 회수하여 재사용 하거나 폐기할 수도 있다.-
公开(公告)号:KR1020090052294A
公开(公告)日:2009-05-25
申请号:KR1020080115895
申请日:2008-11-20
申请人: (주)대우건설 , 충청대학교 산학협력단 , 한국기술개발 주식회사 , 주식회사 동아기술공사 , 주식회사 도우엔지니어즈 , (주)아텍스
摘要: 콘크리트 방식 혼화제에 관한 것으로, 지하에 매설되는 콘크리트 구조물 중의 하수관로와 같이 항상 습기를 유지하면서 음식물 찌꺼기 또는 기타의 유기물과 접촉된 상태에서 열화의 진행이 쉽게 진행되는 구조물을 보호할 수 있는 콘크리트용 방식 혼화제가 개시된다. 본 발명에 의하면, 콘크리트 방식용 혼화제로서, 2-클로로페놀, 4-브로모페놀, 2,4-디클로로페놀에서 선택된 1종 이상을 포함하는 콘크리트 방식용 혼화제를 제공함으로써 그 목적을 달성할 수 있다.
-
公开(公告)号:KR101176774B1
公开(公告)日:2012-08-23
申请号:KR1020080115895
申请日:2008-11-20
申请人: (주)대우건설 , 충청대학교 산학협력단 , 한국기술개발 주식회사 , 주식회사 동아기술공사 , 주식회사 도우엔지니어즈 , (주)아텍스
摘要: 콘크리트 방식 혼화제에 관한 것으로, 지하에 매설되는 콘크리트 구조물 중의 하수관로와 같이 항상 습기를 유지하면서 음식물 찌꺼기 또는 기타의 유기물과 접촉된 상태에서 열화의 진행이 쉽게 진행되는 구조물을 보호할 수 있는 콘크리트용 방식 혼화제가 개시된다. 본 발명에 의하면, 콘크리트 방식용 혼화제로서, 2-클로로페놀, 4-브로모페놀, 2,4-디클로로페놀에서 선택된 1종 이상을 포함하는 콘크리트 방식용 혼화제를 제공함으로써 그 목적을 달성할 수 있다.
-
公开(公告)号:KR101151778B1
公开(公告)日:2012-06-01
申请号:KR1020080115896
申请日:2008-11-20
申请人: (주)대우건설 , 충청대학교 산학협력단 , 한국기술개발 주식회사 , 주식회사 동아기술공사 , 주식회사 도우엔지니어즈 , (주)아텍스
摘要: 조습성능이강한콘크리트용혼화제가개시된다. 본발명에의하면, 시멘트와조습성이강한천연물또는인공물을혼합하여혼화제로사용하는데, 펄라이트, 펄프, 질석, 분쇄된짚, 숯중에서 1종이상을선택하여혼화제로사용함으로써그 목적을달성하게된다.
-
公开(公告)号:KR1020100040343A
公开(公告)日:2010-04-20
申请号:KR1020080099388
申请日:2008-10-10
申请人: (주)대우건설 , 충청대학교 산학협력단 , 한국기술개발 주식회사 , 주식회사 동아기술공사 , 주식회사 도우엔지니어즈
摘要: PURPOSE: A method for testing neutralization promotion of concrete is provided to protect and repair concrete by concrete degradation. CONSTITUTION: A method for testing concrete neutralization promotion comprises: a step of injecting water to one side of a container having concrete through a through hole; and a step of injecting carbon dioxide through other through hole. The water temperature is 0-50°C. The injection of water is performed using air compressor or vacuum pump. The pressure of carbon dioxide is 0.1~900 Torr. The injected water after test is reused of disposed.
摘要翻译: 目的:提供混凝土中和促进试验方法,通过具体退化对混凝土进行保护和修复。 构成:用于测试混凝土中和促进的方法包括:通过通孔向具有混凝土的容器的一侧注入水的步骤; 以及通过其他通孔注入二氧化碳的步骤。 水温为0-50°C。 使用空气压缩机或真空泵进行水的注入。 二氧化碳的压力为0.1〜900乇。 试验后注入的水被重新利用处置。
-
公开(公告)号:KR100810027B1
公开(公告)日:2008-03-07
申请号:KR1020060105126
申请日:2006-10-27
申请人: (주)대우건설 , 충청대학교 산학협력단 , 주식회사 도우엔지니어즈 , 한국기술개발 주식회사 , 주식회사 동아기술공사
CPC分类号: C04B20/1062 , C04B40/0039 , C04B2103/61 , C04B2111/0081 , Y02W30/92 , Y02W30/94 , C04B14/28 , C04B14/34 , C04B18/08 , C04B18/141 , C04B28/02 , C04B2103/0013 , C04B2103/0016
摘要: An anti-corrosive admixture for concrete is provided to prevent corrosion of concrete when being added to concrete, and thus increase a service life of concrete. An anti-corrosive admixture for concrete is prepared by mixing 5-20wt% of a copper ion-containing compound, 5-20wt% of a nickel ion-containing compound, 2-10wt% of a metal powder, and 30-50wt% of an admixture material. The admixture material is at least one selected from fly ash, blast furnace slag, and limestone powder. The copper ion-containing compound is at least one selected from copper acetate, copper cyanide, and copper fluoride. The nickel ion-containing compound is at least one selected from nickel carbonate and nickel hydroxide. Further, the metal powder is at least one selected from Fe, Al, Zn, Mg or Sn.
摘要翻译: 提供混凝土防腐外加剂,以防止混凝土在混凝土中的腐蚀,从而增加混凝土的使用寿命。 通过混合5-20重量%的含有铜离子的化合物,5-20重量%的含镍离子的化合物,2-10重量%的金属粉末和30-50重量%的金属粉末混合物来制备混凝土的防腐蚀混合物, 外加材料。 混合材料是选自飞灰,高炉矿渣和石灰石粉末中的至少一种。 含铜离子的化合物是选自乙酸铜,氰化铜和氟化铜中的至少一种。 含镍离子的化合物是选自碳酸镍和氢氧化镍中的至少一种。 此外,金属粉末是选自Fe,Al,Zn,Mg或Sn中的至少一种。
-
公开(公告)号:KR1020090052295A
公开(公告)日:2009-05-25
申请号:KR1020080115896
申请日:2008-11-20
申请人: (주)대우건설 , 충청대학교 산학협력단 , 한국기술개발 주식회사 , 주식회사 동아기술공사 , 주식회사 도우엔지니어즈 , (주)아텍스
CPC分类号: C04B14/18 , C04B14/202 , C04B16/02 , C04B18/068 , C04B20/026 , C04B28/02
摘要: 조습성능이 강한 콘크리트용 혼화제가 개시된다. 본 발명에 의하면, 시멘트와 조습성이 강한 천연물 또는 인공물을 혼합하여 혼화제로 사용하는데, 펄라이트, 펄프, 질석, 분쇄된 짚, 숯 중에서 1종 이상을 선택하여 혼화제로 사용함으로써 그 목적을 달성하게 된다.
-
公开(公告)号:KR1020110129062A
公开(公告)日:2011-12-01
申请号:KR1020100048478
申请日:2010-05-25
申请人: 충청대학교 산학협력단
CPC分类号: G01N17/002 , G01N3/60 , G01N33/383 , G01N2203/0226 , G01N2203/0228
摘要: PURPOSE: A concrete degradation accelerator is provided to realize the environmental conditions in a test chamber by a temperature/humidity control unit, CO2 concentration control unit, and a water spraying unit and perform various test related to the degradation of concrete under various environmental conditions. CONSTITUTION: A concrete degradation accelerator comprises a test chamber, an operating unit, a temperature/humidity control unit, a CO2 concentration control unit, a water spraying unit, a pressure control unit, and a display unit. The test chamber comprises an opening/closing unit and can hold concrete specimen. The operating unit sets environmental conditions and a pattern to control the environmental conditions. The temperature/humidity control unit compares the conditions input to the operating unit with information transferred from the temperature/humidity sensor to control temperature and relative humidity in the test chamber.
摘要翻译: 目的:通过温度/湿度控制单元,CO2浓度控制单元和喷水单元,实现试验箱内的环境条件,并对各种环境条件下混凝土的降解进行各种试验。 构成:具体的劣化加速器包括测试室,操作单元,温度/湿度控制单元,CO 2浓度控制单元,喷水单元,压力控制单元和显示单元。 测试室包括开/关单元,并且可以容纳混凝土样品。 操作单元设置环境条件和控制环境条件的模式。 温度/湿度控制单元将输入到操作单元的条件与从温度/湿度传感器传送的信息进行比较,以控制测试室中的温度和相对湿度。
-
公开(公告)号:KR101180325B1
公开(公告)日:2012-09-07
申请号:KR1020100048478
申请日:2010-05-25
申请人: 충청대학교 산학협력단
摘要: 본 발명은 계절 변화에 따른 여러가지 환경조건을 조절하여 콘크리트의 열화(劣化)를 촉진시킴으로써 이후의 내구성을 측정할 수 있도록 하는 장치에 관한 것으로서, 온도, 습도, 공기 중 CO
2 농도, 압력, 염류량 등의 조건에 따른 콘크리트의 중성화, 동결융해, 염해 등의 진행경과를 파악할 수 있도록 하는 콘크리트 열화 촉진기에 관한 것이다.
본 발명은 전술한 과제의 해결을 위해 개폐수단을 구비하고 콘크리트 공시체를 수용하도록 구성된 시험챔버; 상기 시험챔버 내의 환경조건과 환경조건제어 패턴을 설정하는 조작부; 상기 조작부에 입력된 조건과 온습도센서에서 전달하는 정보를 비교하여, 상기 시험챔버 내부의 온도와 상대습도를 조절하는 온습도 조절장치; 상기 조작부에 입력된 조건과 CO
2 센서에서 전달하는 정보를 비교하여, 상기 시험챔버 내부의 CO
2 농도를 조절하는 CO
2 농도 조절장치; 상기 조작부에 입력된 조건에 따라 상기 시험챔버 내부에 물을 분사하는 물분사장치; 상기 조작부에 입력된 조건과 압력센서에서 전달하는 정보를 비교하여, 상기 시험챔버 내부의 압력을 조절하는 압력조절장치; 및 상기 시험챔버 내부의 실시간 환경조건과 환경조건의 변화 패턴을 나타내는 디스플레이부; 를 포함하여 구성되는 콘크리트 열화 촉진기를 제공한다.
-
-
-
-
-
-
-
-
-