염화실리케이트계 형광체 및 그 제조 방법
    3.
    发明公开
    염화실리케이트계 형광체 및 그 제조 방법 有权
    氯硅酸盐及其制备方法

    公开(公告)号:KR1020140047635A

    公开(公告)日:2014-04-22

    申请号:KR1020140033446

    申请日:2014-03-21

    摘要: The present invention relates to a chlorosilicate based fluorescent body containing rare-earth metals and a production method of the same, and specifically, to a chlorosilicate based fluorescent body containing rare-earth metals having an effect of emitting light in long wavelengths using large ion radius of chlorine elements, and a production method of the same. The production method comprises the following steps: obtaining a metal salt-SiO2 sol mixture solution by mixing a metal salt mixture solution containing metal chloride for synthesizing the chlorosilicate based fluorescent body containing the rare-earth metals with SiO2 sol in a liquid phase; impregnating the metal salt-SiO2 sol mixture solution in a polymer material before drying the mixture; and performing low temperature calcination, pre-oxidation burning, and post-reduction burning processes to obtain the chlorosilicate based fluorescent body. [Reference numerals] (AA) Metal solution, water-soluble silicon compound(WSS); (BB) Immersion(cellulose); (CC) Stirring, grinding, and drying under ultrasound; (DD) First sintering(150-400째C, air); (EE) Second sintering(500-1000째C, air); (FF) 700-1400째C, sintering under reduction; (GG) Fluorescent body

    摘要翻译: 本发明涉及含有稀土金属的氯硅酸盐系荧光体及其制造方法,具体而言,涉及具有使用大离子半径的长波长发光效果的稀土金属的氯硅酸盐系荧光体 的氯元素及其制造方法。 该制备方法包括以下步骤:通过混合含有金属氯化物的金属盐混合物溶液来合成含有稀土金属的氯硅酸盐基荧光体与SiO 2溶胶在液相中来获得金属盐-SiO 2溶胶混合物溶液; 在混合物干燥之前将金属盐-SSiO 2溶胶混合物溶液浸渍在聚合物材料中; 进行低温煅烧,预氧化,后还原燃烧等工序,得到氯硅酸系荧光体。 (附图标记)(AA)金属溶液,水溶性硅化合物(WSS); (BB)浸渍(纤维素); (CC)在超声波下搅拌,研磨和干燥; (DD)第一次烧结(150-400℃,空气); (EE)第二烧结(500-1000℃,空气); (FF)700-1400℃C,还原烧结; (GG)荧光体

    염화실리케이트계 형광체 및 그 제조 방법
    7.
    发明公开
    염화실리케이트계 형광체 및 그 제조 방법 有权
    氯硅酸盐及其制备方法

    公开(公告)号:KR1020140049533A

    公开(公告)日:2014-04-25

    申请号:KR1020140033448

    申请日:2014-03-21

    IPC分类号: C09K11/79 C09K11/77

    摘要: The present invention relates to a chlorosilicate based fluorescent body containing rare-earth metals and a production method of the same, and specifically, to a chlorosilicate based fluorescent body containing rare-earth metals having an effect of emitting light in long wavelengths using large ion radius of chlorine elements, and a production method of the same. The obtained chlorosilicate based fluorescent body has a composition of M-Si-O-Cl, M-Si-B-O-Cl, M-Si-Al-O-Cl, or M-Si-P-O-Cl, wherein M is selected from the group consisting of alkali metal, alkali earth metal, transition metals, the rare-earth metal, and a combination thereof. [Reference numerals] (AA) Metal solution, water-soluble silicon compound(WSS); (BB) Immersion(cellulose); (CC) Stirring, grinding, and drying under ultrasound; (DD) First sintering(150-400째C, air); (EE) Second sintering(500-1000째C, air); (FF) 700-1400째C, sintering under reduction; (GG) Fluorescent body

    摘要翻译: 本发明涉及含有稀土金属的氯硅酸盐系荧光体及其制造方法,具体而言,涉及具有使用大离子半径的长波长发光效果的稀土金属的氯硅酸盐系荧光体 的氯元素及其制造方法。 获得的氯硅酸盐基荧光体具有M-Si-O-Cl,M-Si-BO-Cl,M-Si-Al-O-Cl或M-Si-PO-Cl的组成,其中M选自 由碱金属,碱土金属,过渡金属,稀土金属组成的组及其组合。 (附图标记)(AA)金属溶液,水溶性硅化合物(WSS); (BB)浸渍(纤维素); (CC)在超声波下搅拌,研磨和干燥; (DD)第一次烧结(150-400℃,空气); (EE)第二烧结(500-1000℃,空气); (FF)700-1400℃C,还原烧结; (GG)荧光体

    알칼리토 금속을 포함하는 알루미네이트계 산화물 형광체 및 그의 분말 제조 방법
    10.
    发明公开
    알칼리토 금속을 포함하는 알루미네이트계 산화물 형광체 및 그의 분말 제조 방법 有权
    包括碱金属金属的铝酸盐及其制备方法

    公开(公告)号:KR1020110002446A

    公开(公告)日:2011-01-07

    申请号:KR1020100063597

    申请日:2010-07-01

    IPC分类号: C09K11/64 C09K11/55

    摘要: PURPOSE: A method for preparing aluminate phosphors including alkaline earth metals is provided to prepare phosphor powder with a nano-submicron, uniform particle size distribution, and excellent luminous efficiency. CONSTITUTION: A method for preparing aluminate phosphors including alkaline earth metals comprises the steps of: impregnating a metal salt solution including alkaline-earth metal salt and aluminum salt in a polymer; and firing the precursor in a furnace preheated to the temperature of 500-1000 °C for a short time and again firing the precursor in a reducing atmosphere at a temperature of 1000-1500 °C.

    摘要翻译: 目的:提供一种制备包括碱土金属在内的铝酸盐荧光体的方法,以制备具有纳米亚微米,粒度分布均匀,发光效率优良的荧光体粉末。 构成:用于制备包括碱土金属的铝酸盐荧光体的方法包括以下步骤:在聚合物中浸渍包括碱土金属盐和铝盐的金属盐溶液; 并在预热至500-1000℃的炉中短时间焙烧前体,再次在1000-1500℃的还原气氛中焙烧前体。