公开(公告)号:KR1020160145618A
公开(公告)日:2016-12-20
申请号:KR1020167029711
申请日:2015-04-22
Applicant: 쌩-고벵 글래스 프랑스
Inventor: 자니오에리크 , 쁘띠피에르-올리비에 , 블랑샤벵자망
CPC classification number: C03C25/1095 , C03B19/06 , C03C3/118 , C03C8/06 , C03C8/16 , C03C13/00 , C03C25/42 , C03C2207/00 , C03C2213/00 , C03C2218/17 , B32B17/02 , B32B17/067 , B32B38/145 , B32B2260/021 , B32B2262/101 , B32B2315/085
Abstract: 본발명은하기연속단계: (a) 유리패브릭에유리프릿의층을적층하는단계이며, 여기서프릿의유리와패브릭의유리가본질적으로동일한조성을갖는것인단계; (b) 유리프릿의층을, 프릿의층을유리패브릭과동일한조성을갖는에나멜층으로전환시키기에충분히긴 시간동안온도 T > T- 20℃ (여기서 T은유리프릿의리틀톤온도임)에노출시키기위해, 유리섬유를가열하는단계; 및 (c) 단계 (b)에서수득된, 에나멜로함침되거나에나멜층을지지하는유리섬유를냉각시켜유리시트를수득하는단계를포함하는, 편평유리의제조방법에관한것이다. 본발명은또한상기방법에의해수득될수 있는유리시트에관한것이다.
Abstract translation: 它还涉及能够通过该方法获得的玻璃板。
-
公开(公告)号:KR1020150100662A
公开(公告)日:2015-09-02
申请号:KR1020157015960
申请日:2013-12-20
Applicant: 쌩-고벵 이조베르
CPC classification number: C03B5/027 , C03B37/04 , C03B37/09 , C03C3/062 , C03C3/064 , C03C3/087 , C03C3/091 , C03C3/097 , C03C13/06 , C03C2213/00
Abstract: 본 발명은 Fe
2 O
3 형태로 표시되는 산화철 3 중량% 이상을 포함하는 화학적 조성의 유리를 제조하는 방법으로서, 용융 유리 중에 침지된 전극을 사용하여, 망가니즈가 +2보다 높은 산화 상태로 존재하는 1종 이상의 망가니즈 운반체를 함유하는 유리화가능한 원료 혼합물을 전기 용융시키는 단계를 포함한다.-
3.PREPARATION OF BOROSILICATE FIBER GLASS BATCHES FOR LONG FIBER CONTAINING CULLET OF TFT-LCD SUBSTRATE GLASS 有权
Title translation: 用于含TFT-LCD基板玻璃杯的长纤维的玻璃纤维玻璃批料的制备公开(公告)号:KR100917269B1
公开(公告)日:2009-09-16
申请号:KR20090001173
申请日:2009-01-07
Applicant: IND ACADEMIC COOP
Inventor: KIM KI DONG , LEE SEUNG HEUN
IPC: C03C6/02
CPC classification number: C03C1/002 , C03C3/04 , C03C2213/00
Abstract: A composition of borosilicate-based long glass fiber batches containing cullet of TFT-LCD substrate glass is provided to lower a melting temperature without the chemical and chemicophysical deterioration of glass. A composition of borosilicate-based long glass fiber batches containing cullet of TFT-LCD substrate glass includes 3-65 parts of TFT-LCD cullet on a basis of 100 parts of pyrophylite among batch composition. Aside from TFT-LCD cullet, the batch composition is composed of 100 parts of pyrophylite, 9-17 parts of colemanite, 52-75 parts of limestone, 3-8 parts of borax and 0.5-1.5 parts of Natrii sulfas.
Abstract translation: 提供含有TFT-LCD基板玻璃碎玻璃的硼硅酸盐长玻璃纤维批料组合物,以降低熔融温度,而不会导致玻璃的化学和化学物理性能下降。 含有TFT-LCD基板玻璃碎玻璃的硼硅酸盐长玻璃纤维组合物的组合物包括在批量组成中基于100份叶蜡石的3-65份TFT-LCD碎玻璃。 除了TFT-LCD碎玻璃之外,批量组成由100份叶蜡,9-17份石灰石,52-75份石灰石,3-8份硼砂和0.5-1.5份硝基硫酸钠组成。
-
公开(公告)号:KR20180011785A
公开(公告)日:2018-02-02
申请号:KR20177036413
申请日:2016-03-07
CPC classification number: C03C13/00 , C03C3/095 , C03C2213/00
Abstract: 본발명은고탄성계수유리섬유조성물및 그유리섬유와복합재료를제공한다. 그중, 유리섬유조성물의각 성분의함량은중량백분비로, SiO55-64%,AlO13-24%,YO0.1-6%,CaO 3.4-10.9%,MgO 8-14%,CaO+MgO+SrO 0.26로표시한다. 이조성물은유리의탄성계수를현저히제고시키고, 유리의결정화경향을효과적으로억제하고, 유리의액상선온도를저하시켜, 비교적이상적인△T치를얻을수 있으며, 특히고탄성계수유리섬유의탱크가마화생산에적합하다.
Abstract translation: 本发明提供高模量玻璃纤维组合物和玻璃纤维及其复合材料。 其中,按重量百分比,SiO55-64%,AlO13-24%,YO0.1-6%,CaO的3.4-10.9%的MgO 8-14%,CaO的+ MgO的+的SrO <涉及的玻璃纤维组合物的各成分的含量 LIO +的NaO + KO <2%,二氧化钛<2%,FeO的<1.5%,22%表示为LaO0-1.2%,且重量百分比C1 =(LIO +的NaO + KO)的比例/(YO + LAO) 范围表示为> 0.26。 失谐圣是和显著提高玻璃的弹性模量,以有效地抑制玻璃的结晶化倾向和降低玻璃的液相线温度,并且是较理想的△Ť获得的值,特别适合的罐炉花生产的高弹性模量的玻璃纤维的 我会的。
-
公开(公告)号:KR1020140109929A
公开(公告)日:2014-09-16
申请号:KR1020147018740
申请日:2012-02-01
Applicant: 벨 제임스 달톤
Inventor: 벨제임스달톤
IPC: G02B6/02
CPC classification number: G02B6/02395 , C03C3/04 , C03C13/045 , C03C13/046 , C03C2201/31 , C03C2213/00 , G02B1/00 , G02B6/02 , G02B6/028 , G02B6/0281 , G02B6/0286 , G02B2006/12061
Abstract: 고순도 유리로 형성된 클래딩 층 또는 고순도 동위원소 비율 변경 유리로 형성된 클래딩 층을 가지고 있고, 고순도 동위원소 비율 변경 유리로 된 코어를 가지고 있는 광 도파로로서, 코어 유리의 굴절률이 클래딩 유리의 굴절률보다 더 크고, 상기 고순도 동위원소 비율이 변경된 코어 물질은 상기 코어의 모든 실리콘 원자의 최대 4.447% Si-29(원자/원자) 또는 상기 코어의 적어도 4.90%의 Si-29(원자/원자) 원자의 Si-29 동위원소 비율을 나타내거나, 또는 상기 코어의 모든 게르마늄 원자의 최대 7.2% Ge-73 (원자/원자) 또는 상기 코어 영역의 게르마늄 원자의 적어도 8.18%의 Ge-73 (원자/원자)의 Ge-73 동위원소 비율을 나타내는 광 도파로.
-
6.PREPARATION OF SODA LIME BOROSILICATE GLASS BATCHES FOR GLASS WOOL CONTAINING CULLET OF TFT-LCD SUBSTRATE GLASS 有权
Title translation: 含有TFT-LCD基板玻璃的玻璃纤维的玻璃纤维玻璃瓶的制备公开(公告)号:KR100929869B1
公开(公告)日:2009-12-04
申请号:KR20090001174
申请日:2009-01-07
Applicant: IND ACADEMIC COOP
Inventor: KIM KI DONG , LEE SEUNG HEUN
CPC classification number: C03C13/006 , C03C1/002 , C03C13/06 , C03C2213/00 , C03C2214/14
Abstract: PURPOSE: A soda lime borosilicate-based monofilament glass badge composition is provided to lower melting point and to prevent the deterioration of the physicochemical properties of glass even by using the broken glass of a TFT LCD glass substrate. CONSTITUTION: A soda lime borosilicate-based monofilament glass badge composition comprises 3 ~ 55 parts by weight of the broken glass of TFT LCD based on 100 parts by weight of silica, quartzite or a mixture of silica and quartzite. The composition comprises further 45 ~ 54 parts by weight of soda ash, 7 ~ 23 parts by weight of colemanite, 1.5 ~ 2.5 parts by weight of limestone, 17 ~24 parts by weight of dolomite, and 0.5 ~ 1.5 parts by weight of Mirabilite based on 100 parts by weight of silica, quartzite or a mixture of silica and quartzite.
Abstract translation: 目的:提供基于钠钙硼硅酸盐的单丝玻璃徽章组合物以降低熔点,并且通过使用TFT LCD玻璃基板的碎玻璃来防止玻璃的物理化学性质的劣化。 构成:基于钠钙硼硅酸盐的单丝玻璃徽章组合物包含基于100重量份二氧化硅,石英岩或二氧化硅和石英岩的混合物的3〜55重量份的TFT LCD的碎玻璃。 该组合物还包含45〜54重量份的苏打灰,7〜23重量份的氯硅藻土,1.5〜2.5重量份的石灰石,17〜24重量份的白云石和0.5〜1.5重量份的紫晶 基于100重量份的二氧化硅,石英岩或二氧化硅和石英岩的混合物。
-
公开(公告)号:KR20180011786A
公开(公告)日:2018-02-02
申请号:KR20177036424
申请日:2016-03-21
CPC classification number: C03C13/00 , C03C3/095 , C03C2213/00
Abstract: 본발은고성능유리섬유조성물및 그유리섬유와복합재료를제공한다. 그중, 유리섬유조성물의각 성분의함량은중량백분비로, SiO53-64%,AlO>19%,
Abstract translation: 主要部分提供高性能玻璃纤维组合物及其玻璃纤维和复合材料。 其中,玻璃纤维组合物的各成分的含量包含,按重量百分比,SiO53-64%,的AlO> 19%,<25%,YO + LAO + GdO0.05-7%,LIO +的NaO + KO≤1%,CaO的 + MgO + SrO 10-24%,CaO 1.5-12%,TiO 2 <2%和FeO <1.5%。 该制备大大提高了玻璃的弹性模量和化学稳定性,克服了容器中难以生产高性能玻璃,传统高性能玻璃结晶风险高的问题, 并且在相同条件下显着降低玻璃的结晶速度,特别适用于化学稳定性优良的高性能玻璃纤维槽罐玻璃的生产。
-
公开(公告)号:KR1020170141803A
公开(公告)日:2017-12-26
申请号:KR1020177035232
申请日:2015-10-15
Applicant: 주시 그룹 코., 엘티디.
CPC classification number: C03C13/00 , C03C3/087 , C03C3/091 , C03C3/112 , C03C3/118 , C03C2213/00 , C03C13/046
Abstract: 본발명은고성능유리섬유조성물및 유리섬유와복합재료를제공한다. 유리섬유조성물의각 성분의함유량은중량백분율로, SiO58 ~ 62%,AlO14 ~ 18%,CaO+MgO 20 ~ 24.5%,CaO>14%,LiO0.01 ~ 0.4%,NaO+KO
Abstract translation: 本发明提供高性能玻璃纤维组合物和玻璃纤维及复合材料。 玻璃纤维组合物的各成分的含量,SiO58〜62%为重量百分比,AlO14〜18%,CaO的+ MgO的20〜24.5%,CaO的> 14%,LiO0.01〜0.4%,的NaO + KO <2%, 的TiO <3.5%,FeO的<1%,F <由1%表示时,非C1 =的CaO /重量百分比范围的MgO是具有C1是大于2,2.6 gwagat或更小,重量百分比比率C2 =的SiO / CaO的范围是3.3至4.3。 失谐化合物nophyeo机械强度显著给和软化玻璃纤维的温度,并同时降低玻璃的高温粘度,从而有效地抑制玻璃的结晶化倾向和降低玻璃的液相温度,即使在大规模罐窑生产 这是合适的。
-
9.유리 제품, 발광 물질 입자들을 갖는 유리 제품, 유리 제품을 제조하기 위한 장치, 유리 제품을 제조하기 위한 방법 및 발광 물질 입자들을 갖는 유리 제품을 제조하기 위한 방법 审中-实审
Title translation: 具有用于制造玻璃制品的玻璃制品的方法和用于生产具有发光 - 物质颗粒的玻璃物品的方法的玻璃物质玻璃物品公开(公告)号:KR1020160124206A
公开(公告)日:2016-10-26
申请号:KR1020167025884
申请日:2015-02-12
Applicant: 오스람 오엘이디 게엠베하
Inventor: 베루스,토마스
CPC classification number: H01L51/5268 , C03B5/173 , C03C11/00 , C03C13/04 , C03C14/004 , C03C14/006 , C03C2213/00 , C03C2214/04 , C03C2214/16 , C03C2214/34 , C09K11/025 , H01L33/501 , H01L51/56 , H01L31/04
Abstract: 본발명은상이한실시예들에서유리제품(200)과관련이있으며, 상기유리제품(200)은표면을구비한유리매트릭스, 제 1 유형의입자(208) 및적어도하나의제 2 유형의입자(210)를포함하고, 이때제 2 유형의입자들(210)은제 1 유형의입자들(208)보다더 높은굴절률을갖고, 이때상기제 1 유형의입자들(208)은상기유리매트릭스(204)에의해완전히둘러싸임으로써, 결과적으로상기유리매트릭스(204)의표면에는상기제 1 유형의입자들(208)이없고, 그리고상기유리제품(200)의굴절률을높이기위해, 상기제 1 유형의입자들(208) 위의및/또는사이의상기제 2 유형의입자(210)들은적어도부분적으로상기유리매트릭스(204) 내에서상기유리매트릭스(204)의표면에배치되어있다.
-
10.
公开(公告)号:KR101652140B1
公开(公告)日:2016-08-29
申请号:KR1020117017002
申请日:2009-12-21
Applicant: 오씨브이 인텔렉츄얼 캐피탈 엘엘씨
CPC classification number: C03C13/00 , C03B5/235 , C03B5/43 , C03B7/06 , C03B7/065 , C03B37/04 , C03B2207/60 , C03B2211/00 , C03C3/085 , C03C3/087 , C03C3/091 , C03C2213/00 , C08J5/043 , C08J2300/00 , F23C5/08 , F23M2900/05004 , Y02P40/55 , Y02P40/57
Abstract: 백금또는다른귀금속재료가실질적으로포함되지않는유리용융장치에서고강도유리섬유를성형하는방법, 이방법에의해만들어지는생성물, 및이 방법에사용되기에적합한원료조합조성물이개시된다. 본발명에서사용되는일 유리조성물은 50 ∼ 75 중량%의 SiO, 13 ∼ 30 중량%의 AlO, 5 ∼ 20 중량%의 MgO, 0 ∼ 10 중량%의 CaO, 0 ∼ 5 중량%의 RO (이때, RO 는 LiO, NaO 및 KO 의합) 를포함하고, 높은섬유화온도 (예컨데 2400 ∼ 2900 ℉ (1316 ∼ 1593 ℃)) 및/또는섬유화온도보다적어도 45 ℉ (25 ℃) 만큼낮은액상화온도를가진다. 본발명의방법에서사용되는다른유리조성물은최대약 64 ∼ 75 중량%의 SiO, 16 ∼ 24 중량%의 AlO, 8 ∼ 12 중량%의 MgO, 및 0.25 ∼ 3 중량%의 RO (이때, RO 는 LiO, NaO 및 KO 의합) 으로구성되고, 약 2650 ℉ (1454 ℃) 미만의섬유화온도및 적어도 80 ℉ (45 ℃) 의ΔT 를가진다. 용융된유리를유리용융장치 (10) 로부터성형위치로전송하기위한전로 (12) 가제공된다. 백금또는다른귀금속재료를실질적으로사용하지않은용광로및/또는전로를사용함으로써, 귀금속재료로라이닝처리된용융용광로를사용하여생상되는섬유의비용과비교하여유리섬유의생산비용이현저히줄어든다. 또한, 고강도유리섬유를포함하는고강도복합재료제품이개시된다.
-
-
-
-
-
-
-
-
-