토사, 산업폐기물, 해사와 사막모래의 경화체 및 그것의 제조방법
    2.
    发明授权
    토사, 산업폐기물, 해사와 사막모래의 경화체 및 그것의 제조방법 有权
    包含土壤,工业废物,海洋沙粒和沙沙的硬化材料及其制备方法

    公开(公告)号:KR100988151B1

    公开(公告)日:2010-10-18

    申请号:KR1020100036826

    申请日:2010-04-21

    摘要: PURPOSE: A hardened material of earth sand, industrial wastes, sea sand, and desert sand, and a manufacturing method thereof are provided to improve the density, the intensity, and the elasticity of the material by adding a hardener. CONSTITUTION: A hardened material contains 20~32 parts of magnesium chloride by weight, 20~32 parts of sodium chloride by weight, 15~28 parts of potassium chloride by weight, 10~19 parts of calcium chloride by weight, 2~8 parts of sodium sulfate by weight, 1~10 parts of sodium triphosphate by weight, and 1.5~7 parts of lignosulfonate by weight. The hardened material comprise more than one mixture selected from the group consisting of earth sand, industrial wastes, sea sand, and desert sand.

    摘要翻译: 目的:提供土砂,工业废物,海砂,沙漠沙的硬化物及其制造方法,通过添加硬化剂来提高材料的密度,强度和弹性。 构成:硬化材料含有20〜32重量份氯化镁,20〜32重量份氯化钠,15〜28重量份氯化钾,10〜19重量份氯化钙,2〜8份 的硫酸钠,1〜10重量份的三磷酸钠和1.5〜7重量份的木质素磺酸钠。 硬化材料包含多于一种选自土砂,工业废物,海砂和沙漠沙的混合物。

    지반 그라우트 및 충전재용 무기 결합재
    4.
    发明公开
    지반 그라우트 및 충전재용 무기 결합재 有权
    无机粘合剂用于弱接地布线和插入材料

    公开(公告)号:KR1020130077380A

    公开(公告)日:2013-07-09

    申请号:KR1020110146059

    申请日:2011-12-29

    申请人: (주)한일

    摘要: PURPOSE: An inorganic binder for a weak ground grout and an insert material is provided to reduce the amount of Portland cement used, to prevent environmental problems such as the generation of carbon dioxide, and to reduce the excessive use of limestone. CONSTITUTION: An inorganic binder for a weak ground grout and an insert material consists of 15-25 wt% of cement, 50-75 wt% of fly ash, 9-20 wt% of bypass dust, and 1-5 wt% of water-soluble polymer. The fly ash has a fineness of 4000-5000 cm^2/g. The water-soluble polymer is one or a mixture of two or more selected from polyacrylate, cellulose, polyvinylalcohol, and polyacrylamide. [Reference numerals] (AA) Content of portland cement; (BB) Concentration of CO_2 in the atmosphere

    摘要翻译: 目的:为了减少硅酸盐水泥的使用量,为了防止生成二氧化碳等环境问题,减少了石灰石的过度使用,提供了弱底泥浆和嵌入材料的无机粘合剂。 构成:用于弱地层砂浆和嵌入材料的无机粘合剂由15-25重量%的水泥,50-75重量%的飞灰,9-20重量%的旁路粉尘和1-5重量%的水组成 可溶性聚合物。 飞灰的细度为4000-5000cm ^ 2 / g。 水溶性聚合物是选自聚丙烯酸酯,纤维素,聚乙烯醇和聚丙烯酰胺中的一种或两种以上的混合物。 (附图标记)(AA)波特兰水泥的含量; (BB)大气中CO_2的浓度

    비백화성의 시멘트질 모르타르 조성물
    10.
    发明公开
    비백화성의 시멘트질 모르타르 조성물 失效
    非破坏性细胞组织

    公开(公告)号:KR1020070110540A

    公开(公告)日:2007-11-19

    申请号:KR1020077022962

    申请日:2006-03-09

    IPC分类号: C04B28/14 C04B28/06 C04B28/04

    摘要: The invention provides a non-efflorescing cementitious mortar composition, free of reactive silica material, in the form of a dry-mortar composition or an aqueous mortar composition, comprising a) from 1% by weight to 10% by weight of ordinary portland cement, based on the dry weight of the cementitious mortar composition b) from 1% by weight to 30% by weight of calcium aluminate cement, based on the dry weight of the cementitious mortar composition c) from 1% by weight to 15% by weight of calcium sulfate, based on the dry weight of the cementitious mortar composition and d) from 0.5% by weight to 30% by weight, based on the dry weight of the cementitious mortar composition, of an aqueous polymer dispersion or a water-redispersible polymer powder of polymers based on one or more monomers from the group consisting of vinyl esters, (meth) acrylates, vinyl aromatics, olefins, 1,3-dienes and vinyl halides and, if required, further monomers copolymerizable therewith.