公开(公告)号:KR1020100050212A
公开(公告)日:2010-05-13
申请号:KR1020080109393
申请日:2008-11-05
申请人: 나형우
CPC分类号: C04B41/5035 , C04B41/009 , C04B2111/00017 , C04B2111/20 , C04B2111/2023 , C04B2111/23 , C04B2111/27 , C09D1/02 , C04B41/5024 , C04B41/4582 , C04B41/4922 , C04B2103/40 , C04B28/00 , C04B28/001
摘要: PURPOSE: An inorganic ceramic waterproof agent for concrete waterproof, protection, and reinforcement is provided to pass air and to prevent infiltration of water with acid resistance, weather resistance, and alkali resistance. CONSTITUTION: A ceramic waterproof agent for protecting and reinforcing concreate cotnaisn 0.1-5 weight parts of silicon dioxide, 2-8 weight parts of hydrogen silicide, 40-60 weight parts of distilled water, and 1-3 weight parts of surfactant based on 33-43 weight parts of silicate. Preferably, the ceramic waterproof agent contains 3 weight parts of silicon dioxide, 5 weight parts of hydrogen silicide,, 50 weight parts of distilled water, and 2 weight parts of surfactant based on 38 weight parts of silicate.
摘要翻译: 目的:提供用于混凝土防水,防护和加固的无机陶瓷防水剂,以通风,防止耐酸,耐候,耐碱性的水渗透。 构成:用于保护和加固混合物的陶瓷防水剂0.1-5重量份二氧化硅,2-8重量份氢化硅,40-60重量份蒸馏水和1-3重量份基于33的表面活性剂 -43重量份硅酸盐。 优选地,陶瓷防水剂含有3重量份二氧化硅,5重量份氢化硅,50重量份蒸馏水和2重量份基于38重量份硅酸盐的表面活性剂。
-
公开(公告)号:KR1020170023157A
公开(公告)日:2017-03-02
申请号:KR1020177002252
申请日:2015-06-24
申请人: 씨알 미네랄즈 컴파니, 엘엘씨
发明人: 토마스,조셉이얼 , 카터,리차드더글라스 , 위든,제프레이알렉산더
IPC分类号: C04B7/13 , C04B28/02 , C04B18/08 , C04B40/00 , C04B103/00 , C04B111/20 , C04B111/21
CPC分类号: C04B18/088 , C04B14/14 , C04B18/08 , C04B28/02 , C04B40/0039 , C04B2111/2015 , C04B2111/2023 , C04B2111/21 , C04B2111/26 , Y02W30/92 , Y02W30/94 , C04B7/13 , C04B28/021 , C04B2103/0088 , C04B2201/50 , C04B14/106 , C04B14/16 , C04B14/18 , C04B14/22 , C04B18/023 , C04B18/141 , C04B18/146
摘要: 비사양플라이애시에천연또는다른포졸란의추가는 F급또는 C급플라이애시로써 ASTM C618 및 AASHTO 295 하에인증받을수 있는정도까지상기비사양플라이애시의특성을상당히향상시킨다는것이뜻밖에발견되었다. 상기천연포졸란은부석또는펄라이트와같은화산분출물이될 수있다. 다른포졸란은또한이러한선광공정에사용될수 있다. 많은포졸란은실험적으로시험되었고비사양플라이애시를인증할수 있는 F급플라이애시로선광하는데사용될수 있다. 게다가, 본발명은 C급플라이애시를더욱가치가큰 F급플라이애시로변환하는방법을제공한다. 이러한발견은 F급플라이애시공급감소를연기할것이고비사양플라이애시폐기물스트림을콘크리트, 모르타르및 그라우트를보호하고향상시키는가치있고, 인증된플라이애시포졸란으로바꿀것이다.
摘要翻译: 已经意外地发现,将非规格飞灰添加到天然或其他火山灰中可显着地改善非规格飞灰的性能,使其可以根据ASTM C618和AASHTO 295认证为F类 或C级飞灰。 天然火山灰可能是火山喷发,如浮石或珍珠岩。 其他火山灰也可用于该选矿过程。 许多火山灰经过实验测试,可用于将非规格飞灰粉碎成可验证的F级粉煤灰。 此外,本公开提供了将C类飞灰转化为更有价值的F级飞灰的方法。 这一发现将扩大F级飞灰供应的减少,并将非规格飞灰废物流转化为有价值的,经过认证的飞灰火山灰,这将保护和增强混凝土,砂浆和灌浆。
-
公开(公告)号:KR1020100056607A
公开(公告)日:2010-05-28
申请号:KR1020080115486
申请日:2008-11-20
申请人: 쌍용양회공업(주)
CPC分类号: C04B28/04 , C04B2111/00215 , C04B2111/00318 , C04B2111/1025 , C04B2111/2023 , Y02W30/92 , C04B7/52 , C04B14/28 , C04B18/08 , C04B22/143 , C04B24/122 , C04B28/02 , C04B22/10 , C04B2103/52
摘要: PURPOSE: A cement composition for inhibition of alkali silica reaction and a manufacturing method thereof are provided, which can remarkably improve alkali silica reaction inhibition effect by mixing fly ash, limestone, and triisopropanolamine. CONSTITUTION: A cement composition for inhibition of alkali silica reaction comprises: clinker 100.0 parts by weight in which the total alkali content is 1.2% or less; fly ash 10-40 parts by weight in which the total alkali content is 3.0% or less, ignition loss is 4% or less, and SiO2+Al2O3+Fe2O3 content is 70% or greater; limestone 1-10 parts by weight in which the CaCO3 content is 80% or greater; and triisopropanolamine 0.005-0.1 parts.
摘要翻译: 目的:提供一种用于抑制碱二氧化硅反应的水泥组合物及其制造方法,其可以通过混合飞灰,石灰石和三异丙醇胺来显着提高碱二氧化硅反应抑制效果。 构成:用于抑制碱性二氧化硅反应的水泥组合物包括:熟料100.0重量份,其中总碱含量为1.2%以下; 总碱含量为3.0%以下的粉煤灰10-40重量份,灼烧损失为4%以下,SiO 2 + Al 2 O 3 + Fe 2 O 3为70%以上。 石灰石1-10重量份,其中CaCO 3含量为80%以上; 和三异丙醇胺0.005-0.1份。
-
公开(公告)号:KR100975477B1
公开(公告)日:2010-08-11
申请号:KR1020080109393
申请日:2008-11-05
申请人: 나형우
CPC分类号: C04B41/5035 , C04B41/009 , C04B2111/00017 , C04B2111/20 , C04B2111/2023 , C04B2111/23 , C04B2111/27 , C04B41/4582 , C04B41/4922 , C04B41/5024 , C04B2103/40 , C04B28/00 , C04B28/001
摘要: 본 발명은 콘크리트의 방수, 보호, 보강을 위한 콘크리트 침투형, 친환경, 무기질의 세라믹 방수제에 관한 것으로, 규산염 33 내지 43 중량부에 대해서, 이산화규소 0.1 내지 5중량부, 규화수소 2 내지 8중량부, 증류수 40 내지 60중량부, 계면활성제 1 내지 3중량부가 균일하게 혼합, 용해된 세라믹 방수제를 구성하여, 콘크리트 제품, 콘크리트 구조물은 물론, 점토 벽돌 및 기타 다양한 무기성 재질의 모재에 상기 세라믹 방수제를 다수회 도포하여, 세라믹 방수제를 모재 내부로 침투시킨 뒤에, 양생하고 건조하는 방수 시공을 함에 따라, 상기 모재에 침투된 세라믹 방수제가 공극을 메우고, 모재 표면에는 방수층이 형성되어, 모재로의 물의 침투는 막고, 공기는 통과하며, 방수 시공된 모재를 방수, 보호 및 보강을 하고, 방수 시공 후의, 내산성, 내후성, 내알카리성 내구성이 우수하며, 비휘발성 및 무취, 무해한 세라믹 방수제로, 친환경적이고 작업성이 우수한 것이다.
세라믹, 방수제, 무기질, 친환경, 콘크리트 침투, 보호, 보강, 규산염, 내후성-
公开(公告)号:KR100971226B1
公开(公告)日:2010-07-20
申请号:KR1020100014996
申请日:2010-02-19
申请人: 최상릉 , 이종인 , 김기현 , 노재호 , (주)제이엔티아이엔씨
CPC分类号: C04B28/02 , C04B28/16 , C04B2111/0075 , C04B2111/2023 , Y02W30/92 , Y02W30/94 , C04B18/08 , C04B18/141 , C04B20/008 , C04B22/064 , C04B22/143 , C04B2103/22 , C04B7/00
摘要: PURPOSE: A salt resistant cement mixture for paving and repairing a road is provided to prevent chlorides from penetrating into concrete for road pavement by improving an air gap structure of the concrete and to prevent the expansion of the concrete due to a reaction of alkali and aggregates by reducing alkali amount of the concrete. CONSTITUTION: A salt resistant cement mixture for paving and repairing a road includes 30-50 weight% of cement, 20-40 weight% of blast furnace slag micropowder,10-30 weight% of fly ash, 0.5-5 weight% of industrial calcium hydroxide, 3-10 weight% of anhydrite, 0.05-1 weight% of a setting retarder, and 1-10 weight% of admixture having high strength. The industrial calcium hydroxide is white powder which is obtained after a reaction of quicklime(CaO) and water.
摘要翻译: 目的:提供一种用于铺路修复的耐盐水泥混合物,以防止氯化物通过改善混凝土的气隙结构而渗入混凝土中,防止混凝土由于碱和骨料的反应而膨胀 通过减少混凝土的碱量。 构成:用于铺路修复的耐盐水泥混合物包括30-50重量%的水泥,20-40重量%的高炉渣微粉,10-30重量%的飞灰,0.5-5重量%的工业钙 氢氧化物,3-10重量%的无水石膏,0.05-1重量%的固化缓凝剂和1-10重量%的具有高强度的混合物。 工业氢氧化钙是在生石灰(CaO)与水反应后得到的白色粉末。
-
公开(公告)号:KR101899969B1
公开(公告)日:2018-09-18
申请号:KR1020180074843
申请日:2018-06-28
申请人: 석성기업주식회사
发明人: 강정용
IPC分类号: C04B22/06 , C04B24/04 , C04B24/38 , C04B111/20 , C04B103/65 , C04B103/30 , C04B111/74 , C04B103/00
CPC分类号: C04B22/06 , C04B24/04 , C04B24/38 , C04B2103/0001 , C04B2103/34 , C04B2103/65 , C04B2111/2023 , C04B2111/74
摘要: 본발명은콘크리트용복합항알칼리제와이를이용한콘크리트구조체에관한것으로, 그목적은콘크리트구조물또는콘크리트구조체에적용되어, 백화현상및 부식발생을방지하고, 내구성및 강도를증진시킬수 있는콘크리트용복합항알칼리제와이를이용한콘크리트구조체를제공하는것이다. 본발명에따른콘크리트용복합항알칼리제는, 반응성이산화규소 20∼35wt%, 가용성금속비누계방수제 15∼25wt%, 메타카올린(metakaolin) 20∼30wt%, 폴리카르복실레이트감수제 3∼10wt%, 헥사메타인산나트륨(sodium hexameta phosphate) 1∼5wt%, 물(증류수) 15∼30wt% 로이루어져있으며, 이와같은복합항알칼리제는콘크리트구조체의형성시, 시멘트 100 중량부에대하여, 3∼20 중량부첨가되도록되어있다.
-
公开(公告)号:KR100909212B1
公开(公告)日:2009-07-23
申请号:KR1020080034658
申请日:2008-04-15
申请人: 한국건설기술연구원 , 강원대학교산학협력단 , (주)삼우아이엠씨 , 한국도로공사
CPC分类号: C04B28/02 , C04B28/10 , C04B2111/00293 , C04B2111/00448 , C04B2111/0075 , C04B2111/2015 , C04B2111/2023 , C04B2111/2038 , Y02W30/92 , C04B18/088 , C04B22/064 , C04B7/02
摘要: A concrete composition for pavement repairing is provided to show excellent resistance to sulfate while reducing hydration heat and permeability and to suppress an alkali aggregate reaction. A concrete composition for pavement repairing comprises: 17-19wt% of binder containing 85-90wt% of ultra-rapid hardening cement and 10-15wt% of ultra-fine fly ash; and 5-15wt% of calcium hydroxide on a basis of the ultra-fine fly ash. A ratio of water to cement is 44-48% by weight. The content of fine aggregate is 32-37wt%. The content of coarse aggregate is 36-41wt%. The maximum size of the coarse aggregate is 19mm. The concrete composition for pavement repairing additionally contains 0.3-0.5wt% of multifunctional air-entaining agent and 0.2-0.5wt% of retarding agent on a basis of the binder.
摘要翻译: 提供了用于路面修复的具体组合物,以显示出优异的耐硫酸盐性,同时降低水化热和渗透性并抑制碱聚集反应。 用于路面修复的混凝土组合物包括:含有85-90wt%超快硬化水泥和10-15wt%超细粉煤灰的粘结剂17-19wt%; 和基于超细粉煤灰的氢氧化钙5-15重量%。 水与水泥的比例为44-48重量%。 细骨料含量为32-37wt%。 粗骨料含量为36-41wt%。 粗骨料的最大尺寸为19mm。 用于路面修补的混凝土组合物另外含有0.3-0.5重量%的多功能空气引入剂和0.2-0.5重量%的基于粘合剂的延迟剂。
-
公开(公告)号:KR101865570B1
公开(公告)日:2018-06-08
申请号:KR1020160169941
申请日:2016-12-13
申请人: (주)포스코켐텍
发明人: 임윤탁
IPC分类号: C04B7/42 , C04B7/36 , C04B7/44 , C04B111/20
CPC分类号: C04B7/424 , C04B7/362 , C04B7/44 , C04B2111/2023
摘要: 고알칼리저항성해수마그네시아클링커가제공된다.본발명은, 마그네시아클링커의화학성분을기준으로 CaO/SiO중량함량비가 2.4~5.0를만족하도록, 해수마그네시아클링커의제조과정에서형성되는합성수산화마그네슘슬러리에수산화칼슘슬러리(석회유, milk lime)를첨가하여이루어진고 알카리성해수마그네시아클링커에관한것이다.
-
公开(公告)号:KR1020180000690A
公开(公告)日:2018-01-03
申请号:KR1020170078897
申请日:2017-06-22
申请人: 에보니크 데구사 게엠베하
发明人: 푸쉬만,디르크 , 보겔,미하엘 , 야로슬라브스키,블라디슬라브 , 티모피바,엘레나 , 리흐터,블라디미르
CPC分类号: C04B24/281 , C03C25/103 , C03C25/36 , C04B14/42 , C04B20/1037 , C04B38/00 , C04B38/02 , C04B2111/00586 , C04B2111/00603 , C04B2111/2023 , C04B2111/28 , C04B2111/40 , C04B2111/52 , C04B2111/60 , C04B2111/763 , C08G59/245 , C08G59/50 , C08G59/502 , C08G59/5026 , C08G59/56 , C08L63/00 , D06M15/55 , E04C5/07 , Y02W30/97 , C04B28/02 , C04B40/024 , C04B20/0048 , C04B14/386 , C04B14/4668 , C04B14/46 , C04B18/24 , C04B16/06 , C08L7/02
摘要: 본발명은본질적으로 A) 적어도 1종의섬유상캐리어, 및 B) 에폭시화합물 B1) 대디아민및/또는폴리아민성분 B2)의화학량론비 0.8:1 내지 2:1의, B1) 적어도 1종의에폭시화합물및 B2) 적어도 1종의디아민및/또는폴리아민으로형성된, 매트릭스재료로서의경화조성물, 및 C) 임의로추가보조제및 첨가제로형성된리바를포함하는, 오토클레이브기포콘크리트 (AAC)로제조된보강빌딩블록및 그의제조방법에관한것이다.
摘要翻译: 为二胺和/或多胺成分B2)药物化学量的本发明基本上是A)中的至少一种的纤维载体,和B)环氧化合物B1)ronbi 0.8:1至2:,B1)的至少一种的1的环氧化合物 和B2),固化的组合物作为基体材料,和C)任选地,包括通过加入助剂和添加剂,将高压釜加气混凝土(AAC)玫瑰条增强建筑块和一种二胺和/或多胺中的至少形成形成的钢筋 及其制造方法。
-
公开(公告)号:KR101086870B1
公开(公告)日:2011-11-25
申请号:KR1020080115486
申请日:2008-11-20
申请人: 쌍용양회공업(주)
CPC分类号: C04B28/04 , C04B2111/00215 , C04B2111/00318 , C04B2111/1025 , C04B2111/2023 , Y02W30/92 , C04B18/08 , C04B22/10 , C04B22/143 , C04B2103/52 , C04B24/122
摘要: 알칼리 실리카 반응을 억제할 수 있는 시멘트 조성물과 그의 제조방법에 관한 것이다. 본 발명은 클링커, 석고, 플라이 애쉬 및 석회석을 분쇄하여 제조한 시멘트에 있어서, 전알칼리 함량(Na
2 O eq)이 1.2% 이하인 클링커 100 중량부; SiO
2 +Al
2 O
3 +Fe
2 O
3 함량이 70% 이상이고, 강열감량이 4% 이하이며, 전알칼리 함량(Na
2 O eq)이 3.0% 이하인 플라이 애쉬 10~40 중량부; CaCO
3 함량이 80% 이상인 석회석 1~10 중량부; 분쇄조제로써 트리이소프로판올아민을 0.005~0.1 중량부 포함하는 시멘트로서, 시멘트의 SO
3 함량이 1.5~4.5%가 되도록 이수석고 또는 이수석고와 무수석고 혼합물을 사용하면서, 분말도 3000 ~ 5000 cm
2 /g로 분쇄한 것을 특징으로 하는 알칼리 실리카 반응 억제용 시멘트 조성물을 제공한다. 본 발명은 시멘트 응결 및 강도 발현성이 우수하면서, 알칼리 실리카 반응을 억제하는 효과를 현저하게 개선한 시멘트를 제공할 수 있다.
알칼리 실리카 반응, 시멘트, 플라이 애쉬, 석회석, 트리이소프로판올아민, 반응성 골재
-
-
-
-
-
-
-
-
-