公开(公告)号:KR1020170039075A
公开(公告)日:2017-04-10
申请号:KR1020167030065
申请日:2015-07-03
申请人: 도레이 카부시키가이샤
IPC分类号: B32B27/36 , B32B27/08 , B32B27/18 , C08G63/189
CPC分类号: B32B27/36 , C08G63/189 , G02B5/26
摘要: 본발명은특정대역의광을반사하는다층적층필름에있어서, 폴리에틸렌나프탈레이트수지를사용했을때에문제가되는층간박리가없는필름을제공한다. 주된반복단위가에틸렌-2,6-나프탈레이트인폴리에스테르 A로이루어지는 A층과, 주된반복단위가에틸렌테레프탈레이트로이루어지는 A층을구성하는폴리에스테르의굴절률보다낮은굴절률을갖는폴리에스테르 B로이루어지는 B층을서로적어도 201층이상적층시킨다층적층필름이며, 폴리에스테르 A가이하의요건을만족시키는것을특징으로하는다층적층필름이다. (1) 카르복실산말단기량이 5eq/t 이상 20eq/t 이하. (2) 인산알칼리금속염을 1.3몰/ton 이상, 3.0몰/ton 이하이며, 또한인산을인산알칼리금속염에대해서 0.4배이상, 1.5배이하의몰비로함유한다. (3) 고유점도가 0.55 이상, 0.63 이하.
摘要翻译: 本发明根据用于反射预定频带的光,用聚对苯二甲酸乙酯树脂膜当与没有分层是一个问题的多层层叠膜提供。 主要重复单元为乙烯2,6-萘二甲酸是聚酯A层,和由对苯二甲酸乙二醇酯的聚酯A构成的主重复单元,其包含具有比构成A层的聚酯的折射率低的折射率的聚酯乙 B层彼此并由此至少201层或层叠膜的层,多层层叠膜,其包括满足下该聚酯一个要求的一个步骤的多个层。 (1)羧酸端基量不小于5eq / t且不大于20eq / t。 (2)在小于0.4倍,1.5倍为磷酸的碱金属盐的摩尔比磷酸1.3摩尔/吨以上,超过3.0摩尔/吨,并且还磷酸的碱金属盐。 (3)特性粘度不小于0.55且不大于0.63。
-
公开(公告)号:KR1020150140716A
公开(公告)日:2015-12-16
申请号:KR1020157031297
申请日:2014-04-08
申请人: 캐논 가부시끼가이샤
IPC分类号: G03G9/087 , C08G63/181 , G03G9/08
CPC分类号: G03G9/08755 , C08G63/00 , C08G63/181 , C08G63/189 , C08J3/12 , C08J2367/00 , C08J2367/02 , G03G9/0804 , G03G9/0806 , G03G9/08795 , G03G9/08797
摘要: 본발명은샤프멜트성을갖고, 정착성과블로킹특성을양립시키고, 대전성이양호한결정성폴리에스테르수지를제공하며, 상기토너용결정성폴리에스테르수지는하기관계식을만족한다. 25 ≤ Tg ≤ 70 및 (Tg+273)/(Mp+273) ≥ 0.75 상기식에서 Tg (℃)는토너용결정성폴리에스테르수지의유리전이온도를나타내고, Mp (℃)는토너용결정성폴리에스테르수지의융점을나타낸다.
摘要翻译: 本发明提供具有陡峭的熔融性,良好的定影性和粘连特性以及良好的带电性的结晶性聚酯树脂,并且调色剂用结晶性聚酯树脂满足以下关系式。 25占Tg 70和(Tg + 273)/(Mp + 273)≤0.75其中Tg(占)是调色剂用结晶聚酯树脂的玻璃化转变温度,Mp 代表酯树脂的熔点。
-
公开(公告)号:KR101217294B1
公开(公告)日:2012-12-31
申请号:KR1020077011205
申请日:2005-09-15
申请人: 쓰리엠 이노베이티브 프로퍼티즈 컴파니
发明人: 허브린크,티모시,제이. , 덴커,마틴,이. , 치엔,버트,티. , 존슨,매튜,비. , 톰슨,리차드,제이. , 덕스,크리스토퍼,제이. , 메릴,윌리엄,더블유. , 리,푸밍,비.
IPC分类号: C08G63/183 , C08G63/189 , C08J5/18 , B32B27/36
CPC分类号: C08G63/189 , B32B27/36 , C08G63/181 , C08G63/183 , Y10T428/24942 , Y10T428/2495 , Y10T428/31507 , Y10T428/31786
摘要: 비교적낮은굴절율및 비교적높은유리전이온도를가진개질코폴리에스테르가개시되어있다. 다층중합체필름과같은광학필름에하나이상의층을형성하는데있어서이러한개질코폴리에스테르가사용될수 있다.
-
公开(公告)号:KR1020070084310A
公开(公告)日:2007-08-24
申请号:KR1020077011205
申请日:2005-09-15
申请人: 쓰리엠 이노베이티브 프로퍼티즈 컴파니
发明人: 허브린크,티모시,제이. , 덴커,마틴,이. , 치엔,버트,티. , 존슨,매튜,비. , 톰슨,리차드,제이. , 덕스,크리스토퍼,제이. , 메릴,윌리엄,더블유. , 리,푸밍,비.
IPC分类号: C08G63/183 , C08G63/189 , C08J5/18 , B32B27/36
CPC分类号: C08G63/189 , B32B27/36 , C08G63/181 , C08G63/183 , Y10T428/24942 , Y10T428/2495 , Y10T428/31507 , Y10T428/31786
摘要: Modified copolyesters having relatively low refractive indices and relatively high glass transition temperatures are disclosed. These modified copolyesters can be used in forming one or more layers in an optical film, such as a multilayer polymer film.
摘要翻译: 公开了具有相对低的折射率和相对高的玻璃化转变温度的改性共聚酯。 这些改性共聚酯可用于在诸如多层聚合物膜的光学膜中形成一层或多层。
-
公开(公告)号:KR100375087B1
公开(公告)日:2003-05-12
申请号:KR1019950027356
申请日:1995-08-25
申请人: 제이에프이 엔지니어링 가부시키가이샤 , 교도인사쓰가부시키가이샤
IPC分类号: C08G63/181 , B65D65/00 , C08G63/66
CPC分类号: C08G63/199 , B65D65/38 , C08G63/189 , C08L67/02 , Y10T428/1352 , Y10T428/1355 , Y10T428/1397 , Y10T428/24 , C08L69/00
摘要: An ester copolymer resin having a general formula ÄIÜ. wherein Ar represents 2,6-naphthalene group or phenylene group, R represents ethylene group or 1,4-cyclohexylene group, and n is a number of 100 to 1000 and a polymer alloy having a solubility parameter of 10.8 to 11.9 consisting essentialy of the ester copolymer and a polycarbonate resin are provided. The ester resin and the alloy are transparent and has a heat resistance and a hot water resistance (resistance to whitening) resisting sterilization of food, a good heat sealebility to aluminum closure, and recycling ability with PET resin.
摘要翻译: 具有通式的酯共聚物树脂。 < CHEM> 其中Ar代表2,6-亚萘基或亚苯基,R代表亚乙基或1,4-亚环己基,n为100至1000的数,以及溶解度参数为10.8至11.9的聚合物合金,其组成为 酯共聚物和聚碳酸酯树脂。 酯树脂和合金是透明的,具有耐食品性和抗热水性(耐白化性),抗食品消毒,对铝封闭具有良好的热封性,以及与PET树脂的再循环能力。
-
公开(公告)号:KR1020020079472A
公开(公告)日:2002-10-19
申请号:KR1020020018457
申请日:2002-04-04
申请人: 에보닉 데구사 게엠베하
IPC分类号: C08L31/08
CPC分类号: B29C71/02 , B29K2067/00 , B29K2105/06 , B29L2031/3493 , C08G63/183 , C08G63/189 , C08G63/88 , C08L67/02 , C08L2666/02
摘要: PURPOSE: Provided are a process for manufacturing molded objects with better short time deflection temperature under load properties, as well as the molded objects of high dimensional stability manufactured thereby. CONSTITUTION: A process for manufacturing a molded object, comprises the steps of: (a) preparing a shaped object by molding a formulation of: 35 to 100% by weight of a thermoplastic polyester, 0 to 60% by weight of filler or a reinforcing material, 0 to 20% by weight of an impact modifying rubber, 0 to 30% by weight of a flame retardant, 0 to 20% by weight of a synergist and 0 to 5% by weight of other additives and/or processing agents; and (b) treating the molded object for at least 1 hour at a temperature ranging from 180 to 250 deg. C. Therefore, a molded object is prepared with improved short-time deflection temperature under load properties.
摘要翻译: 目的:提供一种用于制造在负载特性下具有更好的短时间挠曲温度的模制物体的方法,以及由此制造的具有高尺寸稳定性的模制物体。 构成:用于制造模制物体的方法包括以下步骤:(a)通过模制以下配方来制备成形物体:35至100重量%的热塑性聚酯,0至60重量%的填料或增强剂 材料,0至20重量%的抗冲击改性橡胶,0至30重量%的阻燃剂,0至20重量%的增效剂和0至5重量%的其它添加剂和/或加工剂; 和(b)在180-250度的温度范围内处理模塑物体至少1小时。 因此,在负载特性下制备具有改善的短时挠曲温度的成型物体。
-
公开(公告)号:KR100286251B1
公开(公告)日:2001-03-15
申请号:KR1019990006107
申请日:1999-02-24
申请人: 한국과학기술연구원 , 에쓰대시오일 주식회사
IPC分类号: C08F12/34
CPC分类号: C08G63/85 , C08G63/189 , C08G63/87
摘要: 티타늄화합물과인 화합물로구성된특수복합촉매를사용하여, 2,6-NDCA를주성분으로하는디카르복실산또는그의유도체, 혹은 2,6-NDC를주성분으로하는디카르복실산에스테르또는그의유도체를, 에틸렌글리콜또는이를주성분으로하는글리콜및 그의유도체와에스테르화반응시켜비스(베타-히드록시에틸)나프탈레이트및/또는그의저중합체를주성분으로하는에스테르화합물을얻고이를계속해서중축합반응시켜 PEN계중합체를얻는제조방법을제공한다. 이와같이제조된 PEN계중합체는색상과물성이우수한 PEN계중합체이며, 아울러본 발명의제조방법은상기에스테르화반응및 중축합반응시간을상당히단축시킨다.
-
公开(公告)号:KR100231406B1
公开(公告)日:1999-11-15
申请号:KR1019970704673
申请日:1996-10-25
申请人: 미쓰이 가가쿠 가부시키가이샤
CPC分类号: C08G63/189 , C08G63/78 , C08G63/82
摘要: 본 발명의 폴리에틸렌 나프탈레이트의 제조방법에서, 나프탈렌디카르복실산과 에틸렌글리콜간의 반응을 반응 개시할 때 부터 반응계내에 물을 주입하고, 필요에 따라 질산, 카르복실산, 인산, 인산1수소등의 염 및 아민으로 된 군중에서 선택한 적어도 1개의 촉매의 존재하에서 실시하여, 45~80%의 에스테르화율을 실현하여, 나프탈렌디카르복실산, 카르복실-히드록시에톡시카르보닐나프탈렌, 및 비스(히드록시에톡시카르보닐)나프탈렌을 함유한 나프탈렌디카르복실산 에스테르화반응 생성혼합물을 얻는다. 이어서 이 혼합액으로부터 결정체를 분리하여 에스테르화반응 생성혼합물을 얻는다. 그 후에 필요에 따라 이 혼합물에 에틸렌글리콜을 가하여 중축합한다. 본 발명의 방법에 의해 제조한 폴리에틸렌 나프탈레이트는 각각 디에틸렌글리콜골격을 갖는 나프탈렌디카르복실산의 함량이 적으므로, 예를 들어 외관등의 품질이 우수하다.
-
公开(公告)号:KR20180048664A
公开(公告)日:2018-05-10
申请号:KR20187006051
申请日:2016-09-01
IPC分类号: C08G61/02 , C08F232/08 , C08G63/189 , C08J5/18 , C09D145/00 , C09D165/00 , C09D167/02 , G02B1/04
CPC分类号: C09D165/00 , C08F232/00 , C08F232/08 , C08G61/02 , C08G63/189 , C08G2261/12 , C08G2261/312 , C08G2261/3325 , C09D145/00 , C09D167/02
摘要: 본발명에따른실시형태는, 각각 1종이상의단량체를전촉매또는활성제와함께포함하는성분 A 및성분 B를함유하는조성물을망라하며, 해당단량체는, 상기의성분 2종을혼합했을때 비닐첨가중합을일으켜실질적으로투명한필름을형성한다. 본발명에서채택된단량체는 1.4~1.8 범위의굴절률을가지고, 따라서이들조성물을조정하여다양한굴절률을가지는투명필름을형성할수 있다. 그결과, 본발명의조성물은다양한광전자분야의용도, 그중에서도코팅재, 봉입재, 충전재, 균염제(leveling agent)에유용하게쓰인다.
-
公开(公告)号:KR1020150040788A
公开(公告)日:2015-04-15
申请号:KR1020147028173
申请日:2013-06-19
申请人: 도레이 카부시키가이샤
IPC分类号: B32B27/36 , C08J7/04 , C09D175/04 , C09D175/14 , G02B1/10 , C08G18/62 , C08G18/70 , C08G63/189
CPC分类号: C09D133/26 , B32B27/36 , C08F2220/343 , C08G18/6229 , C08G18/6254 , C08G18/706 , C08J7/042 , C08J2367/02 , C08J2467/02 , C08J2475/14 , C09D175/04 , G02B1/105 , G02B1/14 , Y10T428/31533 , Y10T428/31565 , C08G63/189 , C09D175/14 , C08F220/14 , C08F2220/1808 , C08F220/58
摘要: 본원발명은투명성, 하드코트층을적층했을때의홍채형상모양(간섭무늬)의억제(시인성)가우수하고, 또한하드코트층과의초기접착성, 고온고습하에서의밀착성(내습열접착성), 내UV 접착성(UV 조사후의접착성)이우수하고, 또한비등수에침지했을때의접착성(내자비접착성), 내자비투명성이우수한적층폴리에스테르필름을제공하는것을목적으로한다. 그목적은폴리에스테르필름중 적어도편면에수지층(X)을갖는적층폴리에스테르필름으로서, 상기수지층(X)이아크릴·우레탄공중합수지(a)와, 나프탈렌골격을갖는폴리에스테르수지(b)를포함하는도료조성물로형성된층이고, 자비처리시험전후의필름헤이즈변화량(ΔHz)(ΔHz=자비처리시험전후의필름헤이즈-자비처리시험전의필름헤이즈)가 3.0% 미만인것으로함으로써달성된다.
摘要翻译: 虹膜状的本发明抑制(可见性)高斯数,进而在初始附着力,高的温度和硬涂层的高湿度下的粘合(在湿热粘合性)(干涉)当层叠透明度,硬涂层, 所述UV粘合剂内(粘合剂UV照射电阻之后)yiwoosu,此外,本发明的目的是提供一种粘合性(在比密合性)时,透明性优异,在沸水中浸泡时层叠在比该聚酯膜。 本发明的目的是提供一种在聚酯膜的至少一面上具有树脂层(X)的层合聚酯膜,其中树脂层(X)包含丙烯酸聚氨酯共聚物树脂(a),聚酯树脂 从包括涂料组合物形成的层,前和膜的雾度(ΔHz)的变化后煮沸处理试验 - 是由该(ΔHz=煮沸处理试验前和煮沸处理试验前的膜的雾度薄膜的雾度后)实现的是小于3.0%。
-
-
-
-
-
-
-
-
-