결정형산화제2세륨의제조방법

    公开(公告)号:KR100379653B1

    公开(公告)日:2003-06-11

    申请号:KR1019950017864

    申请日:1995-06-28

    IPC分类号: C01D17/00

    摘要: The present invention is to provide a process for preparing ceric oxide particles used as an abrasive or polishing material for producing semiconductors or as a UV ray-absorbing material for plastics, glass and the like. The present invention relates to a process for preparing cerium (IV) oxide particles having a particle size of from 0.03 mu m to 5 mu m, which comprises adjusting an aqueous medium containing cerium (IV) hydroxide and a nitrate to a pH of from 8 to 11 with an alkaline substance and heating the aqueous medium at a temperature of from 100 DEG to 200 DEG C. under pressure.

    摘要翻译: 本发明提供制备用作制造半导体的磨料或抛光材料或用作塑料,玻璃等的紫外线吸收材料的氧化铈颗粒的方法。 本发明涉及一种制备粒度为0.03μm-5μm的氧化铈(IV)颗粒的方法,该方法包括将含有氢氧化铈(IV)和硝酸盐的水介质调节至pH为8 用碱性物质将所述含水介质加热至100℃,并在100〜200℃的温度下加热所述含水介质。

    란가사이트 분말과 그 제조방법
    3.
    发明授权
    란가사이트 분말과 그 제조방법 失效
    란가사이트분말과그제조방법

    公开(公告)号:KR100382160B1

    公开(公告)日:2003-05-01

    申请号:KR1019990045659

    申请日:1999-10-20

    申请人: 신건철

    IPC分类号: C01D17/00

    摘要: PURPOSE: Provided are langasite(La3Ga5SiO14) powder having a chemically quantitative composition at low temperature and its manufacture method. CONSTITUTION: The method comprises steps of: (i) pouring ethylene glycol into a crucible and adding citric acid thereto with heating and stirring at a temperature of 50-90 deg.C to dissolve the citric acid in the ethylene glycol; (ii) dissolving (C2H5O)4Si, La(NO3)3·6H2O and Ga(NO3)3·nH2O wherein a molar ratio of La : Ga : Si is 3 : 5 : 1, in the citric acid dissolved solution at a temperature of 50-90 deg.C to obtain reaction solution; (iii) after stirring the reaction solution, polyesterifying the solution with heating and condensing it at a temperature of 100-130 deg.C; (iv) heat-treating the condensation of the step (iii) in an electric furnace at a temperature of 300-500 deg.C for 0.5-1 hour to obtain langasite precursor; and (v) calcining the prepared precursor at a temperature of 800-1,300 deg.C for 0.5-3 hours.

    摘要翻译: 目的:提供在低温下具有化学定量组成的硅酸镧(La3Ga5SiO14)粉末及其制造方法。 组成:该方法包括以下步骤:(i)将乙二醇倒入坩埚中,加入柠檬酸并加热搅拌,温度为50-90℃,使柠檬酸溶解于乙二醇中; (ii)在溶解的柠檬酸中溶解(C 2 H 5 O)4 Si,La(NO 3)3·6H 2 O和Ga(NO 3)3·nH 2 O(其中La:Ga:Si的摩尔比为3:5:1) 溶液在50-90℃的温度下反应得到反应溶液; (iii)搅拌反应溶液后,加热使溶液聚酯化并在100-130℃的温度下冷凝; (iv)将步骤(iii)在300-500℃的电炉中进行0.5-1小时的热处理,得到lang ite石前驱体; 和(v)在800-1,300℃的温度下煅烧所制备的前体0.5-3小时。

    육불화인산리튬의 제조방법

    公开(公告)号:KR100288825B1

    公开(公告)日:2001-05-02

    申请号:KR1019980063278

    申请日:1998-12-31

    IPC分类号: C01D17/00

    摘要: 본 발명은 오염화인(PCl
    5 ), 염화리튬(LiCl), 및 불산(HF)을 원료로하여 육불화인산리튬(LiPF
    6 )을 제조하는 방법에 있어서, 오염화인을 불산과 반응시켜 오불화인(PF
    5 )을 제조하는 단계(제1단계 반응)와 오불화인을 불산용액중에서 염화리튬과 반응시켜 육불화인산리튬을 제조하는 단계(제2단계 반응)로 구성시키고, 상기 1, 2 단계 반응에서 불소가스로 처리하여 수분을 완전히 제거한 무수불산을 사용하는 것을 특징으로하고 제2단계 반응에서 F
    2 개스를 처리하여 반응계 중의 LiPO
    x F
    y 를 배제시켜 육불화인산리튬을 제조하는 방법에 관한 것이다.
    본 발명은 PCl
    5 및 LiCl등 중저가의 원료를 사용하면서도 반응계중에 전해로 얻어지는 고순도의 F
    2 개스를 이용하므로서 고수율 고순도의 육불화인산리튬을 제조할 수 있다는 장점을 갖는다.

    육불화인산리튬의 제조방법
    5.
    发明公开
    육불화인산리튬의 제조방법 有权
    柠檬酸十六烷酯磷酸盐的生产工艺

    公开(公告)号:KR1020000046590A

    公开(公告)日:2000-07-25

    申请号:KR1019980063278

    申请日:1998-12-31

    IPC分类号: C01D17/00

    摘要: PURPOSE: A production process of a lithium hexafluoro phosphate is provided which uses not only PCl5 and LiCl with middle or a low price but also F2 gas with high purity so that a LiPF6 with high purity and yield is produced. CONSTITUTION: A production process of the LiPF6 whose raw materials are PCl5, LiCl and HF is as follows: (1) a first step reaction wherein PCl5 and HF are reacted to produce PF5; and (2) a second reaction wherein PCL5 is mixed with lithium chloride in a HF solution to produce the LiPF6. The both reactions use anhydrous HF that is treated with F2 gas to eliminate water and the second reaction is touched with F2 gas to exclude LiPOxFy in a reactor.

    摘要翻译: 目的:提供六氟磷酸锂的生产方法,不仅使用具有中等或低价的PCl5和LiCl,而且还使用高纯度的F2气体,从而产生高纯度和高产率的LiPF 6。 构成:原料为PCl5,LiCl和HF的LiPF6的制备方法如下:(1)第一步反应,其中PCl5和HF反应生成PF5; 和(2)其中PCL5与HF溶液中的氯化锂混合以产生LiPF 6的第二反应。 两种反应都使用用F2气处理的无水HF消除水,第二反应用F2气体接触以排除反应器中的LiPO x F y。

    고밀도 세슘 및 루비듐 염 용액 생성 방법
    6.
    发明授权
    고밀도 세슘 및 루비듐 염 용액 생성 방법 失效
    生产高密度油和硫酸盐溶液的方法

    公开(公告)号:KR100160829B1

    公开(公告)日:1998-11-16

    申请号:KR1019950701863

    申请日:1993-11-10

    IPC分类号: C01D17/00

    CPC分类号: C01D17/00

    摘要: 본 발명은 고-밀도 진한 세슘 및 루비듐 염 용액을 생성하는 방법에 관한 것이다. 본 발명에 따라, 비-하소된 세슘광 및/또는 하소된 레피돌라이트는 입자 크기 0.1mm로 분쇄되고, 200-280℃의 온도, 20-40 bar의 압력, 및 4-15중량%의 현탁액 밀도에서, 1-3시간의 기간내에 SiO
    2 :CaO≥1:2의 몰비에서 열수 온침된다. 불용성 고형물이 여과되고 세척된다. 칼슘 및 리튬이 이산화탄소를 도입하고 용해 여과물로 부터 침착된 탄산염을 여과시킴으로써 제거된다. 잔여의 용액은 농축되고, 세슘 및 루비듐의 염은 약 6 이하의 pH까지 산 또는 산무수물의 첨가에 의해 형성되고, 이때 온침후에 분리된 여과물은 열수 온침 방법에서 여러번 사용된다.

    음극 활물질용 그래핀 나노시트 및 제조방법
    7.
    发明公开
    음극 활물질용 그래핀 나노시트 및 제조방법 审中-实审
    负极活性物质用石墨烯纳米片及其制造方法

    公开(公告)号:KR1020170085323A

    公开(公告)日:2017-07-24

    申请号:KR1020160004797

    申请日:2016-01-14

    摘要: 본발명은표면에알칼리클로라이드층이형성되어있는음극활물질용그래핀나노시트및 그제조방법에관한것으로, 본발명의음극활물질용그래핀나노시트는표면에알칼리클로라이드층이형성되어있으므로, 비표면적이조절되어전해액과의부반응이감소되어, 이를포함하는음극이통상의미처리그래핀(bare graphene)에비해안정한고체전해질(Solid Electrolyte Interface; SEI) 피막을형성할수 있어서고온내구성이향상될수 있으며, 또한이를포함하는리튬이차전지의초기효율이향상될수 있으므로, 리튬이차전지의제조에유용하게사용될수 있다.

    摘要翻译: 由于本发明是肯定的用于与碱金属氯化物层的负极活性材料中的销纳米片的表面上形成并涉及制造其的方法,负电极的石墨烯纳米薄片用于本发明的活性物质中,形成在表面,比表面积在碱金属氯化物层 部分失谐降低与电解质的副反应,阴极通常是指处理的石墨烯(裸石墨烯)EBI以包含其的稳定的固体电解质;在能够形成(固体电解质界面SEI)膜可以提高高温耐久性,并且 锂二次电池的初始效率是如此可以提高包括相同,可以在锂二次电池的制备中有效地使用。

    신규한 혼합금속산화물
    8.
    发明授权
    신규한 혼합금속산화물 有权
    新型混合金属氧化物

    公开(公告)号:KR101595533B1

    公开(公告)日:2016-02-19

    申请号:KR1020150097325

    申请日:2015-07-08

    发明人: 옥강민 송승윤

    IPC分类号: C01B19/00 C01D17/00 C01F17/00

    摘要: 본발명은신규한혼합금속산화물에관한것으로, 혼합금속산화물의층상골격구조에의한특성을기반으로, 레이저소자, 비선형광학소자, 압전센서, 무선통신, 촉매, 전력저장수송장치, 컴퓨터소자, 양자간섭장치, 층간삽입복합체, 약물전달체, 이차전지양극제또는전기광학재료물질등에적용된제품개발에사용할수 있다.

    摘要翻译: 本发明涉及一种新型的混合金属氧化物,其可用于显影应用于诸如激光装置,非线性光学元件,压电传感器,无线通信装置,催化剂,电力传输和存储装置,计算机元件,量子干涉 基于来自混合金属氧化物的层状骨架结构的特性的装置,中间层插层复合物,药物递送载体,二次电池用正极或电光材料。 本发明的新型混合金属氧化物通过Rb2CO3,Sc(NO3)3xH2O(x = 0〜6)和SeO2的水热反应合成,并由化学式RbSc(SeO_3)_2表示。