摘要:
세라믹전자부품이나유전체자기조성물에서, 폭넓은온도영역에서의온도특성을향상시킨다. 제1 원소군과제2 원소군을포함하며, 제1 원소군은 Ba, Si, 및 Al로이루어지고, Ba가 BaO이며, Si가 SiO이고, Al이 AlO인제1 원소군의 100중량부중에, Ba를 BaO 환산으로 20 이상 40중량부이하, Si를 SiO환산으로 48 이상 75중량부이하, Al을 AlO환산으로 5 이상 20중량부이하의비율로함유한다. 제2 원소군은 Ti 및 Fe 중적어도하나, Mn, Sr, 및 Mg로이루어지고, Ba가 BaO, Si가 SiO, Al이 AlO인제1 원소군의 100중량부에대하여, Mn을 MnO 환산으로 1 이상 10중량부이하, Sr을 SrO 환산으로 1 이상 35중량부이하, Mg를 MgO 환산으로 0.1 이상 6중량부이하, Ti를 TiO환산으로, Fe를 FeO환산으로, 1 이상 35중량부이하의비율로함유한다.
摘要翻译:陶瓷电子部件或具有第一元素组和第二元素组的介电陶瓷组合物。 第一元素组由Ba,Si和Al构成,并且在100重量份的第一元素组中包含20至40重量份的BaO,48至75重量份的SiO 2和5至20重量份的 Al2O3的重量。 第二元素组由Ti和Fe,Mn,Sr和Mg中的至少一种组成,并且相对于100重量份的第一元素组,含有1至10重量份的MnO,1至35重量份 的SrO,0.1〜6重量份的MgO和1〜35重量份的TiO 2和/或Fe 2 O 3。
摘要:
PURPOSE: A high crystalline dielectric material and a manufacturing device and a method of manufacture thereof are provided to improve the crystallinity of particles. CONSTITUTION: A high crystalline dielectric material has a crystallization axial ratio of 1.003-1.010, a BET non-surface area of 4-80 m^2/g, and a particle size of 15-200 nanometers. The dielectric substance has a perovskite structure marked as ABO3. In the structure of ABO3, A is one or more selected from Mg, Ca, Sr, Pb, Ba and La. B is one or more selected from Ti, Zr and Hf. The manufacturing device of the high crystalline dielectric substance comprises a pair of material feeders(10,20), a mixing tank(30), an autoclave(40) and a cooling pump(50). A manufacturing method of the high crystalline dielectric substance comprises the following steps: dissolving starting raw material A and B in each reactor; manufacturing the nuclei of granules by reacting the starting raw material A and B in the blending tank; and growing the nuclei in a thermostat autoclave. [Reference numerals] (31) Ultrasonic device; (33) High pressure pump; (AA) Filter
摘要:
비유전율 및 교류 파괴 전압이 높고, 유전 손실이 낮으며, 온도 특성 및 소결성이 양호한 유전체 자기 조성물을 제공하는 것이다. (Ba 1 -uvw , Ca u , Mg v , Sr w ) α (Ti 1 -x , Zr x )0 3 의 조성식으로 표시되는 주성분과, 산화니켈과, 산화세륨과, 산화망간을 가지는 유전체 자기 조성물로서, 상기 조성식 중의 u가 0.20~0.27이고, 상기 조성식 중의 v가 0.018~0.049이며, 상기 조성식 중의 w가 0.004~0.018이고, 상기 조성식 중의 x가 0.118~0.149이며, 상기 조성식 중의 α가 0.95~1.02이고, 상기 산화니켈을 상기 주성분 100중량부에 대해 0.03~0.4중량부 함유하고, 상기 산화세륨을 상기 주성분 100중량부에 대해 0.03~0.4중량부 함유하며, 상기 산화망간을 상기 주성분 100중량부에 대해 0.03~0.4중량부 함유하는 유전체 자기 조성물.
摘要:
유전 특성을 손상시키지 않고 소성 온도를 저하할 수 있는 유전체 자기 조성물의 제조 방법을 제공하는 것을 목적으로 한다. 본 발명에 따른 유전체 자기 조성물의 제조 방법은, 조성식 [(Ca x Sr 1 -x )O] m [(Ti y Zr 1 -y- z Hf z )O 2 ](식 중 x, y, z, m은, 각각 0.5≤x≤1.0, 0.01≤y≤0.10, 0<z≤0.20, 0.90≤m≤1.04이다)로 표시되는 유전체 산화물을 조제하는 공정, 그 유전체 산화물 100 중량부에 대해, 소결조제를 1 내지 10 중량부 및 필요에 따라 나트륨 화합물을 Na 2 O 환산으로 0.1 내지 0.5 중량부 혼합하는 공정, 및 얻어진 혼합물을 소성하는 공정을 포함하는 유전체 자기 조성물의 제조 방법으로서, 상기 소결조제가, 소결조제의 전량 100 중량% 중에, 망간 화합물을 MnO 환산으로 30 내지 69 중량%, 산화 알루미늄을 Al 2 O 3 환산으로 1 내지 20 중량%, 산화 규소를 SiO 2 환산으로 30 내지 50 중량% 함유하여 이루어지는 것을 특징으로 한다.
摘要:
A gold nanoparticle of peptide and cyanine phosphor is provided to selectively in vivo detect and image protease, and quantitatively analyze the expression amount of protease, so that the gold nanoparticle is useful as a sensor for realtime cell imaging and early diagnosis of non-hygroscopic disease by being selectively absorbed into the cell or tissue. A gold nanoparticle for imaging MMP(matrix metalloprotease) expressed in the cell or tissue contains a peptide with -SH end group which is specifically degraded by MMP coupled with a cyanine phosphor, wherein the peptide with -SH end group is Gly-Pro-Leu-Gly-Leu-Phe-Ala-Arg-Cys; and the MMP is MMP-1, MMP-2, MMP-3, MMP-7, MMP-8, MMP-9, MMP-10, MMP-11, MMP-12, MMP-13, MMP-14, MMP-15, MMP-16, MMP-17, MMP-18, MMP-19, MMP-20, MMP-21, MMP-22, MMP-23, MMP-24, MMP-25, MMP-26, MMP-27 or MMP-28.
摘要:
According to one exemplary embodiment, a dielectric ceramic composition includes a main component group, where the main component group is represented by MgxCayZnzTiO2+x+y+ z, where the sum of x, y, and z is less than or equal to 1.0 such that the dielectric ceramic composition has a wider sintering temperature range and reduced exaggerated grain growth. According to one embodiment, x can be greater than 0.0 and less than 1.0, y can be greater than 0.0 and less than 1.0, and z can be greater than 0.0 and less than 1.0. The dielectric ceramic composition can further include between 0.0 and 50.0 percent by weight of aluminum oxide. The dielectric ceramic composition can further include copper oxide. The dielectric ceramic composition can further include boron oxide.
摘要翻译:根据一个示例性实施方案,电介质陶瓷组合物包括主要组分基团,其中主要组分基团由Mg x Ca y Zn z TiO 2 + x + y + z表示,其中x,y和z的总和小于或等于1.0,使得 介电陶瓷组合物具有更宽的烧结温度范围和减少的夸张的晶粒生长。 根据一个实施例,x可以大于0.0且小于1.0,y可以大于0.0且小于1.0,并且z可以大于0.0且小于1.0。 电介质陶瓷组合物可进一步包含0.0至50.0重量%的氧化铝。 电介质陶瓷组合物还可以包括氧化铜。 电介质陶瓷组合物还可以包括氧化硼。
摘要:
In a start powder mixture of magnesium zinc titanate and a barium boro-silicate flux, it is discovered that the addition of lithium to the flux enables the manufacture of multilayer ceramic capacitors using the powder mixture, that perform to the COG standard including an accelerated life test. This addition of lithium also makes possible the sintering to maturity of COG multilayer capacitors at temperatures as low as 950 DEG C, which in turn allows the use of silver-palladium alloy buried electrodes of high silver and low palladium content which in turn lead to higher capacitor Q and lower manufacturing costs.
摘要:
PURPOSE: A dielectric ceramic composition comprising MgTiO3 as a main component is provided for use as phase shifters operated at the microwave region, requiring dielectric constant(15-17), quality factor(>=70000), and high mechanical strength. CONSTITUTION: The dielectric ceramic composition for phase shifters comprises MgTiO3 as a main component, 0.01-7wt.%(based on MgTiO3) of one or more of CuO and ZnO as sintering aids for lowering sintering temperature(
摘要:
본 발명은 Ca, Bi, Ti 및 산소로 이루어지는 비스무트(bismuth)층형상 화합물을 주성분으로 하는 압전 세라믹에 있어서, 주성분이 되는 비스무트층형상 화합물중의 Ca, Bi 및 Ti의 몰비를 a:b:c라고 했을 때, 0.15≤a/c<0.25, 또한 3.5≤(2a+3b)/c≤3.88의 관계를 만족시킨다.
摘要:
본발명은비유전율이 100이상이고, 고온부하수명시험에있어서의신뢰성이우수한비환원성유전체세라믹조성물, 및상기개선된비환원성유전체세라믹조성물을사용하여형성된모놀리식세라믹커패시터를제공한다. 본발명의유전체세라믹조성물은, 금속원소로서 M(단, M은 Ca, 또는 Ca 및 Sr), Zr 및 Ti를함유하는복합산화물을포함하며, 조성식(CaSr)(ZrTi)O로표현했을때, x, y 및 m의값이 0≤x