METHOD FOR PURIFYING HIGH-PURITY ALUMINIUM BY DIRECTIONAL SOLIDIFICATION AND SMELTING FURNACE THEREFOR
    1.
    发明申请
    METHOD FOR PURIFYING HIGH-PURITY ALUMINIUM BY DIRECTIONAL SOLIDIFICATION AND SMELTING FURNACE THEREFOR 审中-公开
    通过定向固化和熔化炉净化高纯度铝的方法

    公开(公告)号:US20140202653A1

    公开(公告)日:2014-07-24

    申请号:US13977582

    申请日:2011-12-14

    申请人: Tao Hong Imin Nurgul

    发明人: Tao Hong Imin Nurgul

    IPC分类号: C22B21/06 B22D27/04 C22B9/02

    摘要: Provided is a method for preparing high-purity aluminum by directional solidification, comprising the steps of: providing 4N to 5N aluminum as raw material, heating the same to a temperature of 670° C. to 730° C., maintaining the temperature for 7 minutes to 80 minutes, cooling the bottom of chamber (3) to allow the aluminum liquid crystallizing in a direction from the bottom to top of the chamber (3) for 1 hour to 8 hours to obtain a crystalline ingot, during the crystallization process of a finished product of crystalline ingot, stifling and heating the aluminum liquid, maintaining a particular temperature gradient of the aluminum liquid, and removing a portion of the crystalline ingot from one end of the ingot, the remaining portion being the high-purity aluminum. Also provided is a smelting furnace, comprising a shell (1), a heating device (2), a chamber (3), a temperature measurement device, a stirring device and a cooling device (6).

    摘要翻译: 提供了一种通过定向凝固制备高纯度铝的方法,包括以下步骤:提供4N至5N的铝作为原料,将其加热至670℃至730℃的温度,将温度保持在7℃ 分钟至80分钟,冷却室(3)的底部,使铝液在室(3)的底部至顶部的方向上结晶1小时至8小时,以在结晶过程中获得晶体锭 结晶锭的成品,腌制和加热铝液体,保持铝液体的特定温度梯度,并从锭的一端去除一部分结晶锭,其余部分是高纯度铝。 还提供了一种冶炼炉,包括壳体(1),加热装置(2),室(3),温度测量装置,搅拌装置和冷却装置(6)。