Copper foil for current collector of lithium secondary battery with improved wrinkle characteristics
    1.
    发明授权
    Copper foil for current collector of lithium secondary battery with improved wrinkle characteristics 有权
    锂二次电池集电器用铜箔,具有改善皱纹特性

    公开(公告)号:US08349518B2

    公开(公告)日:2013-01-08

    申请号:US13029656

    申请日:2011-02-17

    IPC分类号: H01M4/64

    摘要: A copper foil for a current collector of a lithium secondary battery has a crystalline structure, in which a ratio of the sum of texture coefficients of a (111) surface and a (200) surface to the total sum of texture coefficients of the (111), (200) and (220) surfaces is 60 to 85%, a ratio of the texture coefficient of the (111) surface to the total sum of texture coefficients of the (111), (200) and (220) is 18 to 38%, a ratio of the texture coefficient of the (200) surface thereto is 28 to 62%, and a ratio of the texture coefficient of the (220) surface thereto is 15 to 40%. The copper foil has surface roughness (Rz-JIS) of 2 μm or less, weight deviation of 3% or less, tensile strength of 30 to 40 kgf/mm2, elongation of 3 to 20%, and thickness of 1 to 35 μm.

    摘要翻译: 用于锂二次电池的集电体的铜箔具有晶体结构,其中(111)表面和(200)表面的织构系数之和与(111)的织构系数的总和的比率 (111),(200)和(220)的织构系数的总和的比例为(18),(200)和(220) (200)表面的织构系数的比例为28〜62%,(220)表面的织构系数的比例为15〜40%。 铜箔的表面粗糙度(Rz-JIS)为2μm以下,重量偏差为3%以下,拉伸强度为30〜40kgf / mm 2,伸长率为3〜20%,厚度为1〜35μm。

    COPPER FOIL FOR CURRENT COLLECTOR OF LITHIUM SECONDARY BATTERY
    2.
    发明申请
    COPPER FOIL FOR CURRENT COLLECTOR OF LITHIUM SECONDARY BATTERY 审中-公开
    锂二次电池电流收集器铜箔

    公开(公告)号:US20120040241A1

    公开(公告)日:2012-02-16

    申请号:US12962180

    申请日:2010-12-07

    IPC分类号: H01M4/66

    摘要: A copper foil for a current collector of a lithium secondary battery is configured such that a nodule cluster having an inter-nodule aspect ratio of 0.001 to 2 is provided at a matte side formed on one surface of the copper foil, in aspect of a crystal structure, a ratio of a texture coefficient of a (200) surface to a sum of texture coefficients of a (111) surface and the (200) surface is 30 to 80%, the copper foil has a water contact angle of 90° or below, and impurity spots existing at the surface of the copper foil have a maximum diameter of 100 μm or less, and a minimal spacing distance between the impurity spots is 1 cm or more.

    摘要翻译: 另外,作为锂二次电池用集电体的铜箔,在铜箔的一面形成的无光泽面上设置结晶长宽比为0.001〜2的结核团, (200)表面的织构系数与(111)面和(200)表面的织构系数之和的比例为30〜80%,铜箔的接触角为90°, 并且存在于铜箔表面的杂质点的最大直径为100μm以下,杂质点之间的最小间隔距离为1cm以上。

    COPPER FOIL FOR CURRENT COLLECTOR OF LITHIUM SECONDARY BATTERY WITH IMPROVED WRINKLE CHARACTERISTICS
    3.
    发明申请
    COPPER FOIL FOR CURRENT COLLECTOR OF LITHIUM SECONDARY BATTERY WITH IMPROVED WRINKLE CHARACTERISTICS 有权
    具有改进的特征的锂二次电池的电流收集器的铜箔

    公开(公告)号:US20120015206A1

    公开(公告)日:2012-01-19

    申请号:US13029656

    申请日:2011-02-17

    IPC分类号: B32B15/01

    摘要: A copper foil for a current collector of a lithium secondary battery has a crystalline structure, in which a ratio of the sum of texture coefficients of a (111) surface and a (200) surface to the total sum of texture coefficients of the (111), (200) and (220) surfaces is 60 to 85%, a ratio of the texture coefficient of the (111) surface to the total sum of texture coefficients of the (111), (200) and (220) is 18 to 38%, a ratio of the texture coefficient of the (200) surface thereto is 28 to 62%, and a ratio of the texture coefficient of the (220) surface thereto is 15 to 40%. The copper foil has surface roughness (Rz-JIS) of 2 μm or less, weight deviation of 3% or less, tensile strength of 30 to 40 kgf/mm2, elongation of 3 to 20%, and thickness of 1 to 35 μm.

    摘要翻译: 用于锂二次电池的集电体的铜箔具有晶体结构,其中(111)表面和(200)表面的织构系数之和与(111)的织构系数的总和的比率 (111),(200)和(220)的织构系数的总和的比例为(18),(200)和(220) (200)表面的织构系数的比例为28〜62%,(220)表面的织构系数的比例为15〜40%。 铜箔的表面粗糙度(Rz-JIS)为2μm以下,重量偏差为3%以下,拉伸强度为30〜40kgf / mm 2,伸长率为3〜20%,厚度为1〜35μm。