Method of producing an iron-, cobalt- and nickel-base alloy having low
contents of sulphur, oxygen and nitrogen
    2.
    发明授权
    Method of producing an iron-, cobalt- and nickel-base alloy having low contents of sulphur, oxygen and nitrogen 失效
    生产含硫,氧,氮含量低的铁,钴,镍基合金的方法

    公开(公告)号:US4820485A

    公开(公告)日:1989-04-11

    申请号:US10598

    申请日:1987-02-03

    摘要: A method of producing an alloy containing at least one major ingredient selected from the group consisting of iron (Fe), cobalt (Co), and Nickel (Ni) and having low contents of sulphur, oxygen, and nitrogen, comprises steps of:(a) holding a molten alloy in a container selected from the group consisting of a lime crucible, a lime crucible furnace, a converter and a ladle lined with a basic refractory consisting of 15-85% of calcium oxide (CaO), and 15-75% of magnesium oxide (MgO), wherein said alloy consists essentially of at least one major ingredient selected from the group consisting of iron (Fe), nickel (Ni), and cobalt (Co);(b) adding at least one additive, based on the molten alloy, into said molten alloy in an atmosphere selected from the group consisting of a non-oxidizing atmosphere and a vacuum, wherein said additive is selected from the group consisting of aluminum (Al), aluminum alloys, silicon and silicon alloys;(c) desulphurizing, deoxidizing and denitrifying said molten alloy under an atmosphere selected from the group consisting of a non-oxidizing atmosphere and a vacuum, whereby the molten alloy contains 0.005 to 7.0% of residual aluminum, 0.0001 to 0.02% of residual calcium, and 0.0005 to 0.03% of residual magnesium; and(d) casting said molten alloy into a mold.

    摘要翻译: 包含选自铁(Fe),钴(Co)和镍(Ni)中的至少一种主要成分并具有低含量的硫,氧和氮的合金的方法包括以下步骤:( a)将熔融合金保持在选自石灰坩埚,石灰坩埚炉,转炉和用15-85%的氧化钙(CaO)组成的碱性耐火材料的浇包中的容器中, 75%的氧化镁(MgO),其中所述合金基本上由选自铁(Fe),镍(Ni)和钴(Co)的至少一种主要成分组成。 (b)在选自非氧化性气氛和真空的气氛中,将至少一种基于所述熔融合金的添加剂加入到所述熔融合金中,其中所述添加剂选自铝(Al ),铝合金,硅和硅合金; (c)在选自非氧化性气氛和真空的气氛下对所述熔融合金进行脱硫,脱氧,脱氮,由此熔融合金含有0.005〜7.0%的残留铝,0.0001〜0.02%的残余钙, 和0.0005〜0.03%的残余镁; 和(d)将所述熔融合金浇铸到模具中。

    Method of producing an iron-, cobalt- and nickel-base alloy having low
contents of sulphur, oxygen and nitrogen
    4.
    发明授权
    Method of producing an iron-, cobalt- and nickel-base alloy having low contents of sulphur, oxygen and nitrogen 失效
    生产含硫,氧,氮含量低的铁,钴,镍基合金的方法

    公开(公告)号:US4999053A

    公开(公告)日:1991-03-12

    申请号:US441600

    申请日:1989-11-27

    摘要: A method of producing an alloy containing at least one major ingredient selected from the group consisting of iron (Fe), cobalt (Co), and Nickel (Ni) and having low contents of sulphur, oxygen, and nitrogen, comprises steps of:(a) holding a molten alloy in a container selected from the group consisting of a lime crucible, a lime crucible furnace, a converter and a ladle lined with a basic refractory consisting of 15-85% of calcium oxide (CaO), and 15-75% of magnesium oxide (MgO), wherein said alloy consists essentially of at least one major ingredient selected from the group consisting of iron (Fe), nickel (Ni), and cobalt (Co);(b) adding at least one additive, based on the molten alloy, into said molten alloy in an atmosphere selected from the group consisting of a non-oxidizing atmosphere and a vacuum, wherein said additive is selected from the group consisting of aluminum (Al), aluminum alloys, silicon and silicon alloys;(c) desulphurizing, deoxidizing and denitrifying said molten alloy under an atmosphere selected from the group consisting of a non-oxidizing atmosphere and a vacuum, whereby the molten alloy contains 0.005 to 7.0% of residual aluminum, 0.0001 to 0.02% of residual calcium, and 0.005 to 0.03% of residual magnesium; and(d) casting said molten alloy into a mold.

    摘要翻译: 包含选自铁(Fe),钴(Co)和镍(Ni)中的至少一种主要成分并具有低含量的硫,氧和氮的合金的方法包括以下步骤:( a)将熔融合金保持在选自石灰坩埚,石灰坩埚炉,转炉和用15-85%的氧化钙(CaO)组成的碱性耐火材料的浇包中的容器中, 75%的氧化镁(MgO),其中所述合金基本上由选自铁(Fe),镍(Ni)和钴(Co)的至少一种主要成分组成。 (b)在选自非氧化性气氛和真空的气氛中,将至少一种基于所述熔融合金的添加剂加入到所述熔融合金中,其中所述添加剂选自铝(Al ),铝合金,硅和硅合金; (c)在选自非氧化性气氛和真空的气氛下对所述熔融合金进行脱硫,脱氧,脱氮,由此熔融合金含有0.005〜7.0%的残留铝,0.0001〜0.02%的残余钙, 和0.005〜0.03%的残余镁; 和(d)将所述熔融合金浇铸到模具中。

    Method of producing an iron; cobalt and nickel base alloy having low
contents of sulphur, oxygen and nitrogen
    5.
    发明授权
    Method of producing an iron; cobalt and nickel base alloy having low contents of sulphur, oxygen and nitrogen 失效
    铁的生产方法 钴和镍基合金,含硫量低,氧含量低,氮含量低

    公开(公告)号:US4729787A

    公开(公告)日:1988-03-08

    申请号:US937426

    申请日:1986-12-03

    摘要: A method of producing an alloy containing at least one major ingredient selected from the group consisting of iron (Fe), cobalt (Co), and Nickel (Ni) and having low contents of sulphur, oxygen, and nitrogen, comprises steps of:(a) holding a molten alloy in a container selected from the group consisting of a lime crucible, a lime crucible furnace, a converter and a ladle lined with a basic refractory consisting of 15-85% of calcium oxide (CaO), and 15-75% of magnesium oxide (MgO), wherein said alloy consists essentially of at least one major ingredient selected from the group consisting of iron (Fe), nickel (Ni), and cobalt (Co);(b) adding at least one additive, based on the molten alloy, into said molten alloy in an atmosphere selected from the group consisting of a non-oxidizing atmosphere and a vacuum, wherein said additive is selected from the group consisting of aluminum (Al), aluminum alloys, silicon and silicon alloys;(c) desulphurizing, deoxidizing and denitrifying said molten alloy under an atmosphere selected from the group consisting of a non-oxidizing atmosphere and a vacuum, whereby the molten alloy contains 0.005 to 7.0% of residual aluminum, 0.0001 to 0.02% of residual calcium, and 0.0005 to 0.03% of residual magnesium; and(d) casting said molten alloy into a mold.

    摘要翻译: 包含选自铁(Fe),钴(Co)和镍(Ni)中的至少一种主要成分并具有低含量的硫,氧和氮的合金的方法包括以下步骤:( a)将熔融合金保持在选自石灰坩埚,石灰坩埚炉,转炉和用15-85%的氧化钙(CaO)组成的碱性耐火材料的浇包中的容器中, 75%的氧化镁(MgO),其中所述合金基本上由选自铁(Fe),镍(Ni)和钴(Co)的至少一种主要成分组成。 (b)在选自非氧化性气氛和真空的气氛中,将至少一种基于所述熔融合金的添加剂加入到所述熔融合金中,其中所述添加剂选自铝(Al ),铝合金,硅和硅合金; (c)在选自非氧化性气氛和真空的气氛下对所述熔融合金进行脱硫,脱氧,脱氮,由此熔融合金含有0.005〜7.0%的残留铝,0.0001〜0.02%的残余钙, 和0.0005〜0.03%的残余镁; 和(d)将所述熔融合金浇铸到模具中。