Polyamide yarn
    1.
    发明授权
    Polyamide yarn 失效
    聚酰胺纱线

    公开(公告)号:US3917893A

    公开(公告)日:1975-11-04

    申请号:US43897074

    申请日:1974-02-04

    申请人: ALLIED CHEM

    摘要: An improved polyamide yarn is prepared by first applying to the yarn an aqueous emulsion of an oxidized polyethylene wax having an average molecular weight between about 1,000 and about 3,000, and containing between about 3 percent and about 9 percent oxygen by weight, thereafter heating said yarn to a temperature between about 100*C. and about 175*C., and then applying to said yarn a composition comprising an aqueous dispersion of colloidal silica and a polyethylene glycol ester of a C6 to C18 aliphatic acid, said polyethylene glycol having a molecular weight of about 200 to 600. The yarn is particularly useful for industrial purposes such as braided hose, rope belts, etc.

    摘要翻译: 通过首先将平均分子量在约1,000至约3,000之间且含有约3%至约9%的氧的氧化聚乙烯蜡的水性乳液首先施加到纱线上,然后加热所述纱线来制备改进的聚酰胺纱线 至约100℃至约175℃的温度,然后向所述纱线施加包含胶体二氧化硅的水分散体和C6至C18脂族酸的聚乙二醇酯的组合物,所述聚乙二醇具有分子 重量约为200至600.纱线特别适用于工业用途,如编织软管,绳带等。

    Production of polyester yarn
    2.
    发明授权
    Production of polyester yarn 失效
    生产聚酯纱线

    公开(公告)号:US3925588A

    公开(公告)日:1975-12-09

    申请号:US45650274

    申请日:1974-04-01

    申请人: ALLIED CHEM

    IPC分类号: D06M15/53 D02G3/36

    CPC分类号: D06M15/53 Y10T428/2969

    摘要: in which R1 and R2 are the same or different lower alkylene units such as ethylene, propylene and so forth up to 5 carbon atoms, R is an alkyl group containing 5 to 17 carbon atoms, and n has a value to produce a molecular weight of at least about 300. Preferably, the yarn is thereafter heated for 10 to 160 seconds at a temperature of from about 215* to 230*C. The yarn is particularly useful in the production of tire cord.

    An improved polyester yarn is prepared by applying to the yarn a finish composition consisting essentially of a polyalkylene glycol compound having the formula

    摘要翻译: 通过向纱线施加整理剂组合物来制备改进的聚酯纱线,该整理剂组合物基本上由具有式ORA PARALLEL RC-(O-R1-O-R2)n-OH的聚亚烷基二醇化合物组成,其中R 1和R 2相同或不同 低级亚烷基单元如乙烯,丙烯等至多5个碳原子,R是含有5至17个碳原子的烷基,n具有至少约300的分子量的值。优选地,纱线是 然后在约215℃至230℃的温度下加热10至160秒。纱线特别可用于生产轮胎帘线。

    Finishing composition for multi-filament yarns
    3.
    发明授权
    Finishing composition for multi-filament yarns 失效
    多层纱的成品组合物

    公开(公告)号:US3681244A

    公开(公告)日:1972-08-01

    申请号:US3681244D

    申请日:1970-08-19

    申请人: ALLIED CHEM

    IPC分类号: D06M13/34 D06M13/18 D06M13/20

    摘要: THIS INVENTION RELATES TO A FINISHING COMPSOITION AND MORE SPECIFICALLY TO A COMPOSITION CAPALE OF IMPARTING EXCELLENT TRANSLATIONAL EFFICIENCY TO HIGH-STRENGTH MULTI-FILAMENT YARNS. THE COMPOSITIONS ARE PARTICULARLY SUITABLE FOR FINISHING HIGH-STRENGHT YARNS TO BE USED FOR THE PRODUCTION OF TIRE YARNS, CONVEYOR BELTS, SEAT BELTS AND THE LIKE. THE FINISHING COMPOSITION COMPRISES THE REACTION PRODUCTS OF POLYBASIC CARBOXYLIC ACIDS AND PLYESTERS. THESE SIMLE ESTERS ARE OBTAINED BY REACTING MONOCARBOXYLIC ACID WITH A POLYHYDROXY ALCHOL.

    Production of polyesters
    4.
    发明授权
    Production of polyesters 失效
    生产聚酯

    公开(公告)号:US3672977A

    公开(公告)日:1972-06-27

    申请号:US3672977D

    申请日:1970-10-26

    申请人: ALLIED CHEM

    IPC分类号: D06M13/224 C08J1/44 D06M13/00

    摘要: AN IMPROVED MULTIFILAMENT POLYETHYLENE TEREPHTHALATE YARN HAVING A LUBRICATING PROTECTIVE FILM APPLIED THEREON OF FROM ABOUT 0.3 TO ABOUT 0.6 WEIGHT PERCENT BASED ON THE WIGHT OF THE YARN OF A LIQUID COMPOSITION CONSISTING ESSENTIALLY OF ABOUT 10 TO ABOUT 20 WEIGHT PERCENT OF SAID COMPOSITION OF EACH HEXADECYL STEARATE AND REFINED COCONUT OIL, ABOUT 3.0 TO ABOUT 6.0 WEIGHT PERCENT OF SAID COMPOSITION OF ETHOXYLATED TALLOW AMINE, ABOUT 10 TO ABOUT 20 WIGHT PERCENT OF SAID COMPISTION OF ETHOXYLATED LAURYL ALCOHOL, ABOUT 8.0 TO ABOUT 12.0 WEIGHT PERCENT OF SAID COMPOSITION OF SODIUM SALT OF ALKYLARYLSULFONATE, ABOUT 1.0 TO ABOUT 3.0 WEIGHT PERCENT OF DINONYLSODIUM-SULFOSUCCINATE, ABOUT 1.0 TO ABOUT 3.0 WIGHT PERCENT OF SAID COMPOSITION OF 4,4''-THIO-BIS-(3-METHYL-6-TERTBUTYLPHENOL), ABOUT 35 TO 50 WEIGHT PERCENT OF SAID COMPOSITION OF WHITE MINERAL OIL HAVING A BOILING POINT OF BETWEEN 510*F. AND 620*F. WHEREIN AT LEAST ABOUT 0.15 TO ABOUT 0.30 WEIGHT PERCENT IS RETAINED ON SAID YARN, AND THEN TREATING SAID YARN WITH FROM ABOUT 0.7 TO ABOUT 1.2 WEIGHT PERCENT ON SAID YARN OF A LIQUID COMPOSITION SELECTED FROM THE GROPU CONSISTING OF (A) ABOUT 95 TO ABOUT 98 WEIGHT PERCENT OF SAID COMPOSITION OF TRIETHYLENE GLYCOL-DIPELARGONATE AND ABOUT 2 TO ABOUT 5 WEIGHT PERCENT OF SAID COMPOSITION OF 2,2''METHYLENE-BIS-(4METHYL-6-TERT NONYLPHENOL), AND (B) ABOUT 13 TO ABOUT 25 WEIGHT PERCENT OF SAID COMPOSITION SELECTED FROM THE GROUP CONSISTING OF GLYCEROL MONOLEATE AND DECAGLYCEROL TETRAOLEATE WITH ETHOXYLATED TALL OIL FATTY ACIDS, ABOUT 12 TO ABOUT 20 WEIGHT PERCENT OF SAID COMPOSITION SELECTED FROM THE GROUP CONSISTING OF SULFATED GLYCEROL TRIOLEATE AND ETHOXYLATED ALKYLAMINE, AND ABOUT 55 TO ABOUT 75 WEIGHT PERCENT OF SAID COMPOSITION OF HEXADECYL (ISOCETYL) STEARATE.