公开(公告)号:US20070219334A1
公开(公告)日:2007-09-20
申请号:US11686444
申请日:2007-03-15
申请人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa Wilson Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , XiaoHua Qiu , Angela N. Taha
发明人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa Wilson Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , XiaoHua Qiu , Angela N. Taha
IPC分类号: C08F210/00
CPC分类号: C08F210/06 , C08F297/08 , C08F297/083 , C08F210/16 , C08F2500/03
摘要: Embodiments of the invention provide a class of propylene/α-olefin block interpolymers. The propylene/α-olefin interpolymers are characterized by an average block index, ABI, which is greater than zero and up to about 1.0 and a molecular weight distribution, Mw/Mn, greater than about 1.3. Preferably, the block index is from about 0.2 to about 1. In addition or alternatively, the block propylene/α-olefin interpolymer is characterized by having at least one fraction obtained by Temperature Rising Elution Fractionation (“TREF”), wherein the fraction has a block index greater than about 0.3 and up to about 1.0 and the propylene/α-olefin interpolymer has a molecular weight distribution, Mw/Mn, greater than about 1.3.
摘要翻译: 本发明的实施方案提供一类丙烯/α-烯烃嵌段互聚物。 丙烯/α-烯烃互聚物的特征在于平均嵌段指数ABI,其大于零且高达约1.0,分子量分布为M 1 / M 2, SUB>,大于约1.3。 优选地,嵌段指数为约0.2至约1.另外或替代地,嵌段丙烯/α-烯烃互聚物的特征在于具有通过升温洗脱分级(“TREF”)获得的至少一个级分,其中级分具有 大于约0.3且高达约1.0的嵌段指数,并且所述丙烯/α-烯烃互聚物具有大于约1.3的分子量分布,M分子量/ M n 。
-
公开(公告)号:US08273838B2
公开(公告)日:2012-09-25
申请号:US11686444
申请日:2007-03-15
申请人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa Wilson Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , XiaoHua Qiu , Angela N. Taha
发明人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa Wilson Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , XiaoHua Qiu , Angela N. Taha
IPC分类号: C08F210/06 , C08F4/659
CPC分类号: C08F210/06 , C08F297/08 , C08F297/083 , C08F210/16 , C08F2500/03
摘要: Embodiments of the invention provide a class of propylene/α-olefin block interpolymers. The propylene/α-olefin interpolymers are characterized by an average block index, ABI, which is greater than zero and up to about 1.0 and a molecular weight distribution, Mw/Mn, greater than about 1.3. Preferably, the block index is from about 0.2 to about 1. In addition or alternatively, the block propylene/α-olefin interpolymer is characterized by having at least one fraction obtained by Temperature Rising Elution Fractionation (“TREF”), wherein the fraction has a block index greater than about 0.3 and up to about 1.0 and the propylene/α-olefin interpolymer has a molecular weight distribution, Mw/Mn, greater than about 1.3.
摘要翻译: 本发明的实施方案提供一类丙烯/α-烯烃嵌段互聚物。 丙烯/α-烯烃互聚物的特征在于平均嵌段指数ABI,其大于零且高达约1.0,分子量分布Mw / Mn大于约1.3。 优选地,嵌段指数为约0.2至约1.另外或替代地,嵌段丙烯/α-烯烃互聚物的特征在于具有通过升温洗脱分级(“TREF”)获得的至少一个馏分,其中部分具有 大于约0.3且高达约1.0的嵌段指数,丙烯/α-烯烃互聚物的分子量分布Mw / Mn大于约1.3。
-
公开(公告)号:US07893166B2
公开(公告)日:2011-02-22
申请号:US12558234
申请日:2009-09-11
申请人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa Wilson Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , Xiao Hua Qiu , Angela N. Taha
发明人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa Wilson Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , Xiao Hua Qiu , Angela N. Taha
IPC分类号: C08F293/00 , C08F255/00
CPC分类号: C08F212/08
摘要: Embodiments of the invention provide a class of ethylene/α-olefin block interpolymers. The ethylene/α-olefin interpolymers are characterized by an average block index, ABI, which is greater than zero and up to about 1.0 and a molecular weight distribution, Mw/Mn, greater than about 1.3. Preferably, the block index is from about 0.2 to about 1. In addition or alternatively, the block ethylene/α-olefin interpolymer is characterized by having at least one fraction obtained by Temperature Rising Elution Fractionation (“TREF”), wherein the fraction has a block index greater than about 0.3 and up to about 1.0 and the ethylene/α-olefin interpolymer has a molecular weight distribution, Mw/Mn, greater than about 1.3.
摘要翻译: 本发明的实施方案提供一类乙烯/α-烯烃嵌段互聚物。 乙烯/α-烯烃互聚物的特征在于平均嵌段指数ABI,其大于零且高达约1.0,分子量分布Mw / Mn大于约1.3。 优选地,嵌段指数为约0.2至约1.另外或替代地,嵌段乙烯/α-烯烃互聚物的特征在于具有通过升温洗脱分级(“TREF”)获得的至少一个馏分,其中部分具有 大于约0.3且高达约1.0的嵌段指数,并且乙烯/α-烯烃互聚物的分子量分布Mw / Mn大于约1.3。
-
公开(公告)号:US20100069574A1
公开(公告)日:2010-03-18
申请号:US12558234
申请日:2009-09-11
申请人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa W. Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , Xiahua Qiu , Angela N. Taha
发明人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa W. Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , Xiahua Qiu , Angela N. Taha
IPC分类号: C08F293/00
CPC分类号: C08F212/08
摘要: Embodiments of the invention provide a class of ethylene/α-olefin block interpolymers. The ethylene/α-olefin interpolymers are characterized by an average block index, ABI, which is greater than zero and up to about 1.0 and a molecular weight distribution, Mw/Mn, greater than about 1.3. Preferably, the block index is from about 0.2 to about 1. In addition or alternatively, the block ethylene/α-olefin interpolymer is characterized by having at least one fraction obtained by Temperature Rising Elution Fractionation (“TREF”), wherein the fraction has a block index greater than about 0.3 and up to about 1.0 and the ethylene/α-olefin interpolymer has a molecular weight distribution, Mw/Mn, greater than about 1.3.
摘要翻译: 本发明的实施方案提供一类乙烯/α-烯烃嵌段互聚物。 乙烯/α-烯烃互聚物的特征在于平均嵌段指数ABI,其大于零且高达约1.0,分子量分布Mw / Mn大于约1.3。 优选地,嵌段指数为约0.2至约1.另外或替代地,嵌段乙烯/α-烯烃互聚物的特征在于具有通过升温洗脱分级(“TREF”)获得的至少一个馏分,其中部分具有 大于约0.3且高达约1.0的嵌段指数,并且乙烯/α-烯烃互聚物的分子量分布Mw / Mn大于约1.3。
-
公开(公告)号:US07608668B2
公开(公告)日:2009-10-27
申请号:US11376835
申请日:2006-03-15
申请人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa W. Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , Xiahua Qui , Angela N. Taha
发明人: Colin Li Pi Shan , Lonnie G. Hazlitt , Yunwa W. Cheung , Benjamin C. Poon , Phillip D. Hustad , Roger L. Kuhlman , Edmund M. Carnahan , Xiahua Qui , Angela N. Taha
IPC分类号: C08L23/00 , C08L23/04 , C08F210/00 , C08F210/16
CPC分类号: C08F212/08
摘要: Embodiments of the invention provide a class of ethylene/α-olefin block interpolymers. The ethylene/α-olefin interpolymers are characterized by an average block index, ABI, which is greater than zero and up to about 1.0 and a molecular weight distribution, Mw/Mn, greater than about 1.3. Preferably, the block index is from about 0.2 to about 1. In addition or alternatively, the block ethylene/α-olefin interpolymer is characterized by having at least one fraction obtained by Temperature Rising Elution Fractionation (“TREF”), wherein the fraction has a block index greater than about 0.3 and up to about 1.0 and the ethylene/α-olefin interpolymer has a molecular weight distribution, Mw/Mn, greater than about 1.3.
摘要翻译: 本发明的实施方案提供一类乙烯/α-烯烃嵌段互聚物。 乙烯/α-烯烃互聚物的特征在于平均嵌段指数ABI,其大于零且高达约1.0,分子量分布Mw / Mn大于约1.3。 优选地,嵌段指数为约0.2至约1.另外或替代地,嵌段乙烯/α-烯烃互聚物的特征在于具有通过升温洗脱分级(“TREF”)获得的至少一个馏分,其中部分具有 大于约0.3且高达约1.0的嵌段指数,并且乙烯/α-烯烃互聚物的分子量分布Mw / Mn大于约1.3。
-
公开(公告)号:US07985593B2
公开(公告)日:2011-07-26
申请号:US11794417
申请日:2006-01-19
申请人: David T. Gillespie , Colin Li Pi Shan , Lonnie G. Hazlitt , Alexander W. DeGroot , Peter B. Arnoudse , Charles Allen Williams
发明人: David T. Gillespie , Colin Li Pi Shan , Lonnie G. Hazlitt , Alexander W. DeGroot , Peter B. Arnoudse , Charles Allen Williams
CPC分类号: G01N30/468 , G01N25/147 , G01N30/463 , G01N30/54 , G01N33/442 , G01N2030/008 , G01N2030/3007
摘要: Apparatus for GPC/TREF and TREF/GPC characterization of a polymer sample. The apparatus provides for the automated and integrated use of multiple TREF columns and a GPC system employing a multiple flow through detectors. In addition, a method for TREF/GPC characterization of a polymer sample by GPC analysis of TREF fractions at increasing TREF elution temperatures from multiple TREF columns operated in a coordinated and synchronized temperature cycle for increased sample throughput. Also, a method for GPC/TREF characterization of a polymer sample by GPC fractionation followed by TREF fractionation of the GPC fractionations.
摘要翻译: 用于GPC / TREF和TREF / GPC表征聚合物样品的装置。 该装置提供了多个TREF柱的自动化和集成使用以及采用多个流过检测器的GPC系统。 此外,通过在增加TREF洗脱温度的TREF洗脱温度下,通过GPC分析TREF级分,通过在协同和同步的温度循环中操作以提高样品通量的多个TREF柱来对聚合物样品进行TREF / GPC表征的方法。 此外,通过GPC分级随后进行GPC分馏的TREF分馏,GPC / TREF表征聚合物样品的方法。
-
公开(公告)号:US20080166817A1
公开(公告)日:2008-07-10
申请号:US11794417
申请日:2006-01-19
申请人: David T. Gillespie , Colin Li Pi Shan , Lonnie G. Hazlitt , Alexander W. Degroot , Peter B. Arnoudse , Charles Allen Williams
发明人: David T. Gillespie , Colin Li Pi Shan , Lonnie G. Hazlitt , Alexander W. Degroot , Peter B. Arnoudse , Charles Allen Williams
CPC分类号: G01N30/468 , G01N25/147 , G01N30/463 , G01N30/54 , G01N33/442 , G01N2030/008 , G01N2030/3007
摘要: Apparatus for GPC/TREF and TREF/GPC characterization of a polymer sample. The apparatus provides for the automated and integrated use of multiple TREF columns and a GPC system employing a multiple flow through detectors. In addition, a method for TREF/GPC characterization of a polymer sample by GPC analysis of TREF fractions at increasing TREF elution temperatures from multiple TREF columns operated in a coordinated and synchronized temperature cycle for increased sample throughput. Also, a method for GPC/TREF characterization of a polymer sample by GPC fractionation followed by TREF fractionation of the GPC fractionations.
摘要翻译: 用于GPC / TREF和TREF / GPC表征聚合物样品的装置。 该装置提供了多个TREF柱的自动化和集成使用以及采用多个流过检测器的GPC系统。 此外,通过在增加TREF洗脱温度的TREF洗脱温度下,通过GPC分析TREF级分,通过在协同和同步的温度循环中操作以提高样品通量的多个TREF柱来对聚合物样品进行TREF / GPC表征的方法。 此外,通过GPC分级随后进行GPC分馏的TREF分馏,GPC / TREF表征聚合物样品的方法。
-
公开(公告)号:US20110239746A1
公开(公告)日:2011-10-06
申请号:US13160883
申请日:2011-06-15
申请人: David T. Gillespie , Colin Li Pi Shan , Lonnie G. Hazlitt , Alexander W. Degroot , Peter B. Arnoudse , Charles Allen Williams
发明人: David T. Gillespie , Colin Li Pi Shan , Lonnie G. Hazlitt , Alexander W. Degroot , Peter B. Arnoudse , Charles Allen Williams
IPC分类号: G01N30/02
CPC分类号: G01N30/468 , G01N25/147 , G01N30/463 , G01N30/54 , G01N33/442 , G01N2030/008 , G01N2030/3007
摘要: Apparatus for GPC/TREF and TREF/GPC characterization of a polymer sample. The apparatus provides for the automated and integrated use of multiple TREF columns and a GPC system employing a multiple flow through detectors. In addition, a method for TREF/GPC characterization of a polymer sample by GPC analysis of TREF fractions at increasing TREF elution temperatures from multiple TREF columns operated in a coordinated and synchronized temperature cycle for increased sample throughput. Also, a method for GPC/TREF characterization of a polymer sample by GPC fractionation followed by TREF fractionation of the GPC fractionations.
摘要翻译: 用于GPC / TREF和TREF / GPC表征聚合物样品的装置。 该装置提供了多个TREF柱的自动化和集成使用以及采用多个流过检测器的GPC系统。 此外,通过在增加TREF洗脱温度的TREF洗脱温度下,通过GPC分析TREF级分,通过在协同和同步的温度循环中操作以提高样品通量的多个TREF柱来对聚合物样品进行TREF / GPC表征的方法。 此外,通过GPC分级随后进行GPC分馏的TREF分馏,GPC / TREF表征聚合物样品的方法。
-
公开(公告)号:US07579407B2
公开(公告)日:2009-08-25
申请号:US10428353
申请日:2003-05-03
CPC分类号: B32B27/32 , C08J5/18 , C08J2323/10 , C08L23/10 , C08L23/142 , C08L23/16 , C08L101/00 , C08L2205/02 , C08L2207/02 , C09K3/10 , C09K2200/0617 , C09K2200/062 , C08L2666/02 , C08L2666/06
摘要: A unique thermoplastic olefin composition having: (a) at least 40 percent by weight of a propylene-alpha olefin copolymer based on the total weight of polymers in the composition, the propylene-alpha olefin copolymer having at least 60 percent by weight units derived from propylene, at least 6 percent by weight units derived from an alpha olefin, a molecular weight distribution less than 3.5, and a broad composition distribution; and (b) at least 20 percent by weight of a polypropylene based on the total weight of polymers in the composition, the polypropylene having at least 93 percent by weight units derived from propylene, a molecular weight distribution of greater than 3.5, a heat of fusion greater than the heat of fusion exhibited by the propylene-alpha olefin copolymer, and a melting point Tmax of at least 120° C.
摘要翻译: 一种独特的热塑性烯烃组合物,其具有:(a)基于组合物中聚合物总重量的至少40重量%的丙烯-α烯烃共聚物,丙烯-α烯烃共聚物具有至少60重量%的衍生自 丙烯,至少6重量%衍生自α-烯烃的单元,分子量分布小于3.5,并具有宽的组成分布; 和(b)基于组合物中聚合物总重量的至少20重量%的聚丙烯,该聚丙烯具有至少93重量%的衍生自丙烯的单元,分子量分布大于3.5, 熔点大于丙烯-α烯烃共聚物所显示的熔化热,熔点Tmax至少为120℃。
-
公开(公告)号:US07459500B2
公开(公告)日:2008-12-02
申请号:US10429651
申请日:2003-05-05
IPC分类号: C08F8/00
CPC分类号: C09K3/10 , B32B27/32 , C08J5/18 , C08J2323/12 , C08J2367/02 , C08L23/10 , C08L23/142 , C08L23/16 , C08L101/00 , C09K2200/0617 , C09K2200/062 , C08L2666/06
摘要: A unique thermoplastic olefin composition having: (a) at least 40 percent by weight of a propylene-alpha olefin copolymer based on the total weight of polymers in the composition, the propylene-alpha olefin copolymer having at least 60 percent by weight units derived from propylene, at least 6 percent by weight units derived from an alpha olefin, a molecular weight distribution less than 3.5, and a broad composition distribution; and (b) at least 20 percent by weight of a polypropylene based on the total weight of polymers in the composition, the polypropylene having at least 93 percent by weight units derived from propylene, a molecular weight distribution of greater than 3.5, a heat of fusion greater than the heat of fusion exhibited by the propylene-alpha olefin copolymer, and a melting point Tmax of at least 120° C.