Abstract:
A low-loss optical fiber over wide wavelength range includes a transmission loss of less than or equal to 40 dB/km in a whole wavelength range of 400-1400 nm, and being manufactured by drawing an optical fiber preform including a core composed of a silica glass having a hydroxyl-group concentration of less than or equal to 1 ppm and a cladding composed of a silica glass having a fluorine concentration of more than or equal to 3.2 wt %.
Abstract:
A multicore polarization-maintaining fiber 10 includes a plurality of cores 11, a cladding 12 surrounding the plurality of cores 11, and a plurality of stress applying parts 15 provided sandwiching the plurality of cores 11 in a region surrounded by the outer circumferential surface of the cladding 12. The cross sectional area of the stress applying part 15 is greater than the cross sectional area of the core 11. Stress applying parts 15 of the plurality of stress applying parts 15 are disposed in a first direction, and stress applying parts 15 of the plurality of stress applying parts 15 are disposed in a second direction different from the first direction.
Abstract:
A polarization-maintaining optical fiber of the present invention includes a core, a pair of stress-applying parts provided on both sides of the core, and a cladding surrounding the core and the stress-applying parts, and is used in a wavelength range of 400 to 680 nm. The diameter of the cladding is 125 μm, the diameter of the stress-applying part is 33 to 37 μm, a distance between the pair of stress-applying parts is 8.6 to 15.4 μm, a relative refractive index difference between the core and the cladding is 0.35 to 0.45%, and a cut-off wavelength is less than or equal to 400 nm.