METHOD FOR AMMONIUM-ENHANCED FLUE GAS DESULFURIZATION BY USING RED MUD SLURRY

    公开(公告)号:US20200299207A1

    公开(公告)日:2020-09-24

    申请号:US16821043

    申请日:2020-03-17

    Abstract: The present invention discloses a method for ammonium-enhanced flue gas desulfurization (FGD) by using red mud slurry. The method specifically includes: crushing red mud, sieving the crushed red mud, slurrying the red mud, conducting aeration treatment, adding an ammonium salt and/or ammonia, and conducting natural sedimentation to obtain pretreated red mud slurry and pretreated red mud liquor; adding an ammonium salt and/or ammonia to the slurry, adding water and conducting uniform mixing, conducting pre-FGD, conducting deep desulfurization on treated flue gas by using the pretreated red mud liquor, and directly discharging desulfurized flue gas; and charging the pretreated red mud slurry and the pretreated red mud liquor obtained after the treatment to a replacement tank below, adding lime milk to the replacement tank, conducting stirring and natural sedimentation, conducting soilization on subnatant thick red mud slurry, and refluxing the supernatant to a red mud aeration tank.

    Method For Detoxifying Chromium Slag By Using High Sulfur Coal

    公开(公告)号:US20200282252A1

    公开(公告)日:2020-09-10

    申请号:US16809685

    申请日:2020-03-05

    Abstract: The present invention discloses a method for detoxifying chromium slag by using high sulfur coal. The method includes: sieving chromium slag into coarse-grained chromium slag and fine-grained chromium slag, air-drying and crushing both the coarse-grained chromium slag and the fine-grained chromium slag; separately mixing the crushed coarse-grained chromium slag and fine-grained chromium slag with the crushed high sulfur coal uniformly; adjusting pH values of a coarse-grained slag mixture and a fine-grained slag mixture to 8.0-11.0 and moisture content thereof to 12%-18%; conducting reduction on the treated coarse-grained slag mixture and fine-grained slag mixture, where the reduction temperature of the fine-grained slag mixture is 500-700° C., the reduction time of the fine-grained slag mixture is 10-30 min, the reduction temperature of the coarse-grained slag mixture is 800-1000° C., the reduction time of the coarse-grained slag mixture is 10-30 min; after the reduction, conducting water quenching, and discharging the product.

Patent Agency Ranking