摘要:
Disclosed herein is a method that includes mixing opacifying agent particles with a thickening agent to form a first mixture; the mixing being conducted at a shear rate of about 10 to about 2,000 sec−1; the first mixture having a viscosity of greater than or equal to about 70 Krebs units; and mixing a polymer latex binder with the first mixture to form a coating composition; the polymer latex binder including a copolymer that comprises phosphorus containing repeat units and an acrylate polymer.
摘要:
Disclosed herein is a method that includes mixing opacifying agent particles with a thickening agent to form a first mixture; the mixing being conducted at a shear rate of about 10 to about 2,000 sec−1; the first mixture having a viscosity of greater than or equal to about 70 Krebs units; and mixing a polymer latex binder with the first mixture to form a coating composition; the polymer latex binder including a copolymer that comprises phosphorus containing repeat units and an acrylate polymer.