公开(公告)号:US12103082B2
公开(公告)日:2024-10-01
申请号:US17631073
申请日:2020-09-24
Applicant: Toho Titanium Co., Ltd.
Inventor: Masahiro Morita , Masashi Hayakawa , Yosuke Inoue , Hideki Fujii
CPC classification number: B22F3/15 , B22F1/05 , B22F3/04 , B22F2301/205 , B22F2304/10 , B33Y80/00
Abstract: A method for producing a metallic green compact 61 relates to a method for producing the green compact 61 having at least one recess 62, including a step of subjecting a raw material powder filled in a resin mold 1 to cold isostatic pressing while placing a resin core material 11 having a shape corresponding to the recess 62 at a position corresponding to the recess 62 in the resin mold 1.
-
公开(公告)号:US20220274167A1
公开(公告)日:2022-09-01
申请号:US17631073
申请日:2020-09-24
Applicant: Toho Titanium Co., Ltd.
Inventor: Masahiro Morita , Masashi Hayakawa , Yosuke Inoue , Hideki Fujii
Abstract: A method for producing a metallic green compact 61 relates to a method for producing the green compact 61 having at least one recess 62, including a step of subjecting a raw material powder filled in a resin mold 1 to cold isostatic pressing while placing a resin core material 11 having a shape corresponding to the recess 62 at a position corresponding to the recess 62 in the resin mold 1.
-
公开(公告)号:US11502305B2
公开(公告)日:2022-11-15
申请号:US16960230
申请日:2018-03-19
Applicant: TOHO TITANIUM CO., LTD.
Inventor: Masashi Hayakawa , Syogo Tsumagari
Abstract: To provide a titanium-based porous body that has high void fraction to ensure gas permeability and water permeability for practical use as an electrode and a filter, has a large specific surface area to ensure conductivity and sufficient reaction sites with a reaction solution or a reaction gas, thus showing excellent reaction efficiency, and contains less contaminants because of no organic substance used. A titanium-based porous body having a specific void fraction and a high specific surface area is obtained by filling an irregular-shaped titanium powder having an average particle size of 10 to 50 μm in a dry system without using any binder or the like into a thickness of 4.0×10−1 to 1.6 mm, and sintering the irregular-shaped titanium powder at 800 to 1100° C.
-
-