Process for producing aromatic liquid crystalline polyester and film thereof
    1.
    发明授权
    Process for producing aromatic liquid crystalline polyester and film thereof 失效
    芳香族液晶聚酯的制造方法及其膜

    公开(公告)号:US06656578B2

    公开(公告)日:2003-12-02

    申请号:US10238597

    申请日:2002-09-11

    IPC分类号: B32B1502

    摘要: Provided is a process for producing an aromatic liquid crystalline polyester comprising the steps of: charging 80 20 mol % of a compound represented by the following formula (I) and 20 to 80 mol % of a compound represented by the following formula (II) into a reaction vessel; conducting polycondensation reaction at a temperature from 270 to 350° C. to produce a aromatic liquid crystalline polyester; discharging the aromatic liquid crystalline polyester in a molten state from the reaction vessel and solidifying; then, pulverizing the solidified polyester into particles; and heat-treating at a temperature from 200 to 310° C., The aromatic liquid crystalline polyester has improved low temperature molding processability, and the film thereof has sufficient heat-resistance and excellent gas barrier properties.

    摘要翻译: 本发明提供一种芳香族液晶聚酯的制造方法,其特征在于,将下述通式(I)表示的化合物20 20摩尔%,下述式(II)表示的化合物20〜80摩尔%添加到 反应容器; 在270〜350℃的温度下进行缩聚反应,生成芳族液晶聚酯; 将熔融状态的芳族液晶聚酯从反应容器中排出并固化; 然后将固化的聚酯粉碎成颗粒; 在200〜310℃的温度下进行热处理。芳香族液晶聚酯具有改善的低温成型加工性,其膜具有充分的耐热性和优异的阻气性。

    Process for producing aromatic liquid crystalline polyester and film thereof
    2.
    发明授权
    Process for producing aromatic liquid crystalline polyester and film thereof 失效
    芳香族液晶聚酯的制造方法及其膜

    公开(公告)号:US06528164B1

    公开(公告)日:2003-03-04

    申请号:US09649061

    申请日:2000-08-29

    IPC分类号: B32B1502

    摘要: Provided is a process for producing an aromatic liquid crystalline polyester comprising the steps of: charging 80 to 20 mol % of a compound represented by the following formula (I) and 20 to 80 mol % of a compound represented by the following formula (II) into a reaction vessel; conducting polycondensation reaction at a temperature from 270 to 350° C. to produce an aromatic liquid crystalline polyester; discharging the aromatic liquid crystalline polyester in a molten state from the reaction vessel and solidifying; then, pulverizing the solidified polyester into particles; and heat-treating at a temperature from 200 to 310° C., The aromatic liquid crystalline polyester has improved low temperature molding processability, and the film thereof has sufficient heat-resistance and excellent gas barrier properties.