Abstract:
An object is to provide a magnetic filler composed of the ferrite particles having a low apparent density, capable of maintaining various properties in a controllable state and a specified volume is filled with a small weight, and a resin molded product made using the magnetic filler. To achieve the object, a magnetic filler composed of the ferrite particles having an outer shell structure containing a Ti oxide and a resin laminate made using the magnetic filler are employed.
Abstract:
An object of the present invention is to provide a carrier in which decrease in specific gravity is achieved and a volatile organic compound (VOC) is reduced and to provide an electrophotographic developer using the carrier. There is provided a carrier including a core material coated with a resin, the core material including a magnetic component and a nonmagnetic component, wherein the sum total of volatile organic compounds is 1 ppb or more and 1.5 ppm or less. There is also provided an electrophotographic developer using the carrier.
Abstract:
A porous ferrite core material for an electrophotographic developer wherein the apparent density thereof is 1.5 to 1.9 g/cm3, the shape factor SF-2 thereof is 101 to 110 and the magnetization as measured with a VSM at 1K·1000/4π·A/m is 40 to 60 Am2/kg, a resin-coated ferrite carrier for an electrophotographic developer obtained by coating the surface of the porous ferrite core material with a resin, and an electrophotographic developer using the ferrite carrier.
Abstract translation:一种用于电子照相显影剂的多孔铁氧体芯材料,其表观密度为1.5至1.9g / cm 3,其形状系数SF-2为101至110,并且以1K·1000/4& / m为40〜60Am 2 / kg,通过用树脂涂布多孔铁素体芯材的表面而得到的电子照相显影剂用树脂被覆铁氧体载体和使用该铁氧体载体的电子照相显影剂。
Abstract:
Disclosed are a resin-filled ferrite carrier core material for an electrophotographic developer, including a porous ferrite particle having an average compression strength of 100 mN or more and a coefficient of variation of the compression strength of 50% or less, a ferrite carrier obtained by filling a resin in the voids of the ferrite carrier core material, and an electrophotographic developer using the ferrite carrier.
Abstract:
There is provided a resin-filled ferrite carrier for an electrophotographic developer, in which a void of a porous ferrite particle used as a ferrite carrier core material is filled with silicone resin, wherein a true specific gravity (Y) of the porous ferrite particle filled with the silicone resin and a Si/Fe value (X) measured by fluorescent X-ray elemental analysis satisfy the following inequality (1): −350X≦Y−4.83≦−100X (1).
Abstract:
Provided is a resin-coated carrier for an electrophotographic developer, wherein the surface of a magnetic particle is coated with a mixed resin composed of two resins, and when the two resins are denoted by the resin 1 and the resin 2, respectively, the relative difference between the respective adsorbed moisture amounts of the resin 1 and the resin 2 at a temperature of 30° C. and a relative humidity of 80% satisfies the following formula (1): 1≦|ax−b(100−x)|≦10 (1) a: the adsorbed moisture content (% by weight) of the resin 1 b: the adsorbed moisture content (% by weight) of the resin 2 x: the content percentage of the resin 1 (0
Abstract:
Disclosed are a resin-filled ferrite carrier core material for an electrophotographic developer, including a porous ferrite particle having an average compression strength of 100 mN or more and a coefficient of variation of the compression strength of 50% or less, a ferrite carrier obtained by filling a resin in the voids of the ferrite carrier core material, and an electrophotographic developer using the ferrite carrier.
Abstract:
A carrier for an electrophotographic developer comprising spherical magnetic core particles which have a volume average particle size of 25 to 45 nullm, an average void size of 10 to 20 nullm, a volume based particle size distribution having less than 1% of 22 nullm or smaller particles, a magnetization of 67 to 88 emu/g in a magnetic field of 1 kOe, and a difference of 10 emu/g or smaller in magnetization in a magnetic field of 1 kOe between scattered particles and remaining particles.
Abstract:
A carrier for an electrophotographic developer which comprises a carrier core and a resin coat having a conducting agent dispersed therein, the resin coat having an inner layer on the carrier core side and an outer layer coating the inner layer, wherein the inner layer contains 7 to 20% by weight of a conducting agent based on the resinous solid content of the inner layer, the outer layer contains 3 to 15% by weight of a conducting agent based on the resinous solid content of the outer layer, and the conducting agent content of the inner layer is greater than that of the outer layer.