Systems and methods for cooling optical fiber
    11.
    发明授权
    Systems and methods for cooling optical fiber 有权
    光纤冷却系统和方法

    公开(公告)号:US08230704B2

    公开(公告)日:2012-07-31

    申请号:US12911054

    申请日:2010-10-25

    CPC classification number: C03B37/10 C03B37/02718 Y10T29/49391

    Abstract: In one embodiment, an optical fiber cooling system includes a first cooling tube oriented substantially in parallel with and spaced apart from a second cooling tube such that an optical fiber pathway is positioned between the first cooling tube and the second cooling tube. The first cooling tube includes a plurality of cooling fluid outlets positioned along an axial length of the first cooling tube which are oriented to direct a flow of cooling fluid across the optical fiber pathway towards the second cooling tube. The second cooling tube includes a plurality of cooling fluid outlets positioned along an axial length of the second cooling tube which are oriented to direct a flow of cooling fluid across the optical fiber pathway towards the first cooling tube.

    Abstract translation: 在一个实施例中,光纤冷却系统包括基本上与第二冷却管平行并间隔开的第一冷却管,使得光纤通路位于第一冷却管和第二冷却管之间。 第一冷却管包括沿着第一冷却管的轴向长度定位的多个冷却流体出口,其被定向成将冷却流体的流动横跨光纤通路朝向第二冷却管。 第二冷却管包括沿着第二冷却管的轴向长度定位的多个冷却流体出口,其被定向成将冷却流体的流动横跨光纤通路朝着第一冷却管引导。

    Fiber air turn for low attenuation fiber
    13.
    发明申请
    Fiber air turn for low attenuation fiber 有权
    纤维空气转向低衰减光纤

    公开(公告)号:US20090139270A1

    公开(公告)日:2009-06-04

    申请号:US11998366

    申请日:2007-11-29

    CPC classification number: C03B37/02718 C03B37/032 C03B2205/42 Y02P40/57

    Abstract: A method for forming an optical fiber includes drawing the optical fiber from a glass supply and treating the fiber by maintaining the optical fiber in a treatment zone wherein the fiber is cooled at a specified cooling rate. The optical fiber treatment reduces the tendency of the optical fiber to increase in attenuation due to Rayleigh scattering, and/or over time following formation of the optical fiber due to heat aging. Methods for producing optical fibers along nonlinear paths incorporating fluid bearings are also provided thereby allowing for increased vertical space for the fiber treatment zone.

    Abstract translation: 一种形成光纤的方法包括:从玻璃供给部拉出光纤,并通过将光纤维持在处理区域进行处理,其中纤维以特定的冷却速度被冷却。 光纤处理降低了由于瑞利散射引起的光纤衰减增加的趋势,和/或随着热老化形成光纤的时间的延长。 还提供了沿着包含流体轴承的非线性路径生产光纤的方法,从而允许增加纤维处理区的垂直空间。

    Methods and systems for producing thermoplastic coated optical fibers
    14.
    发明授权
    Methods and systems for producing thermoplastic coated optical fibers 有权
    生产热塑性涂层光纤的方法和系统

    公开(公告)号:US08541064B2

    公开(公告)日:2013-09-24

    申请号:US12469316

    申请日:2009-05-20

    CPC classification number: C03C25/106 C03C25/1065 C03C25/18

    Abstract: A method for producing a coated optical fiber may include drawing an optical fiber from a draw furnace along a first vertical pathway. The optical fiber may then be routed through at least one fluid bearing thereby redirecting the optical fiber along a second vertical pathway. Thereafter, a thermoplastic coating may be applied to the optical fiber with a thermoplastic coating system. The optical fiber may then be wound onto a fiber storage spool with a fiber take-up system. The fiber take-up system may be space apart from the thermoplastic coating system such that the thermoplastic coating may be cooled before the optical fiber is wound onto the fiber storage spool.

    Abstract translation: 涂覆光纤的制造方法可以包括沿着第一垂直路径从拉制炉拉制光纤。 然后可以将光纤穿过至少一个流体轴承,从而沿着第二垂直路径重定向光纤。 此后,热塑性涂层可以用热塑性涂层系统施加到光纤上。 然后可以用光纤卷绕系统将光纤卷绕到光纤存储卷轴上。 纤维卷取系统可以是与热塑性涂层体系分开的空间,使得热塑性涂层可以在光纤被卷绕到纤维存储卷轴之前被冷却。

    METHOD FOR PRODUCTING OPTICAL FIBER AT REDUCED PRESSURE
    15.
    发明申请
    METHOD FOR PRODUCTING OPTICAL FIBER AT REDUCED PRESSURE 有权
    降低压力生产光纤的方法

    公开(公告)号:US20110289979A1

    公开(公告)日:2011-12-01

    申请号:US13091376

    申请日:2011-04-21

    CPC classification number: C03B37/02718 C03B2205/09 Y02P40/57

    Abstract: An optical fiber production system and method are provided for producing optical fiber. An optical fiber is drawn from a preform in a furnace and passes through a treatment device under a reduced pressure in the range of 0.01 to 0.80 atm. The treatment device cools the bare optical fiber as it cools to a temperature in the range of at least 1,600° C. to 1,300° C. A non-contact fiber centering device is located near an exit of the treatment device to provide centering of the optical fiber as it exits the treatment device.

    Abstract translation: 提供了用于制造光纤的光纤生产系统和方法。 在炉中从预成型件中拉出光纤,在0.01〜0.80atm的范围内通过减压处理装置。 处理装置将裸光纤冷却至至少1600℃至1300℃的温度。非接触式光纤定心装置位于处理装置的出口附近,以提供定心 光纤在离开治疗装置时。

    Fiber cure with extended irradiators
    16.
    发明授权
    Fiber cure with extended irradiators 有权
    光纤固化与扩展辐射器

    公开(公告)号:US07963124B2

    公开(公告)日:2011-06-21

    申请号:US12276556

    申请日:2008-11-24

    Abstract: A method for producing an optical fiber that includes a method for producing an optical fiber, said method comprising: (i) drawing a bare optical fiber from a preform along a first pathway at a rate of at least 10 m/sec; (ii) contacting said bare optical fiber with a region of fluid in a fluid bearing and redirecting said bare optical fiber along a second pathway as said bare optical fiber is drawn across said region of fluid cushion; (iii) coating the bare optical fiber; and (iv) irradiating said coated fiber in at least one irradiation zone to at least partially cure said coating, while subjecting the optical fiber to UV light.

    Abstract translation: 一种包括光纤制造方法的光纤的制造方法,所述方法包括:(i)以至少10m /秒的速度沿着第一路径从预成型件拉出裸光纤; (ii)使所述裸光纤与流体轴承中的流体区域接触,并且当所述裸光纤穿过所述流体垫的所述区域时沿着第二路径重定向所述裸光纤; (iii)涂覆裸光纤; 以及(iv)在至少一个照射区域照射所述涂覆的纤维,以使所述光纤经受UV光,同时至少部分地固化所述涂层。

    Methods and Systems For Producing Thermoplastic Coated Optical Fibers
    17.
    发明申请
    Methods and Systems For Producing Thermoplastic Coated Optical Fibers 有权
    生产热塑性涂层光纤的方法和系统

    公开(公告)号:US20090297722A1

    公开(公告)日:2009-12-03

    申请号:US12469316

    申请日:2009-05-20

    CPC classification number: C03C25/106 C03C25/1065 C03C25/18

    Abstract: A method for producing a coated optical fiber may include drawing an optical fiber from a draw furnace along a first vertical pathway. The optical fiber may then be routed through at least one fluid bearing thereby redirecting the optical fiber along a second vertical pathway. Thereafter, a thermoplastic coating may be applied to the optical fiber with a thermoplastic coating system. The optical fiber may then be wound onto a fiber storage spool with a fiber take-up system. The fiber take-up system may be space apart from the thermoplastic coating system such that the thermoplastic coating may be cooled before the optical fiber is wound onto the fiber storage spool.

    Abstract translation: 涂覆光纤的制造方法可以包括沿着第一垂直路径从拉制炉拉制光纤。 然后可以将光纤穿过至少一个流体轴承,从而沿着第二垂直路径重定向光纤。 此后,热塑性涂层可以用热塑性涂层系统施加到光纤上。 然后可以用光纤卷绕系统将光纤卷绕到光纤存储卷轴上。 纤维卷取系统可以是与热塑性涂层体系分开的空间,使得热塑性涂层可以在光纤被卷绕到纤维存储卷轴之前被冷却。

    Method for producing optical fiber using linear non-contact fiber centering
    18.
    发明授权
    Method for producing optical fiber using linear non-contact fiber centering 有权
    使用线性非接触式纤维定心制造光纤的方法

    公开(公告)号:US08973408B2

    公开(公告)日:2015-03-10

    申请号:US13091362

    申请日:2011-04-21

    CPC classification number: C03B37/02718 C03B37/032 C03B2205/09 Y02P40/57

    Abstract: An optical fiber production system and method are provided for producing optical fiber. An optical fiber is drawn from a preform in a furnace and passes through a treatment device under a controlled reduced pressure or partial vacuum in the range of 0.01 to 0.8 atm. The treatment device cools the bare optical fiber as it cools to a temperature range of at least 1,600° C. to 1,300° C. A non-contact fiber centering device is located near an exit of the treatment device to provide linear centering of the optical fiber as it exits the treatment device.

    Abstract translation: 提供了用于制造光纤的光纤生产系统和方法。 在炉中从预成型件中拉出光纤,并在0.01〜0.8atm范围内的受控减压或部分真空下通过处理装置。 裸光纤在冷却至至少1600℃至1300℃的温度范围时,将裸光纤冷却。非接触式光纤定心装置位于处理装置的出口附近,以提供光学 纤维在离开处理装置时。

    Method for producing optical fiber at reduced pressure
    19.
    发明授权
    Method for producing optical fiber at reduced pressure 有权
    降低生产光纤的方法

    公开(公告)号:US08573008B2

    公开(公告)日:2013-11-05

    申请号:US13091376

    申请日:2011-04-21

    CPC classification number: C03B37/02718 C03B2205/09 Y02P40/57

    Abstract: An optical fiber production system and method are provided for producing optical fiber. An optical fiber is drawn from a preform in a furnace and passes through a treatment device under a reduced pressure in the range of 0.01 to 0.80 atm. The treatment device cools the bare optical fiber as it cools to a temperature in the range of at least 1,600° C. to 1,300° C. A non-contact fiber centering device is located near an exit of the treatment device to provide centering of the optical fiber as it exits the treatment device.

    Abstract translation: 提供了用于制造光纤的光纤生产系统和方法。 在炉中从预成型件中拉出光纤,在0.01〜0.80atm的范围内通过减压处理装置。 处理装置将裸光纤冷却至至少1600℃至1300℃的温度。非接触式光纤定心装置位于处理装置的出口附近,以提供定心 光纤在离开治疗装置时。

    Fiber Cure with Extended Irradiators
    20.
    发明申请
    Fiber Cure with Extended Irradiators 有权
    光纤固化与扩展辐射器

    公开(公告)号:US20090139269A1

    公开(公告)日:2009-06-04

    申请号:US12276556

    申请日:2008-11-24

    Abstract: A method for producing an optical fiber that includes a method for producing an optical fiber, said method comprising: (i) drawing a bare optical fiber from a preform along a first pathway at a rate of at least 10 m/sec; (ii) contacting said bare optical fiber with a region of fluid in a fluid bearing and redirecting said bare optical fiber along a second pathway as said bare optical fiber is drawn across said region of fluid cushion; (iii) coating the bare optical fiber; and (iv) irradiating said coated fiber in at least one irradiation zone to at least partially cure said coating, while subjecting the optical fiber to UV light.

    Abstract translation: 一种包括光纤制造方法的光纤的制造方法,所述方法包括:(i)以至少10m /秒的速度沿着第一路径从预成型件拉出裸光纤; (ii)使所述裸光纤与流体轴承中的流体区域接触,并且当所述裸光纤穿过所述流体垫的所述区域时沿着第二路径重定向所述裸光纤; (iii)涂覆裸光纤; 以及(iv)在至少一个照射区域照射所述涂覆的纤维,以使所述光纤经受UV光,同时至少部分地固化所述涂层。