Methods and systems for producing thermoplastic coated optical fibers
    1.
    发明授权
    Methods and systems for producing thermoplastic coated optical fibers 有权
    生产热塑性涂层光纤的方法和系统

    公开(公告)号:US08541064B2

    公开(公告)日:2013-09-24

    申请号:US12469316

    申请日:2009-05-20

    CPC classification number: C03C25/106 C03C25/1065 C03C25/18

    Abstract: A method for producing a coated optical fiber may include drawing an optical fiber from a draw furnace along a first vertical pathway. The optical fiber may then be routed through at least one fluid bearing thereby redirecting the optical fiber along a second vertical pathway. Thereafter, a thermoplastic coating may be applied to the optical fiber with a thermoplastic coating system. The optical fiber may then be wound onto a fiber storage spool with a fiber take-up system. The fiber take-up system may be space apart from the thermoplastic coating system such that the thermoplastic coating may be cooled before the optical fiber is wound onto the fiber storage spool.

    Abstract translation: 涂覆光纤的制造方法可以包括沿着第一垂直路径从拉制炉拉制光纤。 然后可以将光纤穿过至少一个流体轴承,从而沿着第二垂直路径重定向光纤。 此后,热塑性涂层可以用热塑性涂层系统施加到光纤上。 然后可以用光纤卷绕系统将光纤卷绕到光纤存储卷轴上。 纤维卷取系统可以是与热塑性涂层体系分开的空间,使得热塑性涂层可以在光纤被卷绕到纤维存储卷轴之前被冷却。

    METHOD FOR PRODUCTING OPTICAL FIBER AT REDUCED PRESSURE
    2.
    发明申请
    METHOD FOR PRODUCTING OPTICAL FIBER AT REDUCED PRESSURE 有权
    降低压力生产光纤的方法

    公开(公告)号:US20110289979A1

    公开(公告)日:2011-12-01

    申请号:US13091376

    申请日:2011-04-21

    CPC classification number: C03B37/02718 C03B2205/09 Y02P40/57

    Abstract: An optical fiber production system and method are provided for producing optical fiber. An optical fiber is drawn from a preform in a furnace and passes through a treatment device under a reduced pressure in the range of 0.01 to 0.80 atm. The treatment device cools the bare optical fiber as it cools to a temperature in the range of at least 1,600° C. to 1,300° C. A non-contact fiber centering device is located near an exit of the treatment device to provide centering of the optical fiber as it exits the treatment device.

    Abstract translation: 提供了用于制造光纤的光纤生产系统和方法。 在炉中从预成型件中拉出光纤,在0.01〜0.80atm的范围内通过减压处理装置。 处理装置将裸光纤冷却至至少1600℃至1300℃的温度。非接触式光纤定心装置位于处理装置的出口附近,以提供定心 光纤在离开治疗装置时。

    Methods and Systems For Producing Thermoplastic Coated Optical Fibers
    3.
    发明申请
    Methods and Systems For Producing Thermoplastic Coated Optical Fibers 有权
    生产热塑性涂层光纤的方法和系统

    公开(公告)号:US20090297722A1

    公开(公告)日:2009-12-03

    申请号:US12469316

    申请日:2009-05-20

    CPC classification number: C03C25/106 C03C25/1065 C03C25/18

    Abstract: A method for producing a coated optical fiber may include drawing an optical fiber from a draw furnace along a first vertical pathway. The optical fiber may then be routed through at least one fluid bearing thereby redirecting the optical fiber along a second vertical pathway. Thereafter, a thermoplastic coating may be applied to the optical fiber with a thermoplastic coating system. The optical fiber may then be wound onto a fiber storage spool with a fiber take-up system. The fiber take-up system may be space apart from the thermoplastic coating system such that the thermoplastic coating may be cooled before the optical fiber is wound onto the fiber storage spool.

    Abstract translation: 涂覆光纤的制造方法可以包括沿着第一垂直路径从拉制炉拉制光纤。 然后可以将光纤穿过至少一个流体轴承,从而沿着第二垂直路径重定向光纤。 此后,热塑性涂层可以用热塑性涂层系统施加到光纤上。 然后可以用光纤卷绕系统将光纤卷绕到光纤存储卷轴上。 纤维卷取系统可以是与热塑性涂层体系分开的空间,使得热塑性涂层可以在光纤被卷绕到纤维存储卷轴之前被冷却。

    Method for producing optical fiber at reduced pressure
    4.
    发明授权
    Method for producing optical fiber at reduced pressure 有权
    降低生产光纤的方法

    公开(公告)号:US08573008B2

    公开(公告)日:2013-11-05

    申请号:US13091376

    申请日:2011-04-21

    CPC classification number: C03B37/02718 C03B2205/09 Y02P40/57

    Abstract: An optical fiber production system and method are provided for producing optical fiber. An optical fiber is drawn from a preform in a furnace and passes through a treatment device under a reduced pressure in the range of 0.01 to 0.80 atm. The treatment device cools the bare optical fiber as it cools to a temperature in the range of at least 1,600° C. to 1,300° C. A non-contact fiber centering device is located near an exit of the treatment device to provide centering of the optical fiber as it exits the treatment device.

    Abstract translation: 提供了用于制造光纤的光纤生产系统和方法。 在炉中从预成型件中拉出光纤,在0.01〜0.80atm的范围内通过减压处理装置。 处理装置将裸光纤冷却至至少1600℃至1300℃的温度。非接触式光纤定心装置位于处理装置的出口附近,以提供定心 光纤在离开治疗装置时。