Abstract:
There is provided a resin-filled ferrite carrier for an electrophotographic developer, in which a void of a porous ferrite particle used as a ferrite carrier core material is filled with silicone resin, wherein a true specific gravity (Y) of the porous ferrite particle filled with the silicone resin and a Si/Fe value (X) measured by fluorescent X-ray elemental analysis satisfy the following inequality (1): −350X≦Y−4.83≦−100X (1).
Abstract:
It is an object of the present invention to provide a ferrite particle having a low apparent density, and being capable of maintaining various properties thereof in controllable states and filling a fixed volume in a small weight thereof, a ferrite carrier core material and a ferrite carrier for an electrophotographic developer using the ferrite particle, and the like. In order to achieve the object, there are employed the ferrite particle having a porous structure in the interior thereof and an outer shell structure on the outer periphery thereof, the ferrite carrier core material and the ferrite carrier for an electrophotographic developer using the ferrite particle, and an electrophotographic developer using the ferrite carrier.
Abstract:
The present invention provides a dry two-component type developer for electrophotography comprising a carrier particle and a toner particle, wherein a toner water adsorption ratio (T) obtained by a following equation (1) for the toner particle ranges from 1.0 to 7.0 and a carrier water adsorption ratio (C) obtained by a following equation (2) is 20.0 or less, and a water adsorption ratio (T/C) expressed in a following equation (3) representing a relationship between the toner water adsorption ratio (T) and the carrier water adsorption ratio (C) is 5.0 or less;a toner water adsorption ratio (T)nullnulla water adsorption amount (TH) of the toner particle/an N2 adsorption amount (TN) of the toner particlenullnullnull(1),a carrier water adsorption ratio (C)nullnulla water adsorption amount (CH) of the carrier particle/an N2 adsorption amount (CN) of the carrier particlenullnullnull(2), anda water adsorption ratio (T/C)nullnulla toner water adsorption ratio (T)/a carrier water adsorption ratio (C)nullnullnull(3).In the dry two-component type developer for electrophotography according to the present invention, even if use conditions are changed, a developing characteristic is less varied.
Abstract:
Provided are a ferrite powder that suppresses decreases in saturation magnetization and decreases in filler filling ratio and also suppresses inhibition of resin curing, and a method for producing the same. A ferrite powder composed of spherical ferrite particles, wherein the ferrite powder contains iron (Fe) 54.0-70.0 mass % and manganese (Mn) 3.5-18.5 mass %, has an average volume particle size of 2.0-20.0 μm, and has a carbon content of 0.100 mass % or lower.
Abstract:
The present invention provides a ferrite particle containing: a ferrite particle body having a spinel crystal structure belonging to a space group Fd-3m and having a spinel composition represented by the following formula (1); and a coating layer having a spinel crystal structure belonging to the space group Fd-3m and coating a surface of the ferrite particle body, in which the coating layer is a layer obtained by subjecting the ferrite represented by the following formula (1) to a heat treatment, and a content ratio of the coating layer in the ferrite particle obtained by subjecting a powder X-ray diffraction pattern to Rietveld analysis is 5 mass % or more and 35 mass % or less, and the ferrite particle satisfies a specific formula (2). The present invention also provides a carrier for an electrophotographic developer.
Abstract:
A magnetic composite includes a resin base material and a ferrite layer provided on a surface of the resin base material, the resin base material has a thickness of 10 μm or more, and the ferrite layer has a thickness of 2.0 μm or more, contains spinel-type ferrite as a principal component, and has a ratio of 0.00 or more and 0.03 or less, wherein the ratio is of an integrated intensity of a 222 plane to an integrated intensity of a 311 plane in X-ray diffraction analysis.
Abstract:
The present invention relates to a ferrite particle containing a crystal phase component containing a perovskite crystal represented by a compositional formula: RZrO3 (provided that R represents an alkaline earth metal element), having a surface roughness Rz of 0.8 µm or more and 3.5 µm or less, and having a standard deviation Rzσ of the surface roughness Rz falling in a range represented by the following formula 0.15 × Rz ≤ Rzσ ≤ 0.60 × Rz. The ferrite particle can be used as an electrophotographic developer carrier core material. In addition, an electrophotographic developer carrier and an electrophotographic developer can be obtained.
Abstract:
The present invention provides: a ferrite particle containing a crystal phase component containing a perovskite crystal represented by the compositional formula RZrO3 (where R is an alkaline earth metal element); and an electrophotographic developer carrier core material, an electrophotographic developer carrier, and an electrophotographic developer containing the ferrite particles.
Abstract:
Ferrite powder of the present invention is ferrite powder detectable with a metal detector, comprising: soft ferrite particles containing Mn of 3.5 mass % or more and 20.0 mass % or less and Fe of 50.0 mass % or more and 70.0 mass % or less. It is preferable that a volume average particle diameter of the particles constituting the ferrite powder is 0.1 μm or more and 100 μm or less. It is preferable that magnetization by a VSM measurement when magnetic field of 5 K·1000/4πA/m is applied is 85 A·m2/kg or more and 98 A·m2/kg or less.
Abstract:
To provide a magnetic core material for electrophotographic developer and carrier for electrophotographic developer which have small environmental dependence of the electric resistance, can suppress the carrier scattering, and can stably provide good images; a developer contains the carrier; a method for producing the magnetic core material for electrophotographic developer; a method for producing the carrier for electrophotographic developer, and a method for producing the developer. The magnetic core material for electrophotographic developer, satisfying a value of Formula (1): a+b×10+c+d+e+f, being from 20 to 150, when a fluoride ion amount is denoted by a (ppm), a chloride ion amount is denoted by b (ppm), a bromide ion amount is denoted by c (ppm), a nitrite ion amount is denoted by d (ppm), a nitrate ion amount is denoted by e (ppm), and a sulfate ion amount is denoted by f (ppm), which are measured by a combustion ion chromatography method.