Method for producing impact resistant thermoplastic resin by continuous
bulk polymerization
    11.
    发明授权
    Method for producing impact resistant thermoplastic resin by continuous bulk polymerization 失效
    通过连续本体聚合制备耐冲击热塑性树脂的方法

    公开(公告)号:US3981944A

    公开(公告)日:1976-09-21

    申请号:US478535

    申请日:1974-06-12

    CPC分类号: C08F285/00 C08F279/02

    摘要: A method is provided for continuously manufacturing high impact strength thermoplastic resins comprised of the sequential steps of (a) bulk-polymerizing a monomer solution, which contains a diene type rubber polymer or a graft polymer obtained by extracting the rubber polymer particle or vinyl monomer grafted polymer particle in latex with vinyl monomers which contain 5-20 percent by weight of water at a temperature of 85.degree.-135.degree.C, while continuously stirring the solution, vaporizing the volatile components, condensing the volatile component and recycling them back to reaction mixture, until the solid content in the reaction mixture reaches 40-75 percent by weight, and thereafter (b) bulk polymerizing the resulting prepolymer solution under the condition that plug-flowing can be attained with a temperature gradient 100.degree.-170.degree.C at the top of the reaction vessel and 170.degree.-270.degree.C at the bottom thereof, while the volatile component of the mixture are evaporated off, condensed and recycled to the reaction mixture, until the solid content is at least 90 percent by weight.

    摘要翻译: 提供一种用于连续制造高冲击强度热塑性树脂的方法,其包括以下顺序步骤:(a)将含有二烯型橡胶聚合物的单体溶液本体聚合或通过萃取橡胶聚合物颗粒或乙烯基单体接枝而获得的接枝聚合物 乙烯基单体的聚合物颗粒在85℃-135℃的温度下含有5-20重量%的水,同时连续搅拌该溶液,蒸发挥发性组分,将挥发性组分冷凝并回收到反应混合物中 直到反应混合物中的固体含量达到40-75重量%,然后(b)在100-170℃的温度梯度下,在可以实现堵塞流动的条件下将所得预聚物溶液本体聚合 反应容器的顶部和底部为170℃-270℃,同时将混合物的挥发性组分蒸发掉 并将其再循环到反应混合物中,直到固体含量为至少90重量%。