11.
公开(公告)号:US20230174388A1
公开(公告)日:2023-06-08
申请号:US17997827
申请日:2021-05-04
Applicant: BASF SE
IPC: C01G53/00
CPC classification number: C01G53/44 , C01G53/006 , C01P2004/61 , C01P2004/53
Abstract: Process for making a particulate (oxy)hydroxide of TM wherein TM comprises nickel wherein said process comprises the steps of: (a) Providing an aqueous solution (α) containing water-soluble salts of Ni and of at least one transition metal selected from Co and Mn, and, optionally, at least one further metal selected from Ti, Zr, Mo, W, Al, Mg, Nb, and Ta, and an aqueous solution (β) containing an alkali metal hydroxide and, optionally, an aqueous solution (γ) containing ammonia, (b) combining a solution (α) and a solution (β) and, if applicable, a solution (γ) at a pH value in the range of from 12.0 to 13.0, thereby creating solid particles of hydroxide containing nickel, (c) continuing combining solutions (α) and (β) and, if applicable, (γ) at a pH value in the range of from 9.0 to 12.0 and in any way below the pH value in step (b), (d) adding a solution (α) and a solution (β) and, if applicable, a solution (γ) at a pH value in the range of from 12.0 to 12.7 and in any way above the pH value in step (c), (e) continuing combining such solutions (α) and (β) and, if applicable, (γ) at a pH value in the range of from 9.0 to 12.0 and in any way below the pH value in step (d), wherein step (d) has a duration in the range of from rt-0.01 to rt-0.15 and wherein it is the average residence time of the reactor in which steps (b) to (e) are carried out.