Abstract:
The present invention provides a water spot cooling apparatus, a water spot cooling method for casting a mold, a method for manufacturing the water spot cooling apparatus and use of the water spot cooling apparatus. The technical solution of the present invention has the following advantages: spot cooling of multiple spots can be realized on each side mold by using only one water inlet pipeline, thereby saving the water cooling pipeline and facilitating field installation; the water inlet and outlet are integrated on a main body, thereby facilitating field implementation; the whole apparatus is easy to process, convenient to maintain, and low in manufacturing cost; and it is not restricted by the product structure and facilitates promotion.
Abstract:
A wheel and a rim with a weight reduction inner flange are provided. The rim includes an inner flange, a middle portion and an outer flange which are all annular and connected end to end to form an annular rim, in which the inner flange or the outer flange includes multiple groups of edge weight reduction sockets arranged side by side on one side of the inner cavity of a hub, and multiple groups of inner weight reduction sockets arranged side by side are provided inside the edge weight reduction sockets on the rim; a group of edge weight reduction sockets includes a first edge weight reduction socket and a second edge weight reduction socket at the edge of the inner flange or the outer flange, and the first edge weight reduction socket is in the shape of a right-angled triangle having round angles.
Abstract:
A water-cooled mold for low-pressure casting of an aluminum alloy wheel includes an upper mold, a lower mold and a side mold which surround a cavity of aluminum alloy, in which a cooling insert is embedded into a side mold frame of the side mold; an upper parting surface, a lower parting surface and a side parting surface of the cooling insert are respectively in contact parting with the side mold frame, the side parting surface includes a front zone and a rear straight zone, and a gap of 1.5-2.5 mm is formed between the rear straight zone and the side mold frame.
Abstract:
The present application relates to a low-pressure casting multi-sprue process and device for an aluminum alloy wheel. A multi-sprue casting method is adopted, and a plurality of sprues are arranged at the end of the inner flange of a wheel, so that molten aluminum enters at the inner flange first, then enters from a center sprue after a mold cavity at the rim is full of the molten aluminum. The mold assembly is pressurized and cooled after the mold cavity is full of the molten aluminum. During cooling, starting from the outer flange of the wheel filled with the molten aluminum last, side mold ring water coolers are started.
Abstract:
A wheel and a rim with weight reduction sockets are provided. The rim is made of an aluminum alloy and includes an inner flange, a middle portion and an outer flange, the inner flange, middle portion and outer flange are all annular and are connected end to end to form a cylindrical rim, in which weight reduction sockets are provided on the outer surface of the middle portion of the rim; the weight reduction sockets are rectangular ones, and are arranged in lattices in turn; and 3-5 rows of weight reduction sockets are arranged annularly on the outer surface of the middle portion of the rim.
Abstract:
The present disclosure provides a low-pressure cast aluminum wheel mold. The back cavity of a top mold (1) is divided into three parts: the back cavity in a rim area is open, and the wall thickness of the top mold is progressively increased by 15-25 mm from bottom to top; the back cavity in a spoke area is machined in a profile-followed manner, and the top mold has an equal wall thickness of 20-30 mm; at each R angle position where the rim is connected with a spoke, the top mold is provided with a boss (11), the axial wall thickness of the boss (11) is 40-60 mm, and the radial wall thickness is 30-50 mm. A temperature gradient beneficial to progressive solidification of a casting is constructed; by designing an annular water cooling structure at the R angle where the rim is connected with the spoke, quick cooling on the hot spot is specifically realized, the cooling capability is stronger, the cooling range is more exact, bad influence on the adjacent thin-wall part is not produced, and smooth feeding of molten aluminum is ensured.
Abstract:
Disclosed in the present application is a low-pressure casting mold for an aluminum wheel. V-shaped grooves are formed in the cavity surface of a side mold, a cavity is formed in the back cavity of the side mold, a cooling duct is arranged in the cavity of the side mold, and a main air pipe is perpendicular to an annular branch; the annular branch is concentric with a wheel casting, and air pipes are 5-10 mm away from the bottom surface of the cavity; the two ends of the annular branch are welded with plugs; air outlet holes are arranged on the annular branch, and the holes are perpendicular to the bottom surface of the cavity; the diameters of the air outlet holes are 3 mm, and the holes are uniformly distributed at intervals of 10-15 mm in the circumferential direction.
Abstract:
A rim with an inner flange having strip weight reduction sockets and a wheel are provided. The rim includes the inner flange, a middle portion and an outer flange which are all annular and are connected end to end to form an annular rim, in which trapezoidal weight reduction sockets are provided on the inner wall of the inner flange; the bottom edges of the weight reduction sockets are flush with the edge of the inner flange; the top edge of each weight reduction socket has fillets; and the weight reduction sockets have a bottom edge length of 5-30 mm, a height of 15-60 mm, a top edge length of 5-15 mm, a base angle of 72-83°, and a depth of 1-5 mm.
Abstract:
The present disclosure provides a low-pressure cast aluminum wheel mold. The back cavity of a top mold (1) is divided into three parts: the back cavity in a rim area is open, and the wall thickness of the top mold is progressively increased by 15-25 mm from bottom to top; the back cavity in a spoke area is machined in a profile-followed manner, and the top mold has an equal wall thickness of 20-30 mm; at each R angle position where the rim is connected with a spoke, the top mold is provided with a boss (11), the axial wall thickness of the boss (11) is 40-60 mm, and the radial wall thickness is 30-50 mm. A temperature gradient beneficial to progressive solidification of a casting is constructed; by designing an annular water cooling structure at the R angle where the rim is connected with the spoke, quick cooling on the hot spot is specifically realized, the cooling capability is stronger, the cooling range is more exact, bad influence on the adjacent thin-wall part is not produced, and smooth feeding of molten aluminum is ensured.
Abstract:
The present invention relates to a universal clamping device for an inscribing machine, having a frame, a base plate, a cushion plate, a fixed support, a lead screw, a linear guide rail, a guide rail slide carriage, a lead screw nut, a bracket, a mandrel, a protective cap, a driven pulley, a fixed support, a synchronous belt, a driving pulley, a mounting rack and a servo motor. The device provided by the present invention can meet the requirements on inscribing work, and is also featured by being simple in structure, convenient to manufacture and stable in performance.