HIGH-GLOSS MULTILAYER EFFECT PIGMENTS HAVING A NARROW SIZE DISTRIBUTION, AND METHOD FOR THE PRODUCTION THEREOF
    15.
    发明申请
    HIGH-GLOSS MULTILAYER EFFECT PIGMENTS HAVING A NARROW SIZE DISTRIBUTION, AND METHOD FOR THE PRODUCTION THEREOF 有权
    具有窄幅分布的高倍数多层效应颜料及其生产方法

    公开(公告)号:US20110265690A1

    公开(公告)日:2011-11-03

    申请号:US13143386

    申请日:2010-08-09

    IPC分类号: C04B14/20 C04B14/00 B05D1/36

    摘要: Multilayer pearlescent pigments based on platelet-shaped transparent substrates with an optically active coating, where the optically active coating includes at least a) a nonabsorbing high-index layer A having a refractive index n≧1.8, b) a low-index layer B having a refractive index n 150 nm, c) an absorbing high-index layer C having a refractive index n≧1.8 and also, d) optionally an outer protective layer D, wherein the multilayer pearlescent pigments have a cumulative frequency distribution of the volume-averaged size distribution function, with the indices D10, D50, D90 and a span ΔD of 0.7-1.4, the span ΔD being calculated in accordance with the formula ΔD=(D90−D10)/D50. The disclosure further relates to a method for producing these multilayer pigments, and to their use.

    摘要翻译: 基于具有光学活性涂层的片状透明基板的多层珠光颜料,其中光学活性涂层至少包括a)折射率n≥1.8的非吸收性高折射率层A,b)低折射率层B,具有 具有光学层厚度> 150nm的折射率n <1.8,c)折射率n≥1.8的吸收性高折射率层C,以及d)任选的外部保护层D,其中多层珠光颜料具有 体积平均尺寸分​​布函数的累积频率分布,其指数为D10,D50,D90,跨度和Dgr; D为0.7-1.4,跨度和Dgr; D根据公式Dgr计算; D =(D90- D10)/ D50。 本公开还涉及一种用于制备这些多层颜料的方法及其用途。