Flexible substrate for OLED device
    12.
    发明授权
    Flexible substrate for OLED device 有权
    用于OLED器件的柔性基板

    公开(公告)号:US08981363B1

    公开(公告)日:2015-03-17

    申请号:US14016478

    申请日:2013-09-03

    Abstract: Flexible substrates and devices including flexible substrates are provided. In an embodiment, a flexible substrate includes a first glass substrate material and a first organic light emitting device, disposed over the first flexible substrate, which includes a first emissive layer The first flexible substrate may have a thickness of not more than 300 μm, a flexural rigidity of 10−1 Nm to 10−6 Nm, a water vapor transmission rate of not more than 10−6 g per square meter per day, a refractive index of not more than 1.6, a glass transition temperature of at least 300 C, a Young's modulus of 60 to 90 GPa, and/or an optical transmission of at least 85% for light in the range of 400 to 800 nm.

    Abstract translation: 提供了柔性基板和包括柔性基板的装置。 在一个实施例中,柔性基板包括设置在第一柔性基板上的第一玻璃基板材料和第一有机发光器件,该第一有机发光器件包括第一发光层。第一柔性基板可以具有不大于300μm的厚度, 10-1Nm至10-6Nm的弯曲刚度,每天每平方米不超过10-6g的水蒸汽透过率,折射率不大于1.6,玻璃化转变温度至少为300℃ ,40至90GPa的杨氏模量和/或400至800nm范围内的光的透光率至少为85%。

    FLEXIBLE SUBSTRATE FOR OLED DEVICE
    13.
    发明申请
    FLEXIBLE SUBSTRATE FOR OLED DEVICE 有权
    OLED器件柔性基板

    公开(公告)号:US20150060777A1

    公开(公告)日:2015-03-05

    申请号:US14016478

    申请日:2013-09-03

    Abstract: Flexible substrates and devices including flexible substrates are provided. In an embodiment, a flexible substrate includes a first glass substrate material and a first organic light emitting device, disposed over the first flexible substrate, which includes a first emissive layer The first flexible substrate may have a thickness of not more than 300 μm, a flexural rigidity of 10−1 Nm to 10−6 Nm, a water vapor transmission rate of not more than 10−6 g per square meter per day, a refractive index of not more than 1.6, a glass transition temperature of at least 300 C, a Young's modulus of 60 to 90 GPa, and/or an optical transmission of at least 85% for light in the range of 400 to 800 nm.

    Abstract translation: 提供了柔性基板和包括柔性基板的装置。 在一个实施例中,柔性基板包括设置在第一柔性基板上的第一玻璃基板材料和第一有机发光器件,该第一有机发光器件包括第一发光层。第一柔性基板可以具有不大于300μm的厚度, 10-1Nm至10-6Nm的弯曲刚度,每天每平方米不超过10-6g的水蒸汽透过率,折射率不大于1.6,玻璃化转变温度至少为300℃ ,40至90GPa的杨氏模量和/或400至800nm范围内的光的透光率至少为85%。

Patent Agency Ranking