METHOD FOR RAISING LUMINOUS EFFICIENCY OF FIELD EMISSIVE LUMINESCENT MATERIAL, LUMINESCENT GLASS ELEMENT AND THE PREPARING METHOD THEREOF
    45.
    发明申请
    METHOD FOR RAISING LUMINOUS EFFICIENCY OF FIELD EMISSIVE LUMINESCENT MATERIAL, LUMINESCENT GLASS ELEMENT AND THE PREPARING METHOD THEREOF 有权
    提高场致发光材料的发光效率的方法,发光玻璃元件及其制备方法

    公开(公告)号:US20120077025A1

    公开(公告)日:2012-03-29

    申请号:US13376385

    申请日:2009-06-23

    IPC分类号: B32B17/06 B05D5/06

    摘要: A method for raising luminous efficiency of field emissive luminescent material, a luminescent glass element and the preparing method thereof are provided. The method for raising luminous efficiency of field emissive luminescent material comprises: forming a nonperiodic metal film having metal micro-nano structure on the surface of a luminescent glass body having a composition of aM2O.bY2O3.cSiO2.dTb2O3; eradiating cathode ray to the metal film, and the cathode ray penetrating the metal film to make the glass body to luminesce. The luminescent glass element has a luminescent glass body, and a nonperiodic metal film having metal micro-nano structure forming on the glass body. The preparing method of the element comprises: preparing a luminescent glass body, forming a metal film on the surface of the luminescent glass body, annealing and cooling to obtain the luminescent glass element. The luminescent glass element in the invention has good transmissivity, high homogenization and luminous efficiency, good stability and simple structure. The preparing method thereof is simple and has a low cost.

    摘要翻译: 提供了一种提高场致发光材料的发光效率的方法,发光玻璃元件及其制备方法。 用于提高场致发光发光材料的发光效率的方法包括:在具有M 2 O·b Y 2 O 3·c SiO 2·d·Tb 2 O 3组成的发光玻璃体的表面上形成具有金属微纳米结构的非周期性金属膜; 将阴极射线溅射到金属膜,阴极射入金属膜,使玻璃体发光。 发光玻璃元件具有发光玻璃体,在玻璃体上形成具有金属微纳米结构的非周期性金属膜。 该元件的制备方法包括:制备发光玻璃体,在发光玻璃体的表面上形成金属膜,进行退火和冷却以获得发光玻璃元件。 本发明的发光玻璃元件具有良好的透射率,高均匀性和发光效率,稳定性好,结构简单。 其制备方法简单,成本低。

    LUMINESCENT GLASS ELEMENT, PRODUCING METHOD THEREOF AND LUMINESCING METHOD THEREOF
    46.
    发明申请
    LUMINESCENT GLASS ELEMENT, PRODUCING METHOD THEREOF AND LUMINESCING METHOD THEREOF 有权
    发光玻璃元件及其制造方法及其制造方法

    公开(公告)号:US20120001092A1

    公开(公告)日:2012-01-05

    申请号:US13229546

    申请日:2011-09-09

    摘要: The present invention relates to a luminescent glass element comprising a luminescent glass substrate, which a metal layer is positioned on a surface thereof. The metal layer is provided with a metal microstructure. The luminescent glass substrate has composite oxides represented as the following formula: aM2O.bY2O3.cSiO2.dSm2O3, wherein M represents alkali metal element, a, b, c and d are, by mol part, 25-60, 1-30, 20-70 and 0.001-10 respectively. The present invention also provides a producing method of the luminescent glass element and a luminescing method thereof. The metal layer is positioned on the luminescent glass substrate, thereby improving luminescence efficiency of the luminescent glass substrate. The luminescent glass element can be used in luminescent devices with ultrahigh brightness or high-speed operation.

    摘要翻译: 本发明涉及包含发光玻璃基板的发光玻璃元件,金属层位于其表面上。 金属层设有金属微结构。 发光玻璃基板具有由下式表示的复合氧化物:aM2O.bY2O3.cSiO2.dSm2O3,其中M表示碱金属元素,a,b,c和d分别为25-60,1-30,20 -70和0.001-10。 本发明还提供了发光玻璃元件的制造方法及其发光方法。 金属层位于发光玻璃基板上,从而提高发光玻璃基板的发光效率。 发光玻璃元件可用于具有超高亮度或高速操作的发光装置。

    LUMINESCENT GLASS ELEMENT, PRODUCING METHOD THEREOF AND LUMINESCING METHOD THEREOF
    47.
    发明申请
    LUMINESCENT GLASS ELEMENT, PRODUCING METHOD THEREOF AND LUMINESCING METHOD THEREOF 有权
    发光玻璃元件及其制造方法及其制造方法

    公开(公告)号:US20110315895A1

    公开(公告)日:2011-12-29

    申请号:US13229509

    申请日:2011-09-09

    摘要: The present invention relates to a luminescent glass element comprising a luminescent glass substrate, which a metal layer is positioned on a surface thereof. The metal layer is provided with a metal microstructure. The luminescent glass substrate has composite oxides represented as the following formula: aM2O.bY2O3.cSiO2.dCe2O3, wherein M represents alkali metal element, a, b, c and d are, by mol part, 25-60, 1-30, 20-70 and 0.001-10 respectively. The present invention also provides a producing method of the luminescent glass element and a luminescing method thereof. The metal layer is positioned on the luminescent glass substrate, thereby improving luminescence efficiency of the luminescent glass substrate. The luminescent glass element can be used in luminescent devices with ultrahigh brightness or high-speed operation.

    摘要翻译: 本发明涉及包含发光玻璃基板的发光玻璃元件,金属层位于其表面上。 金属层设有金属微结构。 发光玻璃基板具有由下式表示的复合氧化物:aM2O.bY2O3.cSiO2.dCe2O3,其中M表示碱金属元素,a,b,c和d分别为25-60,1-30,20 -70和0.001-10。 本发明还提供了发光玻璃元件的制造方法及其发光方法。 金属层位于发光玻璃基板上,从而提高发光玻璃基板的发光效率。 发光玻璃元件可用于具有超高亮度或高速操作的发光装置。

    NEW SALTS
    48.
    发明申请
    NEW SALTS 有权
    新销售

    公开(公告)号:US20110257150A1

    公开(公告)日:2011-10-20

    申请号:US13140490

    申请日:2009-12-17

    CPC分类号: A61K31/397 C07D205/04

    摘要: This invention relates to a hydrochloride, malate, oxalate and tartrate salt forms of 1-(4-{1-[(E)-4-cyclohexyl-3-trifluoromethyl-benzyloxyimino]-ethyl}-2-ethyl-benzyl)-azetidine-3-carboxylic acid (Compound I), to pharmaceutical compositions comprising this salt, to processes for forming this salt and to its use in medical treatment. In addition, the present invention also relates to new polymorphic forms of each of these salts, as well as to pharmaceutical compositions comprising these polymorphic forms, to processes for obtaining them, and their use in medical treatment.

    摘要翻译: 本发明涉及1-(4- {1 - [(E)-4-环己基-3-三氟甲基 - 苄氧基亚氨基] - 乙基} -2-乙基 - 苄基) - 氮杂环丁烷的盐酸盐,苹果酸盐,草酸盐和酒石酸盐 -3-羧酸(化合物I),包含该盐的药物组合物,用于形成该盐的方法及其在医疗中的用途。 此外,本发明还涉及这些盐中的每一种的新的多晶形式,以及包含这些多晶型形式的药物组合物,获得它们的方法及其在医疗中的用途。