公开(公告)号:US07807767B2
公开(公告)日:2010-10-05
申请号:US12232459
申请日:2008-09-17
申请人: No-ma Kim , Jae-gwan Lee , Suk-ky Chang
发明人: No-ma Kim , Jae-gwan Lee , Suk-ky Chang
IPC分类号: C08F12/00
CPC分类号: C08F220/14
摘要: The present invention provides a method for producing acryl syrup by bulk polymerization, comprising a step of preparing a mixture comprising monomer component and 2,4-diphenyl-4methyl-1-pentene; a step of heating the mixture to the initial reaction temperature; and a step of adding an polymerization initiator having the half-life of not more than 30 minutes at 5-80° C., wherein the initial reaction temperature is controlled so that the polymerization initiator has the half-life of up to 30 minutes. The method of the present invention has such advantages that reaction runaway does not occur, the control of molecular weight and conversion rate is possible even at low exothermic temperature, and a partially polymerized acryl syrup can also be prepared therefrom.
摘要翻译: 本发明提供了通过本体聚合制备丙烯酸树脂浆的方法,包括制备包含单体组分和2,4-二苯基-4-甲基-1-戊烯的混合物的步骤; 将混合物加热至初始反应温度的步骤; 以及在5-80℃下加入半衰期不超过30分钟的聚合引发剂的步骤,其中控制初始反应温度,使得聚合引发剂的半衰期长达30分钟。 本发明的方法具有不发生反应失控的优点,即使在低放热温度下也可以控制分子量和转化率,也可以由其制备部分聚合的丙烯酸树脂浆。
-
公开(公告)号:US20090018259A1
公开(公告)日:2009-01-15
申请号:US12232459
申请日:2008-09-17
申请人: No-ma Kim , Jae-gwan Lee , Suk-ky Chang
发明人: No-ma Kim , Jae-gwan Lee , Suk-ky Chang
IPC分类号: C08L33/12
CPC分类号: C08F220/14
摘要: The present invention provides a method for producing acryl syrup by bulk polymerization, comprising a step of preparing a mixture comprising monomer component and 2,4-diphenyl-4methyl-1-pentene; a step of heating the mixture to the initial reaction temperature; and a step of adding an polymerization initiator having the half-life of not more than 30 minutes at 5-80° C., wherein the initial reaction temperature is controlled so that the polymerization initiator has the half-life of up to 30 minutes. The method of the present invention has such advantages that reaction runaway does not occur, the control of molecular weight and conversion rate is possible even at low exothermic temperature, and a partially polymerized acryl syrup can also be prepared therefrom.
摘要翻译: 本发明提供了通过本体聚合制备丙烯酸树脂浆的方法,包括制备包含单体组分和2,4-二苯基-4-甲基-1-戊烯的混合物的步骤; 将混合物加热至初始反应温度的步骤; 以及在5-80℃下加入半衰期不超过30分钟的聚合引发剂的步骤,其中控制初始反应温度,使得聚合引发剂的半衰期长达30分钟。 本发明的方法具有不发生反应失控的优点,即使在低放热温度下也可以控制分子量和转化率,也可以由其制备部分聚合的丙烯酸树脂浆。
-