摘要:
Stable, bulk electrical superconductors are prepared by heating mixed metal oxides in the presence of oxygen in a closed vessel in a preheated oven for 1-5 hours at 850.degree.-900.degree. C. The final oxides are in the molar ratio Ti.sub.0.6-1.1 Ca.sub.2-3 Ba.sub.0.75-1.25 Cu.sub.2-3 O.sub.(5+.delta.)-(9+.delta.), where .delta. is less than one.
摘要:
Stable, bulk electrical superconductors are prepared by heating mixed metal oxides in the presence of oxygen in a closed vessel in a preheated oven for 1-5 hours at 850.degree.-900.degree. C. The final oxides are in the molar ratio Tol.sub.0.6-1.1 Ca.sub.2-3 Ba.sub.0.75-1.25 Cu.sub.2-3 O.sub.(5+.delta.)-(9+.delta.), where .delta. is less than one.
摘要:
Hydrogen is generated from water containing acid by passing electric current through it, using as the cathode a semiconductor exposed to light and having a transition metal metallocenophane compound attached to the surface of the cathode by means of a polymer.