    摘要: The production of UF.sub.6 in which UF.sub.4 is reacted with air or oxygen in the presence of a catalyst at 500.degree. to 700.degree.C. The solid byproduct of this reaction is reduced with hydrogen in the presence of a catalyst at 400.degree. to 600.degree.C. Fresh UO.sub.3 may also be reduced with hydrogen in the same reactor as UO.sub.2 F.sub.2. The reduction product or products are reacted with hydrogen fluoride at 400.degree. to 600.degree.C, producing UF.sub.4 which would be recycled for further reaction to produce UF.sub.6.

    摘要翻译: 在500℃〜700℃下,在催化剂存在下,UF4与空气或氧气反应的UF6的生成。该反应的固体副产物在催化剂存在下在400〜600℃下用氢气还原 新鲜的UO3也可以在与UO2F2相同的反应器中用氢还原。 还原产物在400〜600℃下与氟化氢反应,生成UF4,再循环再进行反应生成UF6。