Method for sulfur compounds removal from contaminated gas and liquid streams
    1.
    发明授权
    Method for sulfur compounds removal from contaminated gas and liquid streams 有权
    从污染气体和液体流中除去硫化合物的方法

    公开(公告)号:US07651550B2

    公开(公告)日:2010-01-26

    申请号:US10559734

    申请日:2003-06-06

    Abstract: A desorption process and a process for producing a catalytically deactivated formed zeolitic adsorbent, whereby both processes are suitable to improve the lifetime of a formed zeolitic adsorbent in the removal of sulfur compounds from sulfur contaminated gas and liquid feed streams. The adsorbent is in particular a synthetic 13X or LSX faujasite with a silica to alumina ratio from 1.9:1.0 to about 3.0:1.0. The cations of the faujasite include alkali and alkaline earth metals. The formed zeolite mixture is preferably catalytically deactivated due to a phosphate treatment. The desorption is carried out thermally, wherein the heat treatment is done at different temperature stages to avoid decomposition of the organic sulfur compounds.

    Abstract translation: 一种解吸工艺和一种制备催化失活的沸石吸附剂的方法,由此两种方法适合于改善形成的沸石吸附剂在从硫污染的气体和液体进料流中除去硫化合物的寿命。 吸附剂特别是二氧化硅与氧化铝比为1.9:1.0至约3.0:1.0的合成的13X或LSX八面沸石。 八面沸石的阳离子包括碱金属和碱土金属。 形成的沸石混合物由于磷酸盐处理而优选被催化失活。 解吸热进行,其中热处理在不同的温度阶段进行,以避免有机硫化合物的分解。

    Method for sulfur compounds removal from contaminated gas and liquid streams
    2.
    发明申请
    Method for sulfur compounds removal from contaminated gas and liquid streams 有权
    从污染气体和液体流中除去硫化合物的方法

    公开(公告)号:US20070193939A1

    公开(公告)日:2007-08-23

    申请号:US10559734

    申请日:2003-06-06

    Abstract: Abstract Described is a desorption process and a process for producing a catalytically deactivated formed zeolitic adsorbent, whereby both processes are suitable to improve the lifetime of a formed zeolithic adsorbant in the removal of sulfur compounds from sulfur contaminated gas and liquid feed streams. The adsorbent is in particular a synthetic 13X or LSX faujasite with a silica to alumina ratio from 1.9:1.0 to about 3.0:1.0. The cations of the faujasite include alkali and alkaline earth metals. The formed zeolite mixture is preferably catalytically deactivated due to a phosphate treatment. The desorption is carried out thermally, wherein the heat treatment is done at different temperature stages to avoid decomposition of the organic sulfur compounds.

    Abstract translation: 摘要描述了一种解吸过程和一种生产催化失活的沸石吸附剂的方法,由此两种方法都适合于改善形成的沸石吸附剂在从硫污染的气体和液体进料流中除去硫化合物的寿命。 吸附剂特别是二氧化硅与氧化铝比为1.9:1.0至约3.0:1.0的合成的13X或LSX八面沸石。 八面沸石的阳离子包括碱金属和碱土金属。 形成的沸石混合物由于磷酸盐处理而优选被催化失活。 解吸热进行,其中热处理在不同的温度阶段进行,以避免有机硫化合物的分解。