Sialon ceramic compositions and methods of fabrication
    1.
    发明授权
    Sialon ceramic compositions and methods of fabrication 失效
    赛隆陶瓷组合物和制造方法

    公开(公告)号:US5316988A

    公开(公告)日:1994-05-31

    申请号:US100888

    申请日:1993-08-02

    IPC分类号: C04B35/597 C04B35/58

    CPC分类号: C04B35/597

    摘要: A method of fabricating a SiAlON ceramic body includes: a) combining quantities of Si.sub.3 N.sub.4, Al.sub.2 O.sub.3 and CeO.sub.2 to produce a mixture; b) forming the mixture into a desired body shape; c) heating the body to a densification temperature of from about 1550.degree. C. to about 1850.degree. C.; c) maintaining the body at the densification temperature for a period of time effective to densify the body; d) cooling the densified body to a devitrification temperature of from about 1200.degree. C. to about 1400.degree. C.; and e) maintaining the densified body at the devitrification temperature for a period of time effective to produce a .beta.'-SiAlON crystalline phase in the body having elemental or compound form Ce incorporated in the .beta.'-SiAlON crystalline phase. Further, a SiAlON ceramic body comprises: a) an amorphous phase; and b) a crystalline phase, the crystalline phase comprising .beta.'-SiAlON having lattice substituted elemental or compound form Ce.

    摘要翻译: 制造SiAlON陶瓷体的方法包括:a)将Si 3 N 4,Al 2 O 3和CeO 2的组合量混合以产生混合物; b)将混合物形成所需的体形; c)将本体加热至约1550℃至约1850℃的致密化温度。 c)将身体保持在致密化温度下一段有效的时间以使身体致密化; d)将致密体冷却至约1200℃至约1400℃的失透温度; 并且e)将致密体保持在失透温度下一段时间,以有效地在体内具有并入β-SiAlON结晶相中的元素或化合物形式的Ce中的β'-SiAlON结晶相。 此外,SiAlON陶瓷体包括:a)非晶相; 和b)结晶相,所述结晶相包含具有晶格取代的元素或化合物形式的Ce的β-SiAlON。