1.
公开(公告)号:US08409421B2
公开(公告)日:2013-04-02
申请号:US12745067
申请日:2008-11-27
申请人: Massimo Maccagni , Silvano Cossali , Carmelita Roncaldier , Carlo Olper , Luigi Olper , Alessandro Olper
发明人: Marco Olper , Massimo Maccagni , Silvano Cossali
IPC分类号: C25C1/18
CPC分类号: C22B13/045 , C22B7/008 , C25C1/18 , Y02P10/122 , Y02P10/234
摘要: The present invention relates to an electrolytic process for producing metallic lead starting from desulfurized lead pastel comprising the following operative phases: a) leaching the desulfurized pastel by putting it in contact with a solution comprising ammonium chloride, with the formation of a leach liquor and evolution of gaseous CO2; b) separating a first solid residue and a first clarified leach liquor from the leach liquor coming from phase a); c) leaching the solid residue separated in phase b) by putting it in contact with a solution comprising ammonium chloride and hydrogen peroxide; d) separating a second solid residue and a second clarified leach liquor from the leach liquor coming from phase c); e) joining the first clarified leach liquor coming from phase b) with the second clarified leach liquor coming from phase d) and forming a single solution; f) subjecting the solution leaving phase e) to electrolysis in a flow cell, with a current density ranging from 50 to 10,000 A/m2, said electrolysis resulting in the formation of a lead sponge. The present invention also relates to the relative desulfurization process of the pastel.
摘要翻译: 本发明涉及一种用于从脱硫铅膏制备金属铅的电解方法,其包括以下操作阶段:a)通过将脱硫粉末与包含氯化铵的溶液接触,浸出脱硫粉末,形成浸出液并进行 的气态二氧化碳; b)从第一阶段a)的浸出液中分离出第一固体残余物和第一澄清浸出液; c)通过使其与包含氯化铵和过氧化氢的溶液接触来浸出在相b)中分离的固体残余物; d)从相c)的浸出液中分离出第二固体残渣和第二澄清浸出液; e)将来自相b)的第一澄清浸出液与来自相d)的第二澄清浸出液接合并形成单一溶液; f)使离开相e)的溶液在流动池中电解,电流密度范围为50至10,000A / m 2,所述电解导致形成铅海绵。 本发明还涉及到粉笔的相对脱硫工艺。
-
2.
公开(公告)号:US20110083970A1
公开(公告)日:2011-04-14
申请号:US12745067
申请日:2008-11-27
申请人: Marco Olper , Carmelita Roncaldier , Carlo Olper , Luigi Olper , Alessandro Olper , Massimo Maccagni , Silvano Cossali
发明人: Marco Olper , Carmelita Roncaldier , Carlo Olper , Luigi Olper , Alessandro Olper , Massimo Maccagni , Silvano Cossali
CPC分类号: C22B13/045 , C22B7/008 , C25C1/18 , Y02P10/122 , Y02P10/234
摘要: The present invention relates to an electrolytic process for producing metallic lead starting from desulfurized lead pastel comprising the following operative phases: a) leaching the desulfurized pastel by putting it in contact with a solution comprising ammonium chloride, with the formation of a leach liquor and evolution of gaseous CO2; b) separating a first solid residue and a first clarified leach liquor from the leach liquor coming from phase a); c) leaching the solid residue separated in phase b) by putting it in contact with a solution comprising ammonium chloride and hydrogen peroxide; d) separating a second solid residue and a second clarified leach liquor from the leach liquor coming from phase c); e) joining the first clarified leach liquor coming from phase b) with the second clarified leach liquor coming from phase d) and forming a single solution; f) subjecting the solution leaving phase e) to electrolysis in a flow cell, with a current density ranging from 50 to 10,000 A/m2, said electrolysis resulting in the formation of a lead sponge. The present invention also relates to the relative desulfurization process of the pastel.
摘要翻译: 本发明涉及一种用于从脱硫铅膏制备金属铅的电解方法,其包括以下操作阶段:a)通过将脱硫粉末与包含氯化铵的溶液接触,浸出脱硫粉末,形成浸出液并进行 的气态二氧化碳; b)从第一阶段a)的浸出液中分离出第一固体残余物和第一澄清浸出液; c)通过使其与包含氯化铵和过氧化氢的溶液接触来浸出在相b)中分离的固体残余物; d)从相c)的浸出液中分离出第二固体残渣和第二澄清浸出液; e)将来自相b)的第一澄清浸出液与来自相d)的第二澄清浸出液接合并形成单一溶液; f)使离开相e)的溶液在流动池中电解,电流密度范围为50至10,000A / m 2,所述电解导致形成铅海绵。 本发明还涉及到粉笔的相对脱硫工艺。
-