摘要:
An injection molding composition includes: 100 parts by weight of a propylene-ethylene copolymer comprising a crystalline portion and a non-crystalline portion; and 17 to 33 parts by weight of inorganic particles capable of imparting at least one of rigidity and heat resistance to the propylene-ethylene copolymer. The propylene-ethylene copolymer has a melt flow rate of 15 to 50 g/10 min and a molecular weight distribution (Mw/Mn) of not less than 5. A crystalline ethylene polymer contained in the crystalline portion and a non-crystalline propylene-ethylene copolymer contained in the non-crystalline portion have a total amount ranging from 10 to 20% by weight.