公开(公告)号:US20080284973A1
公开(公告)日:2008-11-20
申请号:US12122452
申请日:2008-05-16
IPC分类号: G02F1/13
CPC分类号: G02F1/141 , G02F1/1337
摘要: A method of fabricating a liquid crystal display device by introducing a ferroelectric liquid crystal (FLC) between two substrates, contacting the FLC to a molecularly smooth edge, and aligning the FLC by introducing a temperature gradient normal to the edge. In one embodiment, the FLC is aligned by cooling it from an isotropic phase to a smectic phase at a rate that is relatively slow. For example, the cooling rate may be less than about 3 degrees Celsius per hour. In one embodiment, smectic layers are formed that are parallel to the edge. In one embodiment, the molecularly smooth edge is an air bubble.