公开(公告)号:US20240018278A1
公开(公告)日:2024-01-18
申请号:US18253835
申请日:2021-11-17
Inventor: Francis C. RIX , Charles J. HARLAN , KyKA LE , Xiaodan ZHANG
IPC: C08F4/52
CPC classification number: C08F4/52 , C08F2410/01 , C08F2500/04 , C08F2500/17
Abstract: The present disclosure relates to processes for forming alumoxanes and catalyst systems thereof for olefin polymerization. In at least one embodiment, a process includes forming a solution by, in an aliphatic hydrocarbon having a boiling point of less than about 70 degrees Celsius, introducing at least one hydrocarbyl aluminum with at least one non-hydrolytic oxygen-containing compound and a support material. The molar ratio of aluminum to non-hydrolytic oxygen in the solution is greater than or equal to 1.5, and the combining is conducted at a temperature of less than about 70 degrees Celsius. The process includes distilling the solution at a pressure of greater than about 0.5 atm to form a supported alumoxane precursor. The process further includes heating the supported alumoxane precursor to a temperature greater than the boiling point of the aliphatic hydrocarbon fluid and less than about 160 degrees Celsius to form a supported alumoxane.
-
公开(公告)号:US20240400804A1
公开(公告)日:2024-12-05
申请号:US18696216
申请日:2022-10-04
Inventor: Nino RUOCCO , Maria Josefina CARBONE , Etienne RH LERNOUX , Michael A. LEAF , Wen LI , Adriana S. SILVA
Abstract: The present disclosure relates to polyethylene blends, films thereof, and methods thereof. In at least one embodiment, a polymer blend includes a first polyethylene having a density of about 0.94 g/cm3 to about 0.97 g/cm3 and a melt index of about 0.1 g/10 min to about 10 g/10 min. The blend includes a second polyethylene comprising at least 80 wt % ethylene derived-units. The second polyethylene has a density of about 0.918 g/cm3 to about 0.945 g/cm3, a number average molecular weight (Mn) of about 10,000 g/mol to about 20,000 g/mol, a weight-average molecular weight (Mw) of about 75,000 g/mol to about 300,000 g/mol, a melt index (2.16 kg) of about 0.1 g/10 min to about 5 g/10 min, a high load melt index (21.6 kg) of about 25 g/10 min to about 80 g/10 min, and a melt index ratio of about 10 to about 50.
-