Manufacturing method for isothermal evaporation casting process
    1.
    发明授权
    Manufacturing method for isothermal evaporation casting process 有权
    等温蒸发铸造工艺的制造方法

    公开(公告)号:US07648598B2

    公开(公告)日:2010-01-19

    申请号:US11584847

    申请日:2006-10-23

    IPC分类号: C22C19/03 B22D27/00

    CPC分类号: C22C19/007 C22C3/00 C22C23/00

    摘要: A manufacturing method for an isothermal evaporation casting process is disclosed and to design the manufacturing method for the simple atmospheric casting. The present invention can melt the Mg—Ni alloy with the aspect of totally different melting points thereof, and the other elements can be added during melting simultaneously. Through the Mg—Ni alloy with a suitable weight ratio, the eutectic alloy of Mg/Mg2Ni and high purified γ-phase Mg2Ni can be made. Then adding other elements are to produce the composition of Mg/Ni/M. By way of the manufacturing method of the present invention, the melting equipment is simplified; and, through different manufacturing steps, the purposes of time-saving and low cost are reached; further that, a large amount of the eutectic alloy of Mg/Mg2Ni with different kinds of ratios of Mg, high purified γ-phase Mg2Ni, or the composition of Mg/Ni/M can be obtained.

    摘要翻译: 公开了一种等温蒸发铸造工艺的制造方法,并设计了简单大气铸造的制造方法。 本发明可以熔融Mg-Ni合金,其熔点完全不同,其它元素可以在熔融的同时加入。 通过合适重量比的Mg-Ni合金,可以制备Mg / Mg2Ni和高纯γ相Mg2Ni共晶合金。 然后添加其他元素是产生Mg / Ni / M的组成。 通过本发明的制造方法,简化了熔化设备; 通过不同的制造步骤,实现了节省时间和低成本的目的; 此外,可以获得大量的具有不同种类的Mg,高纯度γ相Mg2Ni比的Mg / Mg2Ni或Mg / Ni / M组成的共晶合金。

    Manufacturing method for isothermal evaporation casting process
    2.
    发明申请
    Manufacturing method for isothermal evaporation casting process 有权
    等温蒸发铸造工艺的制造方法

    公开(公告)号:US20080093046A1

    公开(公告)日:2008-04-24

    申请号:US11584847

    申请日:2006-10-23

    IPC分类号: B22D27/00 C22C19/03

    CPC分类号: C22C19/007 C22C3/00 C22C23/00

    摘要: A manufacturing method for an isothermal evaporation casting process is disclosed and to design the manufacturing method for the simple atmospheric casting. The present invention can melt the Mg—Ni alloy with the aspect of totally different melting points thereof, and the other elements can be added during melting simultaneously. Through the Mg—Ni alloy with a suitable weight ratio, the eutectic alloy of Mg/Mg2Ni and high purified γ-phase Mg2Ni can be made. Then adding other elements are to produce the composition of Mg/Ni/M. By way of the manufacturing method of the present invention, the melting equipment is simplified; and, through different manufacturing steps, the purposes of time-saving and low cost are reached; further that, a large amount of the eutectic alloy of Mg/Mg2Ni with different kinds of ratios of Mg, high purified γ-phase Mg2Ni, or the composition of Mg/Ni/M can be obtained.

    摘要翻译: 公开了一种等温蒸发铸造工艺的制造方法,并设计了简单大气铸造的制造方法。 本发明可以熔融Mg-Ni合金,其熔点完全不同,其它元素可以在熔融的同时加入。 通过具有合适重量比的Mg-Ni合金,可以制备Mg / Mg 2 Ni和高纯度γ相Mg 2 Ni的共晶合金。 然后添加其他元素是产生Mg / Ni / M的组成。 通过本发明的制造方法,简化了熔化设备; 通过不同的制造步骤,实现了节省时间和低成本的目的; 此外,大量Mg / Mg 2 Ni的共晶合金与Mg,高纯度γ相Mg 2 Ni的比例不同,或组合物 的Mg / Ni / M。

    Method and apparatus of preventing gas leak in pipeline
    3.
    发明申请
    Method and apparatus of preventing gas leak in pipeline 审中-公开
    防止管道中气体泄漏的方法和装置

    公开(公告)号:US20090091130A1

    公开(公告)日:2009-04-09

    申请号:US11923769

    申请日:2007-10-25

    IPC分类号: F16J15/02

    CPC分类号: F16L25/14 F16L15/04 F16L21/08

    摘要: This invention discloses a method and an apparatus of preventing a gas leak in a pipeline, and the characteristic of expansion occurred when a hydrogen storage material absorbs hydrogen gas is used for setting the hydrogen storage material in a joint between a first pipeline and a second pipeline, such that if hydrogen leaks at the joint, the hydrogen storage material will absorb hydrogen to expand, and the expansion pressure presses the joint to give a tighter connection, so as to achieve the effects of preventing and locking a leak, and compensating a deficiency of tightness due to an accumulated error occurred during the manufacture of the first pipeline and the second pipeline.

    摘要翻译: 本发明公开了一种防止管道中的气体泄漏的方法和装置,并且当储氢材料吸收氢气时发生膨胀的特征,用于将储氢材料设置在第一管线和第二管道之间的接头中 ,使得如果氢气在接头处泄漏,则储氢材料将吸收氢气膨胀,并且膨胀压力按压接头以提供更紧密的连接,从而达到防止和锁定泄漏的效果,并补偿缺陷 由于在第一管道和第二管道的制造期间发生累积的误差而产生的紧密度。