公开(公告)号:US07799889B2
公开(公告)日:2010-09-21
申请号:US11312020
申请日:2005-12-20
申请人: Alexander Meyer , Helmut Einberger , Wolfgang Ebert , Michael Prein , Wilfried Haese , Uli Franz , Stephan Konrad
发明人: Alexander Meyer , Helmut Einberger , Wolfgang Ebert , Michael Prein , Wilfried Haese , Uli Franz , Stephan Konrad
CPC分类号: C08G64/12 , Y10T428/31504 , Y10T428/31507
摘要: The present invention provides a polycarbonate resin produced by the continuous interfacial process characterized in that after alkaline hydrolysis with sodium hydroxide, the polycarbonate resin contains an amount of 0.01 to 150 ppm of carbamate compounds according to formula (1) said amount measured by high pressure liquid chromatography, wherein R1 and R2 independently of one another denote hydrogen or C1-C12-alkyl, or together denote C4-C12-alkylidene, and R3 and R4 independently of one another denote hydrogen. C1-C12-alkyl or phenyl, or together with the carbon atom to which they are bonded form cyclohexyl or trimethylcyclohexyl, the process comprising phosgene reacting with at least one bisphenol at 8 to 17% molar excess of phosgene relative to the bisphenol.
摘要翻译: 本发明提供了一种通过连续界面方法制备的聚碳酸酯树脂,其特征在于在用氢氧化钠碱化后,聚碳酸酯树脂含有0.01至150ppm根据式(1)的氨基甲酸酯化合物,所述量由高压液体 色谱法,其中R 1和R 2彼此独立地表示氢或C 1 -C 12烷基,或一起表示C 4 -C 12亚烷基,并且R 3和R 4彼此独立地表示氢。 C1-C12烷基或苯基,或与它们所键合的碳原子一起形成环己基或三甲基环己基,该方法包括与相对于双酚的8至17摩尔过量的光气与至少一种双酚反应的方法。
-
公开(公告)号:US20060155098A1
公开(公告)日:2006-07-13
申请号:US11312886
申请日:2005-12-20
申请人: Hermann Kauth , Wolfgang Ebert , Wilfried Haese , Helmut Einberger , Alexander Meyer , Andreas Frankenau , Uli Franz , Christian Eh , Stefaan De Vos , Bert Ruytinx
发明人: Hermann Kauth , Wolfgang Ebert , Wilfried Haese , Helmut Einberger , Alexander Meyer , Andreas Frankenau , Uli Franz , Christian Eh , Stefaan De Vos , Bert Ruytinx
IPC分类号: C08G64/00
CPC分类号: C08G64/24 , Y10T428/31507
摘要: An improvement to the phase interface process of preparing aromatic polycarbonate is disclosed. The process is characterized in that the phosgenation is carried out at 0 to 40° C., and in that the temperature of the reaction mixture at the time of addition of the catalyst at 10 to 40° C., and in that the molar ratio of aromatic dihydroxy compounds to phosgene at 1:1.05 to 1:1.20. The polycarbonate thus produced is characterized in its low content of carbamates, making it particularly suitable for the preparation of optical storage media.
摘要翻译: 公开了制备芳族聚碳酸酯的相界面方法的改进。 该方法的特征在于光气化在0至40℃进行,并且在10至40℃下加入催化剂时反应混合物的温度,并且摩尔比 的芳族二羟基化合物与光气的比例为1:1.05至1:1.20。 由此制备的聚碳酸酯的特征在于其低含量的氨基甲酸酯,使其特别适用于制备光学存储介质。
-
公开(公告)号:US07705107B2
公开(公告)日:2010-04-27
申请号:US11312886
申请日:2005-12-20
申请人: Hermann Kauth , Wolfgang Ebert , Wilfried Haese , Helmut Einberger , Alexander Meyer , Andreas Frankenau , Uli Franz , Christian Eh , Stefaan De Vos , Bert Ruytinx
发明人: Hermann Kauth , Wolfgang Ebert , Wilfried Haese , Helmut Einberger , Alexander Meyer , Andreas Frankenau , Uli Franz , Christian Eh , Stefaan De Vos , Bert Ruytinx
CPC分类号: C08G64/24 , Y10T428/31507
摘要: An improvement to the phase interface process of preparing aromatic polycarbonate is disclosed. The process is characterized in that the phosgenation is carried out at 0 to 40° C., and in that the temperature of the reaction mixture at the time of addition of the catalyst at 10 to 40° C., and in that the molar ratio of aromatic dihydroxy compounds to phosgene at 1:1.05 to 1:1.20. The polycarbonate thus produced is characterized in its low content of carbamates, making it particularly suitable for the preparation of optical storage media.
摘要翻译: 公开了制备芳族聚碳酸酯的相界面方法的改进。 该方法的特征在于光气化在0至40℃进行,并且在10至40℃下加入催化剂时反应混合物的温度,并且摩尔比 的芳族二羟基化合物与光气的比例为1:1.05至1:1.20。 由此制备的聚碳酸酯的特征在于其低含量的氨基甲酸酯,使其特别适用于制备光学存储介质。
-
公开(公告)号:US20060135735A1
公开(公告)日:2006-06-22
申请号:US11312020
申请日:2005-12-20
申请人: Alexander Meyer , Helmut Einberger , Wolfgang Ebert , Michael Prein , Wilfried Haese , Uli Franz , Stephan Konrad
发明人: Alexander Meyer , Helmut Einberger , Wolfgang Ebert , Michael Prein , Wilfried Haese , Uli Franz , Stephan Konrad
IPC分类号: C08G64/00
CPC分类号: C08G64/12 , Y10T428/31504 , Y10T428/31507
摘要: A polycarbonate resin that after alkaline hydrolysis with sodium hydroxide contain an amount of 0.01 to 150 ppm of carbamate compounds according to formula (1) wherein R1 and R2 independently of one another denote hydrogen or C1-C12-alkyl, or together denote C4-C12-alkylidene, and R3 and R4 independently of one another denote hydrogen, C1-C12-alkyl or phenyl, or together with the carbon atom to which they are bonded form cyclohexyl or trimethylcyclohexyl, said amount measured after alkaline hydrolysis with sodium hydroxide by high pressure liquid chromatography.
摘要翻译: 用氢氧化钠碱性水解后的聚碳酸酯树脂含有0.01〜150ppm的式(1)的氨基甲酸酯化合物,其中R 1和R 2独立地为1 另一个表示氢或C 1 -C 12 - 烷基,或一起表示C 4 -C 12 - 亚烷基 ,R 3和R 4彼此独立地表示氢,C 1 -C 12 - 烷基或 苯基或与它们键合的碳原子一起形成环己基或三甲基环己基,所述量通过高压液相色谱用氢氧化钠碱化后测量。
-
-
-