公开(公告)号:US20110042625A1
公开(公告)日:2011-02-24
申请号:US12917707
申请日:2010-11-02
申请人: Ichirou Tanaka , Hiroshi Fujimura , Hirokatsu Nitomi , Hiroyoshi Yashiki , Kouji Nishida , Hiroki Takamaru
发明人: Ichirou Tanaka , Hiroshi Fujimura , Hirokatsu Nitomi , Hiroyoshi Yashiki , Kouji Nishida , Hiroki Takamaru
CPC分类号: H01F1/16 , C22C38/004 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/12 , H01F1/14791 , H01F27/245
摘要: A main object thereof is to provide a non-oriented electrical steel sheet being excellent in surface characteristics and having both excellent mechanical characteristics and magnetic characteristics necessary for a rotor of rotating machines such as motors and generators which rotate at a high speed, and a method for producing the same. To achieve the object, the present invention provides a non-oriented electrical steel sheet comprising in % by mass: 0.06% or less of C; 3.5% or less of Si; from 0.05% or more to 3.0% or less of Mn; 2.5% or less of Al; 0.30% or less of P; 0.04% or less of S; 0.02% or less of N; at least one element selected from the group consisting of Nb, Ti, Zr and V in the predetermined range; and a balance consisting of Fe and impurities; and having a recrystallized fraction being less than 90%.
摘要翻译: 其主要目的是提供一种表面特性优异且具有优异的机械特性和磁性特性的非取向电工钢板,其特征在于,高速旋转的电动机和发电机等旋转机械的转子必须具有优异的机械特性和磁特性, 为了生产相同。 为了达到上述目的,本发明提供一种非定向电工钢板,其含有质量%:0.06%以下的C, 3.5%以下的Si; 从0.05%以上至3.0%以下的Mn; 2.5%以下的Al; 0.30%以下的P; 0.04%以下的S; 0.02%以下的N; 选自Nb,Ti,Zr和V中的至少一种元素在预定范围内; 余量由铁和杂质组成; 并且重结晶部分小于90%。
-
2.
公开(公告)号:US06340399B1
公开(公告)日:2002-01-22
申请号:US09593744
申请日:2000-06-14
申请人: Ichiro Tanaka , Hiroyoshi Yashiki , Mitsuyo Maeda , Taisei Nakayama , Noriyuki Honjou , Shinsuke Mita
发明人: Ichiro Tanaka , Hiroyoshi Yashiki , Mitsuyo Maeda , Taisei Nakayama , Noriyuki Honjou , Shinsuke Mita
IPC分类号: H01F1147
CPC分类号: C22C38/06 , C21D8/1205 , C21D8/1261 , C21D8/1272 , C22C38/002 , C22C38/004 , C22C38/02 , C22C38/04 , H01F1/14775 , H02K1/02 , Y02P10/212
摘要: The non-oriented electrical steel sheet having the following chemical composition : C: 0.01% or less, Si: 2.5% or less, Mn: 2% or less, Al: 1 to 5%, Si+Al+0.5×Mn: 2.5 to 5%, with a sheet thickness of 0.1 to 0.4 mm, an average grain diameter of 50 to 180 &mgr;m and a Vickers hardness of 130 to 210. The steel sheet is excellent in workability such as punchability and interlocking performance for forming it into cores for motors and also has a lower iron loss and higher magnetic flux density, and thus when used as a core in a motor, achieves the high a motor efficiency. The steel sheet is particularly suitable as a material for cores in inverter-controlled motors.
摘要翻译: 具有以下化学组成的无取向电工钢板:C:0.01%以下,Si:2.5%以下,Mn:2%以下,Al:1〜5%,Si + Al + 0.5xMn:2.5〜 5%,板厚度为0.1〜0.4mm,平均粒径为50〜180μm,维氏硬度为130〜210。该钢板的加工性优异,可形成为芯的互锁性, 电动机也具有较低的铁损和更高的磁通密度,因此当用作电动机中的铁芯时,实现了高的电动机效率。 钢板特别适用于变频器控制电机的铁心材料。
-
公开(公告)号:US06638368B2
公开(公告)日:2003-10-28
申请号:US09985444
申请日:2001-11-02
申请人: Ichiro Tanaka , Hiroyoshi Yashiki , Mitsuyo Maeda , Taisei Nakayama , Noriyuki Honjou , Shinsuke Mita
发明人: Ichiro Tanaka , Hiroyoshi Yashiki , Mitsuyo Maeda , Taisei Nakayama , Noriyuki Honjou , Shinsuke Mita
IPC分类号: H01F100
CPC分类号: C22C38/06 , C21D8/1205 , C21D8/1261 , C21D8/1272 , C22C38/002 , C22C38/004 , C22C38/02 , C22C38/04 , H01F1/14775 , H02K1/02 , Y02P10/212
摘要: The non-oriented electrical steel sheet having the following chemical composition: C: 0.01% or less, Si: 2.5% or less, Mn: 2% or less, Al: 1 to 5%, Si+Al+0.5×Mn: 2.5 to 5%, with a sheet thickness of 0.1 to 0.4 mm, an average grain diameter of 50 to 180 &mgr;m and a Vickers hardness of 130 to 210. The steel sheet is excellent in workability such as punchability and interlocking performance for forming it into cores for motors and also has a lower iron loss and higher magnetic flux density, and thus when used as a core in a motor, achieves the high a motor efficiency. The steel sheet is particularly suitable as a material for cores in inverter-controlled motors.
-
公开(公告)号:US08157928B2
公开(公告)日:2012-04-17
申请号:US12917707
申请日:2010-11-02
申请人: Ichirou Tanaka , Hiroshi Fujimura , Hirokatsu Nitomi , Hiroyoshi Yashiki , Kouji Nishida , Hiroki Takamaru
发明人: Ichirou Tanaka , Hiroshi Fujimura , Hirokatsu Nitomi , Hiroyoshi Yashiki , Kouji Nishida , Hiroki Takamaru
CPC分类号: H01F1/16 , C22C38/004 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/12 , H01F1/14791 , H01F27/245
摘要: A main object thereof is to provide a non-oriented electrical steel sheet being excellent in surface characteristics and having both excellent mechanical characteristics and magnetic characteristics necessary for a rotor of rotating machines such as motors and generators which rotate at a high speed, and a method for producing the same. To achieve the object, the present invention provides a non-oriented electrical steel sheet comprising in % by mass: 0.06% or less of C; 3.5% or less of Si; from 0.05% or more to 3.0% or less of Mn; 2.5% or less of Al; 0.30% or less of P; 0.04% or less of S; 0.02% or less of N; at least one element selected from the group consisting of Nb, Ti, Zr and V in the predetermined range; and a balance consisting of Fe and impurities; and having a recrystallized fraction being less than 90%.
摘要翻译: 其主要目的是提供一种表面特性优异且具有优异的机械特性和磁性特性的非取向电工钢板,其特征在于,高速旋转的电动机和发电机等旋转机械的转子必须具有优异的机械特性和磁特性, 为了生产相同。 为了达到上述目的,本发明提供一种非定向电工钢板,其含有质量%:0.06%以下的C, 3.5%以下的Si; 从0.05%以上至3.0%以下的Mn; 2.5%以下的Al; 0.30%以下的P; 0.04%以下的S; 0.02%以下的N; 选自Nb,Ti,Zr和V中的至少一种元素在预定范围内; 余量由铁和杂质组成; 并且重结晶部分小于90%。
-
公开(公告)号:US5250123A
公开(公告)日:1993-10-05
申请号:US850857
申请日:1992-03-13
申请人: Hiroyoshi Yashiki , Teruo Kaneko
发明人: Hiroyoshi Yashiki , Teruo Kaneko
摘要: An oriented silicon steel sheet with a very low core loss and a process for producing it at a lower cost are disclosed. The steel sheet consists essentially of Si: 1.5-3.0%, Mn: 1.0-3.0%, sol. Al: 0.003-0.015%, with Si (%)-0.5.times.Mn (%).ltoreq.2.0 and the balance being Fe and incidental impurities, in which the amount of C and N as impurities is not more than 0.0020%, with S being not more than 0.01%. This steel sheet can be produced from a slab containing up to 0.01% C and 0.001-0.010% N through hot rolling, cold rolling, primary and secondary recrystallization, and then decarburization.
-
公开(公告)号:US07922834B2
公开(公告)日:2011-04-12
申请号:US11988296
申请日:2005-12-06
申请人: Ichirou Tanaka , Hiroshi Fujimura , Hirokatsu Nitomi , Hiroyoshi Yashiki , Kouji Nishida , Hiroki Takamaru
发明人: Ichirou Tanaka , Hiroshi Fujimura , Hirokatsu Nitomi , Hiroyoshi Yashiki , Kouji Nishida , Hiroki Takamaru
CPC分类号: H01F1/16 , C22C38/004 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/12 , H01F1/14791 , H01F27/245
摘要: A main object thereof is to provide a non-oriented electrical steel sheet being excellent in surface characteristics and having both excellent mechanical characteristics and magnetic characteristics necessary for a rotor of rotating machines such as motors and generators which rotate at a high speed, and a method for producing the same. To achieve the object, the present invention provides a non-oriented electrical steel sheet comprising in % by mass: 0.06% or less of C; 3.5% or less of Si; from 0.05% or more to 3.0% or less of Mn; 2.5% or less of Al; 0.30% or less of P; 0.04% or less of S; 0.02% or less of N; at least one element selected from the group consisting of Nb, Ti, Zr and V in the predetermined range; and a balance consisting of Fe and impurities; and having a recrystallized fraction being less than 90%.
摘要翻译: 其主要目的是提供一种表面特性优异且具有优异的机械特性和磁性特性的非取向电工钢板,其特征在于,高速旋转的电动机和发电机等旋转机械的转子必须具有优异的机械特性和磁特性, 为了生产相同。 为了达到上述目的,本发明提供一种非定向电工钢板,其含有质量%:0.06%以下的C, 3.5%以下的Si; 从0.05%以上至3.0%以下的Mn; 2.5%以下的Al; 0.30%以下的P; 0.04%以下的S; 0.02%以下的N; 选自Nb,Ti,Zr和V中的至少一种元素在预定范围内; 余量由铁和杂质组成; 并且重结晶部分小于90%。
-
公开(公告)号:US20090202383A1
公开(公告)日:2009-08-13
申请号:US11988296
申请日:2005-12-06
申请人: Ichirou Tanaka , Hiroshi Fujimura , Hirokatsu Nitomi , Hiroyoshi Yashiki , Kouji Nishida , Hiroki Takamaru
发明人: Ichirou Tanaka , Hiroshi Fujimura , Hirokatsu Nitomi , Hiroyoshi Yashiki , Kouji Nishida , Hiroki Takamaru
CPC分类号: H01F1/16 , C22C38/004 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/12 , H01F1/14791 , H01F27/245
摘要: A main object thereof is to provide a non-oriented electrical steel sheet being excellent in surface characteristics and having both excellent mechanical characteristics and magnetic characteristics necessary for a rotor of rotating machines such as motors and generators which rotate at a high speed, and a method for producing the same. To achieve the object, the present invention provides a non-oriented electrical steel sheet comprising in % by mass: 0.06% or less of C; 3.5% or less of Si; from 0.05% or more to 3.0% or less of Mn; 2.5% or less of Al; 0.30% or less of P; 0.04% or less of S; 0.02% or less of N; at least one element selected from the group consisting of Nb, Ti, Zr and Vin the predetermined range; and a balance consisting of Fe and impurities; and having a recrystallized fraction being less than 90%.
摘要翻译: 其主要目的是提供一种表面特性优异且具有优异的机械特性和磁性特性的非取向电工钢板,其特征在于,高速旋转的电动机和发电机等旋转机械的转子必须具有优异的机械特性和磁特性, 为了生产相同。 为了达到上述目的,本发明提供一种非定向电工钢板,其含有质量%:0.06%以下的C, 3.5%以下的Si; 从0.05%以上至3.0%以下的Mn; 2.5%以下的Al; 0.30%以下的P; 0.04%以下的S; 0.02%以下的N; 选自Nb,Ti,Zr和Vin中的至少一种元素为预定范围; 余量由铁和杂质组成; 并且重结晶部分小于90%。
-
公开(公告)号:US5425820A
公开(公告)日:1995-06-20
申请号:US1618
申请日:1993-01-08
申请人: Hiroyoshi Yashiki , Teruo Kaneko , Takashi Tanaka
发明人: Hiroyoshi Yashiki , Teruo Kaneko , Takashi Tanaka
CPC分类号: C21D8/12 , C22C38/02 , C22C38/04 , H01F1/14775 , C21D8/1227 , C21D8/1272
摘要: An oriented magnetic steel sheet with a very low core loss and a process for manufacturing it at a lower cost are disclosed. The steel sheet consists essentially of Si: greater than 3.0% and at most 6.0%, Mn: greater than 2.0% and at moat 8.0%, sol. Al: 0.003-0.015%, with Si (%)-0.5.times.Mn (%).ltoreq.2.0 and the balance being Fe and incidental impurities, The amounts of C, N, and S as impurities are respectively at most 0.005%, at most 0.006%, and at most 0.01%. This steel sheet can be produced from a slab containing up to 0.01% C., up to 0.01% S and 0.001-0.010% N by (i) hot rolling the slab to obtain a hot-rolled steel sheet, (ii) cold rolling the hot-rolled steel sheet, as hot-rolled or after being subsequently annealed, one or more times with an intermediate annealing performed between successive stages of cold rolling to prepare a cold-rolled sheet, (iii) causing primary recrystallization by continuous annealing of the cold-rolled sheet, and (iv) finish annealing the continuously annealed steel sheet. The cold rolling may be carried out at a sheet temperature of 70.degree.-300.degree. C. The finish annealing preferably comprises causing secondary recrystallization by holding the annealed sheet in a temperature range of 825.degree.-925.degree. C. for 7-100 hours in a nitrogen-containing atmosphere, and holding the secondary-recrystallized sheet in a temperature range greater than 925.degree. C. and up to 1050.degree. C. for 4-100 hours in a hydrogen atmosphere to carry out purification annealing.
摘要翻译: 公开了一种磁芯损耗非常低的取向磁性钢板及其制造成本低的方法。 钢板基本上由Si组成:大于3.0%,最多6.0%,Mn:大于2.0%,护城河8.0%,溶胶。 Al:0.003-0.015%,Si(%)-0.5×Mn(%)≤2.0,余量为Fe和杂质,作为杂质的C,N和S的量分别为0.005%以下, 最多0.006%,最多0.01%。 该钢板可以通过(i)热轧板坯得到热轧钢板,由含有高达0.01%C,至多0.01%S和0.001-0.010%N的板坯制造,(ii)冷轧 热轧后或退火后的热轧钢板进行一次以上的连续冷轧后的中间退火,制成冷轧板,(iii)通过连续退火进行一次再结晶 冷轧板,(iv)对连续退火的钢板进行最终退火。 冷轧可以在70℃-300℃的板温下进行。最终退火优选包括通过将退火板保持在825-925℃的温度范围内进行二次再结晶7-100小时 含氮气氛中,并在氢气氛中将二次再结晶的片材在大于925℃和高达1050℃的温度范围内保持4-100小时以进行纯化退火。
-
-
-
-
-
-
-